Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Grupo Repol Dinalon® A1S25 G35 H PA66 35% Glass Fiber, Heat Stabilized

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 40% Glass Fiber Filled
Manufacturer Grupo Repol
Trade Name Dinalon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Grupo Repol Dinalon® A1S25 G35 H PA66 35% Glass Fiber, Heat Stabilized.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Mechanical properties for Dry As Molded samplesInformation provided by Grupo Repol
Physical Properties Metric English Comments
Density 1.41 g/cc
0.0509 lb/in³
ISO 1183/A
Moisture Absorption at Equilibrium <= 0.25 %
<= 0.25 %
Karl-Fischer; ISO 15512/A
Mechanical Properties Metric English Comments
Tensile Strength at Break 205 MPa
29700 psi
ISO 527
Elongation at Break 3.2 %
3.2 %
ISO 527
Tensile Modulus 11.0 GPa
1600 ksi
ISO 527
Flexural Strength 260 MPa
37700 psi
ISO 178
Flexural Modulus 7.30 GPa
1060 ksi
ISO 178
Charpy Impact Unnotched 8.00 J/cm²

@Temperature 23.0 °C
38.1 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 1.20 J/cm²

@Temperature 23.0 °C
5.71 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 250 °C
482 °F
ISO 75/A
Vicat Softening Point >= 230 °C
>= 446 °F
50N; ISO 306