| Category | Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 40% Glass Fiber Filled |
| Manufacturer | DSM Engineering Plastics |
| Trade Name | Akulon® |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | DSM Akulon® N24-G8 PA6-GF40.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.45 g/cc | 0.0524 lb/in³ | dry; ISO 1183 |
| Water Absorption | 5.5 % | 5.5 % | Sim. To ISO 62 |
| Moisture Absorption | 1.70 % | 1.70 % | Sim. To ISO 62 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Ultimate | 200 MPa | 29000 psi | dry; ISO 527-1/-2 |
| Elongation at Break | 2.5 % | 2.5 % | dry; ISO 527-1/-2 |
| Tensile Modulus | 12.0 GPa | 1740 ksi | dry; ISO 527-1/-2 |
| Charpy Impact, Notched | 1.40 J/cm² @Temperature -30.0 °C |
6.66 ft-lb/in² @Temperature -22.0 °F |
dry; ISO 179/1eA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 20.0 µm/m-°C | 11.1 µin/in-°F | dry; ISO 11359-1/-2 |
| CTE, linear, Transverse to Flow | 50.0 µm/m-°C | 27.8 µin/in-°F | dry; ISO 11359-1/-2 |
| Melting Point | 220 °C | 428 °F | 10°C/min; ISO 11357-1/-3 |
| Deflection Temperature at 0.46 MPa (66 psi) | 220 °C | 428 °F | dry; ISO 75-1/-2 |
| Deflection Temperature at 1.8 MPa (264 psi) | 210 °C | 410 °F | dry; ISO 75-1/-2 |
| Flammability, UL94 | HB @Thickness 1.50 mm |
HB @Thickness 0.0591 in |
dry; IEC 60695-11-10 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | >= 1.00e+15 ohm-cm | >= 1.00e+15 ohm-cm | dry; IEC 60093 |
| Dielectric Constant | 3.3 @Frequency 1.00e+6 Hz |
3.3 @Frequency 1.00e+6 Hz |
dry; IEC 60250 |
| 3.5 @Frequency 100 Hz |
3.5 @Frequency 100 Hz |
dry; IEC 60250 | |
| Dissipation Factor | 0.0050 @Frequency 100 Hz |
0.0050 @Frequency 100 Hz |
dry; IEC 60250 |
| 0.015 @Frequency 1.00e+6 Hz |
0.015 @Frequency 1.00e+6 Hz |
dry; IEC 60250 | |
| Comparative Tracking Index | 500 V | 500 V | dry; IEC 60112 |