FeaturesModified copolymer PP for injection moulding, with the ability of modeling the melt flow rate within the interval 5 - 20 g/10 min. Can be used for simple small as well as for large complicated mouldings. It is stabilized against the impact of UV radiation by the UV stabilizer on the HALS basis. Application: external use for stadium seats with guaranteed operating life of the mechanical and surface properties. Delivered in the full RAL color scale.Application: Injection MouldingInformation Provided by Plastcom spol. s r.o.
Physical Properties Metric English Comments
Density 0.903 g/cc
0.0326 lb/in³
STN 64 0111
Linear Mold Shrinkage 0.022 cm/cm
0.022 in/in
STN 64 0808
Linear Mold Shrinkage, Transverse 0.025 cm/cm
0.025 in/in
STN 64 0808
Melt Flow 5.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
5.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
STN EN ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 25.0 MPa
3630 psi
STN EN ISO 527-2
Elongation at Break 200 %
200 %
STN EN ISO 527-2
Tensile Modulus 1.40 GPa
203 ksi
STN EN ISO 527-2
Flexural Strength 40.0 MPa
5800 psi
STN EN ISO 178
Flexural Modulus 1.10 GPa
160 ksi
STN EN ISO 178
Charpy Impact Unnotched NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
STN EN ISO 179
NB

@Temperature -20.0 °C
NB

@Temperature -4.00 °F
STN EN ISO 179
Charpy Impact, Notched 0.400 J/cm²

@Temperature -20.0 °C
1.90 ft-lb/in²

@Temperature -4.00 °F
STN EN ISO 179
0.700 J/cm²

@Temperature 23.0 °C
3.33 ft-lb/in²

@Temperature 73.4 °F
STN EN ISO 179
Thermal Properties Metric English Comments
Melting Point 150 °C
302 °F
DSC; STN EN ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °C
167 °F
STN EN ISO 75/A
Vicat Softening Point 114 °C
237 °F
B; STN EN ISO 306
Processing Properties Metric English Comments
Melt Temperature 200 - 250 °C
392 - 482 °F
Mold Temperature 30.0 - 50.0 °C
86.0 - 122 °F
Injection Pressure 60.0 - 70.0 MPa
8700 - 10200 psi