| Category | Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Glass Fiber/Solid Lube Filled |
| Manufacturer | Quadrant Engineering Plastics Products |
| Trade Name | Nylatron® |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Quadrant EPP Nylatron® 703 XL Cast, Wear Resistant, Zero 'Stick-Slip' (ASTM Product Data Sheet).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.11 g/cc | 1.11 g/cc | ASTM D792 |
| Water Absorption | 0.47 % | 0.47 % | Immersion, 24hr; ASTM D570(2) |
| Water Absorption at Saturation | 7.0 % | 7.0 % | Immersion; ASTM D570(2) |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell M | 65 | 65 | ASTM D785 |
| Tensile Strength | 62.1 MPa | 9000 psi | ASTM D638 |
| Elongation at Break | 15 % | 15 % | ASTM D638 |
| Tensile Modulus | 2.76 GPa | 400 ksi | ASTM D638 |
| Flexural Strength | 89.6 MPa | 13000 psi | ASTM D790 |
| Flexural Modulus | 2.48 GPa | 360 ksi | ASTM D790 |
| Compressive Strength | 68.9 MPa | 10000 psi | 10% Def.; ASTM D695 |
| Compressive Modulus | 2.48 GPa | 360 ksi | ASTM D695 |
| Izod Impact, Notched | 0.374 J/cm | 0.700 ft-lb/in | ASTM D256 Type A |
| Coefficient of Friction, Dynamic | 0.14 | 0.14 | Dry vs. Steel; QTM55007 |
| K (wear) Factor | 52.4 x 10<sup>-8</sup> mm³/N-M | 26.0 x 10<sup>-10</sup> in³-min/ft-lb-hr | QTM 55010 |
| Limiting Pressure Velocity | 0.596 MPa-m/sec | 17000 psi-ft/min | 4:1 safety factor; QTM 55007 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 88.2 µm/m-°C @Temperature -40.0 - 149 °C |
49.0 µin/in-°F @Temperature -40.0 - 300 °F |
ASTM E831 |
| Melting Point | 216 °C | 420 °F | Crystalline, Peak; ASTM D3418 |
| Maximum Service Temperature, Air | 93.3 °C | 200 °F | Long Term |
| Deflection Temperature at 1.8 MPa (264 psi) | 93.3 °C | 200 °F | ASTM D648 |
| Flammability, UL94 | HB | HB | 1/8 inch (Estimated Rating) |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Surface Resistivity per Square | >= 1.00e+12 ohm | >= 1.00e+12 ohm | EOS/ESD S11.11 |
| Compliance Properties | Metric | English | Comments |
|---|---|---|---|
| 3A-Dairy | No | No | |
| Canada AG | No | No | |
| FDA | No | No | |
| NSF | No | No | |
| USDA | No | No | |
| USP Class VI | No | No |
| Chemical Resistance Properties | Metric | English | Comments |
|---|---|---|---|
| Acids, Strong (pH 1-3) | Unacceptable | Unacceptable | |
| Acids, Weak | Limited | Limited | |
| Alcohols | Limited | Limited | |
| Alkalies, Strong (pH 11-14) | Unacceptable | Unacceptable | |
| Alkalies, Weak | Limited | Limited | |
| Chlorinated Solvents | Limited | Limited | |
| Conductive / Static Dissipative | Yes | Yes | |
| Continuous Sunlight | Limited | Limited | |
| Hot Water / Steam | Limited | Limited | |
| Hydrocarbons - Aliphatic | Acceptable | Acceptable | |
| Hydrocarbons - Aromatic | Acceptable | Acceptable | |
| Inorganic Salt Solutions | Acceptable | Acceptable | |
| Ketones, Esters | Acceptable | Acceptable |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Machinability | 1 | 1-10, 1=Easier to Machine |