Circalokâ„¢ 6715 is a two component, medium viscosity, solvent-free silicone which cures at room temperature to an elastomeric, stress-free rubber of outstanding electrical and high temperature properties. It is the ideal product for potting and encapsulating densely packed components and for making flexible molds.All information provided by Lord.
Physical Properties Metric English Comments
Specific Gravity 1.25 g/cc

@Temperature 25.0 °C
1.25 g/cc

@Temperature 77.0 °F
Viscosity 14000 cP

@Temperature 25.0 °C
14000 cP

@Temperature 77.0 °F
Linear Mold Shrinkage 0.0020 cm/cm
0.0020 in/in
Mechanical Properties Metric English Comments
Hardness, Shore A 35
35
Tensile Strength, Yield 1.72 MPa

@Temperature 25.0 °C
250 psi

@Temperature 77.0 °F
Elongation at Yield 160 %
160 %
Tear Strength 4.38 kN/m
25.0 pli
Die B
Thermal Properties Metric English Comments
CTE, linear 1.40 µm/m-°C
0.778 µin/in-°F
Thermal Conductivity 0.346 W/m-K
2.40 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 200 °C
392 °F
Continuous
300 °C
572 °F
Intermittent
Minimum Service Temperature, Air -100 °C
-148 °F
Intermittent
-80.0 °C
-112 °F
Continuous
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm

@Temperature 25.0 °C
1.00e+14 ohm-cm

@Temperature 77.0 °F
Dielectric Constant 3.5

@Temperature 25.0 °C
3.5

@Temperature 77.0 °F
Dielectric Strength 19.7 kV/mm
500 kV/in
Dissipation Factor 0.020

@Frequency 100000 Hz,
Temperature 25.0 °C
0.020

@Frequency 100000 Hz,
Temperature 77.0 °F
Processing Properties Metric English Comments
Shelf Life 6.00 Month
6.00 Month
Descriptive Properties Value Comments
Appearance White