| Category | Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 40% Glass Fiber Filler |
| Manufacturer | Polykemi AB |
| Trade Name | POLYfill |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Polykemi AB POLYfill PPH GF35040 D PP, Glass Fiber-Reinforced, Chemically Coupled, Detergent Resistant.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.22 g/cc | 0.0441 lb/in³ | ISO 1183 |
| Filler Content | 40 % | 40 % | ±2%; Polykemi |
| Linear Mold Shrinkage | 0.0020 cm/cm | 0.0020 in/in | With Flow; ISO 2577 |
| 0.0080 cm/cm | 0.0080 in/in | Across Flow; ISO 2577 | |
| Melt Index of Compound | 25 g/10 min @Load 2.16 kg, Temperature 230 °C |
25 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Flexural Strength | <= 146 MPa | <= 21200 psi | ISO 178 |
| Flexural Modulus | 8.50 GPa @Temperature 23.0 °C |
1230 ksi @Temperature 73.4 °F |
ISO 178 |
| Charpy Impact, Notched | 0.600 J/cm² @Temperature 23.0 °C |
2.86 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 1.8 MPa (264 psi) | 147 °C | 297 °F | 120°C/h; ISO 75/1 |
| Flammability, UL94 | HB @Thickness 1.60 mm |
HB @Thickness 0.0630 in |
|
| Glow Wire Test | 750 °C @Thickness 2.00 mm |
1380 °F @Thickness 0.0787 in |
IEC 695-2-1 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 205 - 260 °C | 401 - 500 °F | |
| Mold Temperature | 40.0 - 80.0 °C | 104 - 176 °F | |
| Drying Temperature | 70.0 - 80.0 °C | 158 - 176 °F | |
| Dry Time | 2 - 4 hour | 2 - 4 hour | in circulation dryer |
| 2 - 4 hour | 2 - 4 hour | in desiccant air dryer | |
| Injection Pressure | 40.0 - 110 MPa | 5800 - 16000 psi | |
| Back Pressure | 1.00 - 2.00 MPa | 145 - 290 psi |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Holding Pressure () | 20-40 | % of injection pressure |
| Injection Speed () | High |