DSM Stanyl® TS250F4D Nylon 46-40% Glass Reinforced (Asian Grade) (Dry)

Category Polymer , Thermoplastic , Nylon , Nylon 46 , Nylon 46, Glass Fiber Reinforced
Manufacturer DSM Engineering Plastics
Trade Name Stanyl®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DSM Stanyl® TS250F4D Nylon 46-40% Glass Reinforced (Asian Grade) (Dry).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temperatures Excellent resistance to wear and low friction Outstanding flow for easy processing and exceptional design freedomStanyl High Flowgrades that match the best flowing LCPs while maintaining a high level of mechanical propertiesKey Applications: Automotive: Powertrain components, Charge-air coolers, EPS and ETC gears, Motor Sensors, Auto connectors, Chain tensionersE&E: Connectors, Microswitches, Bobbins, Memory modules, Motor components, Industrial, Specialty films and fibers, Consumer appliancesInformation provided by DSM.
Physical Properties Metric English Comments
Density 1.56 g/cc
0.0564 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 150 MPa
21800 psi
ISO 527-1/-2
Elongation at Break 2.0 %
2.0 %
ISO 527-1/-2
Tensile Modulus 9.20 GPa
1330 ksi
ISO 527-1/-2
Charpy Impact, Notched 0.800 J/cm²

@Temperature 23.0 °C
3.81 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
0.800 J/cm²

@Temperature -30.0 °C
3.81 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear 30.0 µm/m-°C

@Temperature 20.0 °C
16.7 µin/in-°F

@Temperature 68.0 °F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 80.0 µm/m-°C

@Temperature 20.0 °C
44.4 µin/in-°F

@Temperature 68.0 °F
ISO 11359-1/-2
Melting Point 295 °C
563 °F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 290 °C
554 °F
ISO 75-1/-2
Flammability, UL94 V-0

@Thickness 0.750 mm
V-0

@Thickness 0.0295 in
IEC 60695-11-10