| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 2.60 g/cc | 2.60 g/cc | 60°C for 1,000 hrs with 90% RH; JIS-K-6220 |
| 2.60 g/cc | 2.60 g/cc | 150°C for 1,000 hrs; JIS-K-6220 | |
| 2.60 g/cc | 2.60 g/cc | JIS-K-6220; ASTM D-792 | |
| 2.60 g/cc | 2.60 g/cc | 70°C for 1,000 hrs; JIS-K-6220 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore C | 20 | 20 | 60°C for 1,000 hrs with 90% RH; SRIS0101 |
| 22 | 22 | 70°C for 1,000 hrs; SRIS0101 | |
| 29 | 29 | 150°C for 1,000 hrs; SRIS0101 | |
| Hardness, Shore OO | 49 | 49 | SRIS0101; ASTM D-2240 |
| Tensile Strength, Yield | 0.300 MPa | 43.5 psi | 150°C for 1,000 hrs; JIS-K-6251(#2) |
| 0.500 MPa | 72.5 psi | JIS-K-6251(#2)/ASTM D-412 | |
| 0.600 MPa | 87.0 psi | 60°C for 1,000 hrs with 90% RH; JIS-K-6251(#2) | |
| 0.900 MPa | 131 psi | 70°C for 1,000 hrs; JIS-K-6251(#2) | |
| Elongation at Yield | 50 % | 50 % | 150°C for 1,000 hrs; JIS-K-6251(#2) |
| 50 % | 50 % | 60°C for 1,000 hrs with 90% RH; JIS-K-6251(#2) | |
| 50 % | 50 % | 70°C for 1,000 hrs; JIS-K-6251(#2) | |
| 60 % | 60 % | JIS-K-6251(#2)/ASTM D-412 | |
| Tear Strength | 1.00 kN/m | 5.71 pli | 150°C for 1,000 hrs; JIS-K-6252 (Angle) |
| 2.00 kN/m | 11.4 pli | 70°C for 1,000 hrs; JIS-K-6252 (Angle) | |
| 2.00 kN/m | 11.4 pli | JIS-K-6252 (Angle)/ASTM D-624 | |
| 2.00 kN/m | 11.4 pli | 60°C for 1,000 hrs with 90% RH; JIS-K-6252 (Angle) |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Thermal Conductivity | 1.50 W/m-K | 10.4 BTU-in/hr-ft²-°F | JIS-R-2618; ASTM D2326 |
| 1.50 W/m-K | 10.4 BTU-in/hr-ft²-°F | 60°C for 1,000 hrs with 90% RH; JIS-R-2618 | |
| 1.50 W/m-K | 10.4 BTU-in/hr-ft²-°F | 70°C for 1,000 hrs; JIS-R-2618 | |
| Maximum Service Temperature, Air | 200 °C | 392 °F | |
| Minimum Service Temperature, Air | -60.0 °C | -76.0 °F |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.10e+13 ohm-cm | 1.10e+13 ohm-cm | 60°C for 1,000 hrs with 90% RH; JIS-K-6249 |
| 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | JIS-K-6249/ASTM D257 | |
| 1.10e+15 ohm-cm | 1.10e+15 ohm-cm | 150°C for 1,000 hrs; JIS-K-6249 | |
| 7.40e+15 ohm-cm | 7.40e+15 ohm-cm | 70°C for 1,000 hrs; JIS-K-6249 | |
| Dielectric Strength | 12.0 kV/mm | 305 kV/in | JIS-K-6249; ASTM D-149 |
| 13.0 kV/mm | 330 kV/in | 150°C for 1,000 hrs; JIS-K-6249 | |
| 15.0 kV/mm | 381 kV/in | 70°C for 1,000 hrs; JIS-K-6249 | |
| 20.0 kV/mm | 508 kV/in | 60°C for 1,000 hrs with 90% RH; JIS-K-6249 | |
| Dielectric Breakdown | 9000 V | 9000 V | Withstand Voltage [V/min]; JIS-K-6249; ASTM D-149 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Color | Dark Grey |