| Category | Polymer , Thermoplastic , Nylon , Nylon 612 , Nylon 612, Glass Fiber Filler |
| Manufacturer | DuPont Performance Polymers |
| Trade Name | Zytel® |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | DuPont Performance Polymers Zytel® 77G43L BK031 Nylon 612
(Unverified Data**).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.42 g/cc | 0.0513 lb/in³ | DAM; ISO 1183 |
| Viscosity | 50400 cP @Shear Rate 5000 1/s, Temperature 300 °C |
50400 cP @Shear Rate 5000 1/s, Temperature 572 °F |
ISO 11403-1 -2 |
| 56700 cP @Shear Rate 5000 1/s, Temperature 290 °C |
56700 cP @Shear Rate 5000 1/s, Temperature 554 °F |
ISO 11403-1 -2 | |
| 58400 cP @Shear Rate 5000 1/s, Temperature 280 °C |
58400 cP @Shear Rate 5000 1/s, Temperature 536 °F |
ISO 11403-1 -2 | |
| 127400 cP @Shear Rate 500 1/s, Temperature 300 °C |
127400 cP @Shear Rate 500 1/s, Temperature 572 °F |
ISO 11403-1 -2 | |
| 140300 cP @Shear Rate 500 1/s, Temperature 290 °C |
140300 cP @Shear Rate 500 1/s, Temperature 554 °F |
ISO 11403-1 -2 | |
| 149600 cP @Shear Rate 500 1/s, Temperature 280 °C |
149600 cP @Shear Rate 500 1/s, Temperature 536 °F |
ISO 11403-1 -2 | |
| Linear Mold Shrinkage, Flow | 0.0030 cm/cm | 0.0030 in/in | DAM; ISO 294-4 2577 |
| Linear Mold Shrinkage, Transverse | 0.0080 cm/cm | 0.0080 in/in | DAM; ISO 294-4 2577 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 200 MPa | 29000 psi | DAM; ISO 527-1/-2 |
| Elongation at Break | 3.0 % | 3.0 % | DAM; ISO 527-1/-2 |
| Tensile Modulus | 12.5 GPa | 1810 ksi | DAM; ISO 527-1/-2 |
| Flexural Modulus | 11.0 GPa | 1600 ksi | DAM; ISO 178 |
| Shear Strength | 0.01727 MPa @Shear Rate 50.0 1/s, Temperature 300 °C |
2.505 psi @Shear Rate 50.0 1/s, Temperature 572 °F |
ISO 11403-1 -2 |
| 0.018485 MPa @Shear Rate 50.0 1/s, Temperature 290 °C |
2.6810 psi @Shear Rate 50.0 1/s, Temperature 554 °F |
ISO 11403-1 -2 | |
| 0.02065 MPa @Shear Rate 50.0 1/s, Temperature 280 °C |
2.995 psi @Shear Rate 50.0 1/s, Temperature 536 °F |
ISO 11403-1 -2 | |
| 0.0637 MPa @Shear Rate 500 1/s, Temperature 300 °C |
9.24 psi @Shear Rate 500 1/s, Temperature 572 °F |
ISO 11403-1 -2 | |
| 0.07015 MPa @Shear Rate 500 1/s, Temperature 290 °C |
10.17 psi @Shear Rate 500 1/s, Temperature 554 °F |
ISO 11403-1 -2 | |
| 0.0748 MPa @Shear Rate 500 1/s, Temperature 280 °C |
10.8 psi @Shear Rate 500 1/s, Temperature 536 °F |
ISO 11403-1 -2 | |
| 0.252 MPa @Shear Rate 5000 1/s, Temperature 300 °C |
36.5 psi @Shear Rate 5000 1/s, Temperature 572 °F |
ISO 11403-1 -2 | |
| 0.2835 MPa @Shear Rate 5000 1/s, Temperature 290 °C |
41.12 psi @Shear Rate 5000 1/s, Temperature 554 °F |
ISO 11403-1 -2 | |
| 0.292 MPa @Shear Rate 5000 1/s, Temperature 280 °C |
42.4 psi @Shear Rate 5000 1/s, Temperature 536 °F |
ISO 11403-1 -2 | |
| Izod Impact, Notched (ISO) | 17.0 kJ/m² | 8.09 ft-lb/in² | DAM; ISO 180/1A |
| 15.0 kJ/m² @Temperature -40.0 °C |
7.14 ft-lb/in² @Temperature -40.0 °F |
DAM; ISO 180/1A | |
| Charpy Impact, Notched | 1.70 J/cm² | 8.09 ft-lb/in² | DAM; ISO 179/1eA |
| 1.60 J/cm² @Temperature -40.0 °C |
7.61 ft-lb/in² @Temperature -40.0 °F |
DAM; ISO 179/1eA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 10.0 µm/m-°C | 5.56 µin/in-°F | DAM; ISO 11359-1/-2 |
| 16.0 µm/m-°C @Temperature 55.0 - 160 °C |
8.89 µin/in-°F @Temperature 131 - 320 °F |
DAM; ISO 11359-1/-2 | |
| 21.0 µm/m-°C @Temperature -40.0 - 23.0 °C |
11.7 µin/in-°F @Temperature -40.0 - 73.4 °F |
DAM; ISO 11359-1/-2 | |
| CTE, linear, Transverse to Flow | 104 µm/m-°C | 57.8 µin/in-°F | DAM; ISO 11359-1/-2 |
| 73.0 µm/m-°C @Temperature -40.0 - 23.0 °C |
40.6 µin/in-°F @Temperature -40.0 - 73.4 °F |
DAM; ISO 11359-1/-2 | |
| Melting Point | 218 °C | 424 °F | DAM; 10°C/min; ISO 11357-1/-3 |
| Deflection Temperature at 0.46 MPa (66 psi) | 217 °C | 423 °F | DAM; ISO 75-1/-2 |
| Deflection Temperature at 1.8 MPa (264 psi) | 205 °C | 401 °F | DAM; ISO 75-1/-2 |
| Flammability, UL94 | HB @Thickness 0.700 mm |
HB @Thickness 0.0276 in |
DAM; IEC 60695-11-10 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Part Marking Code | >PA612-GF43< | ISO 11469 |
| Processing | Injection Moulding | |
| Regional Availability | Asia Pacific | |
| Europe | ||
| Global | ||
| Near East/Africa | ||
| North America | ||
| South and Central America | ||
| Resin Identification | PA612-GF43 | |
| PA612-GF43 | ISO 1043 | |
| UL recognition | UL | DAM |