| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.14 g/cc | 0.0412 lb/in³ | DIN 53479; ASTM D792 |
| Water Absorption | 1.8 % | 1.8 % | DIN 53475; ASTM D570 |
| Linear Mold Shrinkage | 0.012 - 0.015 cm/cm | 0.012 - 0.015 in/in | ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 120 | 120 | DIN 53505; ASTM D785 |
| Tensile Strength, Ultimate | 73.5 MPa | 10700 psi | DIN 53455; ASTM D638 |
| Elongation at Break | 150 % | 150 % | DIN 53455; ASTM D638 |
| Flexural Yield Strength | 98.1 MPa | 14200 psi | DIN 53455; ASTM D790 |
| Flexural Modulus | 1.96 GPa | 284 ksi | DIN 53452; ASTM D790 |
| Izod Impact, Notched | 0.785 J/cm | 1.47 ft-lb/in | DIN 53453; ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 80.0 µm/m-°C @Temperature 20.0 °C |
44.4 µin/in-°F @Temperature 68.0 °F |
DIN 53752; ASTM D696 |
| Melting Point | 220 °C | 428 °F | DIN 53736; ASTM D789 |
| Deflection Temperature at 0.46 MPa (66 psi) | 180 °C | 356 °F | DIN 53461; ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 65.0 °C | 149 °F | DIN 53461; ASTM D648 |
| Flammability, UL94 | HB | HB |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Transmission, Visible | 90 % | 90 % | transparent; thickness not quantified |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Dielectric Constant | 3.4 @Frequency 1e+6 Hz |
3.4 @Frequency 1e+6 Hz |
ASTM D150/DIN 53483 |
| Dielectric Strength | 20.0 kV/mm | 508 kV/in | ASTM D149/DIN 53481 |
| Arc Resistance | 120 sec | 120 sec | ASTM D495 |