| Category | Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 30% Glass Fiber Filled |
| Manufacturer | NYCOA, Inc. |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | NYCOA 27/330KNF Glass Filled Nylon 6.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.38 g/cc | 0.0499 lb/in³ | ASTM D792 |
| Water Absorption | 0.90 % | 0.90 % | ASTM D570 |
| Linear Mold Shrinkage | 0.015 cm/cm | 0.015 in/in |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 122 | 122 | ASTM D785 |
| Tensile Strength, Yield | 179 MPa | 26000 psi | ASTM D638 |
| Elongation at Break | 3.0 % | 3.0 % | ASTM D638 |
| Flexural Yield Strength | 240 MPa | 34800 psi | ASTM D790 |
| Flexural Modulus | 8.965 GPa | 1300 ksi | ASTM D790 |
| Izod Impact, Notched | 1.23 J/cm | 2.30 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 221 °C | 430 °F | ASTM D789 |
| Deflection Temperature at 1.8 MPa (264 psi) | 208 °C | 406 °F | ASTM D648 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Processing Temperature | 250 °C | 482 °F | |
| Rear Barrel Temperature | 225 °C | 437 °F | |
| Middle Barrel Temperature | 230 °C | 446 °F | |
| Front Barrel Temperature | 250 °C | 482 °F | |
| Nozzle Temperature | 250 °C | 482 °F | |
| Mold Temperature | 80.0 °C | 176 °F | |
| Drying Temperature | 76.0 °C | 169 °F |