| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 9.13 g/cc | 0.330 lb/in³ | at RT |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Brinell | 389 | 389 | Converted from Rockwell C hardness. |
| Hardness, Knoop | 426 | 426 | Converted from Rockwell C hardness. |
| Hardness, Rockwell C | 42 | 42 | |
| Hardness, Vickers | 410 | 410 | Converted from Rockwell C hardness. |
| Tensile Strength, Ultimate | 1335 MPa | 193600 psi | |
| Tensile Strength, Yield | 1040 MPa @Strain 0.200 % |
151000 psi @Strain 0.200 % |
|
| Elongation at Break | 18.2 % | 18.2 % | in 51 mm |
| Modulus of Elasticity | 225 GPa | 32600 ksi | RT |
| 146 GPa @Temperature 1000 °C |
21200 ksi @Temperature 1830 °F |
||
| 154 GPa @Temperature 900 °C |
22300 ksi @Temperature 1650 °F |
||
| 163 GPa @Temperature 800 °C |
23600 ksi @Temperature 1470 °F |
||
| 174 GPa @Temperature 700 °C |
25200 ksi @Temperature 1290 °F |
||
| 181 GPa @Temperature 600 °C |
26300 ksi @Temperature 1110 °F |
||
| 188 GPa @Temperature 500 °C |
27300 ksi @Temperature 932 °F |
||
| 197 GPa @Temperature 400 °C |
28600 ksi @Temperature 752 °F |
||
| 204 GPa @Temperature 300 °C |
29600 ksi @Temperature 572 °F |
||
| 214 GPa @Temperature 200 °C |
31000 ksi @Temperature 392 °F |
||
| 222 GPa @Temperature 100 °C |
32200 ksi @Temperature 212 °F |
||
| Charpy Impact | 262 J | 193 ft-lb | |
| 144 J @Temperature 980 °C |
106 ft-lb @Temperature 1800 °F |
||
| 148 J @Temperature -196 °C |
109 ft-lb @Temperature -321 °F |
||
| 163 J @Temperature 870 °C |
120 ft-lb @Temperature 1600 °F |
||
| 182 J @Temperature -138 °C |
134 ft-lb @Temperature -216 °F |
||
| 194 J @Temperature 760 °C |
143 ft-lb @Temperature 1400 °F |
||
| 212 J @Temperature -78.0 °C |
156 ft-lb @Temperature -108 °F |
||
| 230 J @Temperature 650 °C |
170 ft-lb @Temperature 1200 °F |
||
| 243 J @Temperature -29.0 °C |
179 ft-lb @Temperature -20.2 °F |
||
| 273 J @Temperature 540 °C |
201 ft-lb @Temperature 1000 °F |
||
| 297 J @Temperature 260 °C |
219 ft-lb @Temperature 500 °F |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 12.3 µm/m-°C @Temperature 25.0 - 100 °C |
6.83 µin/in-°F @Temperature 77.0 - 212 °F |
|
| 12.9 µm/m-°C @Temperature 25.0 - 200 °C |
7.17 µin/in-°F @Temperature 77.0 - 392 °F |
||
| 13.6 µm/m-°C @Temperature 25.0 - 300 °C |
7.56 µin/in-°F @Temperature 77.0 - 572 °F |
||
| 14.3 µm/m-°C @Temperature 25.0 - 500 °C |
7.94 µin/in-°F @Temperature 77.0 - 932 °F |
||
| 14.3 µm/m-°C @Temperature 25.0 - 400 °C |
7.94 µin/in-°F @Temperature 77.0 - 752 °F |
||
| 14.6 µm/m-°C @Temperature 25.0 - 600 °C |
8.11 µin/in-°F @Temperature 77.0 - 1110 °F |
||
| 15.1 µm/m-°C @Temperature 25.0 - 700 °C |
8.39 µin/in-°F @Temperature 77.0 - 1290 °F |
||
| 15.8 µm/m-°C @Temperature 25.0 - 800 °C |
8.78 µin/in-°F @Temperature 77.0 - 1470 °F |
||
| 16.5 µm/m-°C @Temperature 25.0 - 900 °C |
9.17 µin/in-°F @Temperature 77.0 - 1650 °F |
||
| 17.0 µm/m-°C @Temperature 25.0 - 1000 °C |
9.44 µin/in-°F @Temperature 77.0 - 1830 °F |
||
| Thermal Conductivity | 9.40 W/m-K | 65.2 BTU-in/hr-ft²-°F | RT |
| 10.9 W/m-K @Temperature 100 °C |
75.6 BTU-in/hr-ft²-°F @Temperature 212 °F |
||
| 12.9 W/m-K @Temperature 200 °C |
89.5 BTU-in/hr-ft²-°F @Temperature 392 °F |
||
| 14.8 W/m-K @Temperature 300 °C |
103 BTU-in/hr-ft²-°F @Temperature 572 °F |
||
| 16.8 W/m-K @Temperature 400 °C |
117 BTU-in/hr-ft²-°F @Temperature 752 °F |
||
| 18.7 W/m-K @Temperature 500 °C |
130 BTU-in/hr-ft²-°F @Temperature 932 °F |
||
| 20.7 W/m-K @Temperature 600 °C |
144 BTU-in/hr-ft²-°F @Temperature 1110 °F |
||
| 22.6 W/m-K @Temperature 700 °C |
157 BTU-in/hr-ft²-°F @Temperature 1290 °F |
||
| 24.7 W/m-K @Temperature 800 °C |
171 BTU-in/hr-ft²-°F @Temperature 1470 °F |
||
| 26.7 W/m-K @Temperature 900 °C |
185 BTU-in/hr-ft²-°F @Temperature 1650 °F |
||
| 29.2 W/m-K @Temperature 1000 °C |
203 BTU-in/hr-ft²-°F @Temperature 1830 °F |
||
| Melting Point | 1330 - 1410 °C | 2430 - 2570 °F | |
| Solidus | 1330 °C | 2430 °F | |
| Liquidus | 1410 °C | 2570 °F |
| Component Elements Properties | Metric | English | Comments |
|---|---|---|---|
| Carbon, C | 0.10 % | 0.10 % | |
| Chromium, Cr | 20 % | 20 % | |
| Cobalt, Co | 51 % | 51 % | |
| Iron, Fe | <= 3.0 % | <= 3.0 % | |
| Manganese, Mn | 1.5 % | 1.5 % | |
| Nickel, Ni | 10 % | 10 % | |
| Silicon, Si | <= 0.40 % | <= 0.40 % | |
| Tungsten, W | 15 % | 15 % |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Electrical Resistivity | 0.0000886 ohm-cm | 0.0000886 ohm-cm | RT |
| 0.0000950 ohm-cm @Temperature 1000 °C |
0.0000950 ohm-cm @Temperature 1830 °F |
||
| 0.0001011 ohm-cm @Temperature 900 °C |
0.0001011 ohm-cm @Temperature 1650 °F |
||
| 0.0001066 ohm-cm @Temperature 700 °C |
0.0001066 ohm-cm @Temperature 1290 °F |
||
| 0.0001078 ohm-cm @Temperature 800 °C |
0.0001078 ohm-cm @Temperature 1470 °F |