| Category | Polymer , Thermoplastic , Nylon , Nylon 66 |
| Manufacturer | DuPont Performance Polymers |
| Trade Name | Zytel® |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | DuPont Performance Polymers Zytel® FN714 NC010A Nylon 66.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.02 g/cc | 0.0368 lb/in³ | DAM; ISO 1183 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 29.0 MPa @Temperature 23.0 °C |
4210 psi @Temperature 73.4 °F |
DAM; ISO 527 |
| Tensile Strength, Yield | 29.0 MPa @Temperature 23.0 °C |
4210 psi @Temperature 73.4 °F |
DAM; ISO 527 |
| Elongation at Break | >= 50 % @Temperature 23.0 °C |
>= 50 % @Temperature 73.4 °F |
DAM; nominal; ISO 527 |
| 190 % @Temperature 23.0 °C |
190 % @Temperature 73.4 °F |
DAM; nominal; ISO 527 | |
| 220 % @Temperature 23.0 °C |
220 % @Temperature 73.4 °F |
DAM; ISO 527 | |
| Tensile Modulus | 0.475 GPa @Temperature 23.0 °C |
68.9 ksi @Temperature 73.4 °F |
DAM; ISO 527 |
| Flexural Modulus | 0.575 GPa @Temperature 23.0 °C |
83.4 ksi @Temperature 73.4 °F |
DAM; ISO 178 |
| Izod Impact, Notched (ISO) | NB @Temperature 23.0 °C |
NB @Temperature 73.4 °F |
DAM; ISO 180/1A |
| Charpy Impact, Notched | 9.50 J/cm² @Temperature 23.0 °C |
45.2 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 179/1eA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 263 °C | 505 °F | 10°C/min; DAM; ISO 11357-1/-3 |
| Deflection Temperature at 0.46 MPa (66 psi) | 55.0 °C | 131 °F | DAM; ISO 75-1/-2 |
| Deflection Temperature at 1.8 MPa (264 psi) | 45.0 °C | 113 °F | DAM; ISO 75-1/-2 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 285 °C | 545 °F | DAM; Optimum; Extrusion |
| 285 °C | 545 °F | DAM; Optimum; Injection Molding | |
| 275 - 295 °C | 527 - 563 °F | DAM; Extrusion | |
| 275 - 295 °C | 527 - 563 °F | DAM; Injection Molding | |
| Mold Temperature | 60.0 °C | 140 °F | DAM; optimum; Injection Molding |
| 40.0 - 80.0 °C | 104 - 176 °F | DAM; Injection Molding | |
| Drying Temperature | 80.0 °C | 176 °F | DAM; Extrusion |
| 80.0 °C | 176 °F | DAM; Injection Molding | |
| Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | DAM; Injection Molding |
| 4.00 - 6.00 hour | 4.00 - 6.00 hour | DAM; Extrusion | |
| Moisture Content | <= 0.050 % | <= 0.050 % | DAM; Extrusion |
| <= 0.20 % | <= 0.20 % | DAM; Injection Molding |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Appearance | Natural Color | DAM |
| Features | Chemical Resistance, Good | DAM |
| Chemical Resistance, Good | DAM | |
| Flexibility, Good | DAM | |
| Flexibility, Good | DAM | |
| Heat Aging Resistance, Good | DAM | |
| Heat Aging Resistance, Good | DAM | |
| Impact Modified | DAM | |
| Impact Modified | DAM | |
| Forms | Pellets | DAM |
| Generic | Nylon 66 | DAM |
| Material Status | Current | DAM |
| Part Marking Code | >PA66-F< | ISO 11469; DAM |
| Processing Method | Injection Molding | DAM |
| Product Category | Toughened Resins | DAM |
| Unreinforced Resins | DAM | |
| Region Available - Global | Yes | DAM |
| Resin Identification | PA66-F | ISO 1043; DAM |
| RoHS Compliance | Contact Manufacturer | DAM |