| Category | Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Glass Bead Filled |
| Manufacturer | CP-Polymer-Technik GmbH & Co. |
| Trade Name | Wellamid® |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | CP-Polymer-Technik Wellamid® 6000 GS 15 HWCP 15% Glass Sphere Filled Nylon 6, Heat Stabilized, Conditioned.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.23 g/cc | 0.0444 lb/in³ | ISO 1183 |
| Moisture Absorption at Equilibrium | 2.2 - 3.0 % | 2.2 - 3.0 % | 23°C/50%RH, Starting when dry; DIN 53495 |
| Linear Mold Shrinkage | 0.0080 - 0.010 cm/cm @Thickness 4.00 mm |
0.0080 - 0.010 in/in @Thickness 0.157 in |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 40.0 MPa | 5800 psi | 5 mm/min; ISO 527 |
| Elongation at Break | 25 % | 25 % | 5 mm/min; ISO 527 |
| Tensile Modulus | 1.40 GPa | 203 ksi | ISO 527 |
| Charpy Impact Unnotched | NB @Temperature 23.0 °C |
NB @Temperature 73.4 °F |
ISO 179 |
| Charpy Impact, Notched | 1.30 J/cm² @Temperature 23.0 °C |
6.19 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 215 °C | 419 °F | Kofler |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+12 ohm-cm | 1.00e+12 ohm-cm | IEC 93 |
| Surface Resistance | 1.00e+10 ohm | 1.00e+10 ohm | ISO 3915 |
| Dielectric Constant | 6.0 @Frequency 1e+6 Hz |
6.0 @Frequency 1e+6 Hz |
IEC 250 |
| Dielectric Strength | 35.0 kV/mm | 889 kV/in | IEC 243-1 |
| Dielectric Loss Index | 0.20 | 0.20 | At 1 MHz; IEC 250 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 250 - 270 °C | 482 - 518 °F | |
| Mold Temperature | 60.0 - 90.0 °C | 140 - 194 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Back Pressure | Low | |
| Holding Pressure | High | |
| Injection Speed | Medium | |
| Screw Speed | High |