Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Loctite® Gasket Eliminator® 510 Flange Sealant

Category Polymer , Adhesive , Thermoset
Manufacturer Loctite
Trade Name Gasket Eliminator®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Loctite® Gasket Eliminator® 510 Flange Sealant.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Anaerobic GasketingLoctite® 510 High Temperature Rigid Cure Gasket Eliminator® Flange SealantProduct has a temperature range to 400ºF with excellent solvent and chemical resistance. Makes or dresses gaskets in rigid assemblies. Eliminates gasket compression set. Recommended Primer: 7649 (N). UL classified Typical Use: High temperature applications, Excellent solvent resistance
Physical Properties Metric English Comments
Density 1.16 g/cc
0.0419 lb/in³
Viscosity 188000 - 500000 cP
188000 - 500000 cP
Thixotropic
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 204 °C
400 °F
Minimum Service Temperature, Air -53.9 °C
-65.0 °F
Processing Properties Metric English Comments
Cure Time 30.0 - 240 min
0.500 - 4.00 hour
Full Cure; Primed
240 - 1440 min
4.00 - 24.0 hour
Full Cure; Unprimed
Descriptive Properties Value Comments
Color Red
Gap Fill 0.010 in.
Unprimed
0.02 in.
Primed