| Category | Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), Unreinforced |
| Manufacturer | |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Eastman 9921 PET Injection Molded
(discontinued **).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.33 g/cc | 1.33 g/cc | ASTM D792 |
| Bulk Density | 0.817 g/cc | 0.0295 lb/in³ | Poured; ASTM D1895 |
| 0.881 g/cc | 0.0318 lb/in³ | Vibrated; ASTM D1895 | |
| Density | 1.33 g/cc | 0.0480 lb/in³ | ISO 1183 |
| 1.40 g/cc | 0.0506 lb/in³ | Crystalline Density; ASTM D1505 | |
| Melt Density | 1.20 g/cc @Temperature 285 °C |
0.0434 lb/in³ @Temperature 545 °F |
ASTM D1238 |
| Particle Size | 2500 µm | 2500 µm | Pellet Size |
| Viscosity Measurement | 0.78 - 0.82 | 0.78 - 0.82 | Pellet, Intrinsic; VGAS-A-AN-G-V-1 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 112 | 112 | ASTM D785 |
| 114 | 114 | ISO 2039-2 | |
| Tensile Strength at Break | 25.0 MPa | 3630 psi | ISO 527 |
| 25.0 MPa | 3630 psi | ASTM D638 | |
| Tensile Strength, Yield | 57.0 MPa | 8270 psi | ISO 527 |
| 58.0 MPa | 8410 psi | ASTM D638 | |
| Elongation at Break | 120 % | 120 % | ISO 527 |
| 120 % | 120 % | ASTM D638 | |
| Tensile Modulus | 2.40 GPa | 348 ksi | ISO 527 |
| 2.40 GPa | 348 ksi | ASTM D638 | |
| Flexural Yield Strength | 77.0 MPa | 11200 psi | ISO 178 |
| 84.0 MPa | 12200 psi | ASTM D790 | |
| Flexural Modulus | 2.30 GPa | 334 ksi | ISO 178 |
| 2.50 GPa | 363 ksi | ASTM D790 | |
| Izod Impact, Notched | 0.270 J/cm @Temperature -40.0 °C |
0.506 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
| 0.400 J/cm @Temperature 23.0 °C |
0.749 ft-lb/in @Temperature 73.4 °F |
ASTM D256 | |
| Izod Impact, Unnotched | NB | NB | ASTM D4812 |
| NB @Temperature -40.0 °C |
NB @Temperature -40.0 °F |
ASTM D4812 | |
| Izod Impact, Notched (ISO) | 3.10 kJ/m² @Temperature -40.0 °C |
1.48 ft-lb/in² @Temperature -40.0 °F |
ISO 180 |
| 4.50 kJ/m² @Temperature 23.0 °C |
2.14 ft-lb/in² @Temperature 73.4 °F |
ISO 180 | |
| Puncture Energy | 0.800 J @Thickness 2.50 mm, Temperature -40.0 °C |
0.590 ft-lb @Thickness 0.0984 in, Temperature -40.0 °F |
max load; ISO 6603-2 |
| 1.00 J @Thickness 3.20 mm, Temperature -40.0 °C |
0.738 ft-lb @Thickness 0.126 in, Temperature -40.0 °F |
max load; ISO 6603-2 | |
| 1.60 J @Thickness 2.50 mm, Temperature -40.0 °C |
1.18 ft-lb @Thickness 0.0984 in, Temperature -40.0 °F |
max load; ASTM D3763 | |
| 2.10 J @Thickness 3.20 mm, Temperature -40.0 °C |
1.55 ft-lb @Thickness 0.126 in, Temperature -40.0 °F |
max load; ASTM D3763 | |
| 15.0 J @Thickness 2.50 mm, Temperature 23.0 °C |
11.1 ft-lb @Thickness 0.0984 in, Temperature 73.4 °F |
max load; ISO 6603-2 | |
| 18.0 J @Thickness 3.20 mm, Temperature 23.0 °C |
13.3 ft-lb @Thickness 0.126 in, Temperature 73.4 °F |
max load; ISO 6603-2 | |
| 26.0 J @Thickness 2.50 mm, Temperature 23.0 °C |
19.2 ft-lb @Thickness 0.0984 in, Temperature 73.4 °F |
max load; ASTM D3763 | |
| 31.0 J @Thickness 3.20 mm, Temperature 23.0 °C |
22.9 ft-lb @Thickness 0.126 in, Temperature 73.4 °F |
max load; ASTM D3763 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Heat of Fusion | 56.0 J/g | 24.1 BTU/lb | ASTM E793 |
| Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | ASTM E1269 |
| 1.30 J/g-°C @Temperature 80.0 °C |
0.311 BTU/lb-°F @Temperature 176 °F |
ASTM E1269 | |
| 1.40 J/g-°C @Temperature 100 °C |
0.335 BTU/lb-°F @Temperature 212 °F |
ASTM E1269 | |
| 1.90 J/g-°C @Temperature 200 °C |
0.454 BTU/lb-°F @Temperature 392 °F |
ASTM E1269 | |
| 2.10 J/g-°C @Temperature 280 °C |
0.502 BTU/lb-°F @Temperature 536 °F |
ASTM E1269 | |
| Melting Point | 240 °C | 464 °F | Crystalline Peak Melting Point; ASTM D3418 |
| Deflection Temperature at 0.46 MPa (66 psi) | 69.0 °C | 156 °F | ISO 75 |
| 69.0 °C | 156 °F | ASTM D648 | |
| Deflection Temperature at 1.8 MPa (264 psi) | 65.0 °C | 149 °F | ASTM D648 |
| 65.0 °C | 149 °F | ISO 75 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Acetaldehyde | <3ppm | VKCA-A-AS-G-GC-0001 |
| Color, CIE a* | -2.5 ± 1.5 | VGAS-A-AN-G-RS-001 |
| Color, CIE b* | 0.3 ± 1.5 | VGAS-A-AN-G-RS-001 |
| Color, CIE L* | 77.5 min | VGAS-A-AN-G-RS-001 |
| Fines, wt%, max | 0.05 | VGAS-A-AN-G-GA-1 |
| Pellet Shape | Cubical |