SABIC Innovative Plastics LNP STAT-KON RX05488 PA 66

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP STAT-KON
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP STAT-KON RX05488 PA 66.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
LNP STAT-KON* RX05488 is a compound based on Nylon 66 resin containing Carbon Fiber, Flame Retardant, Glass Fiber, PTFE. Added features of this material include: Electrically Conductive.
Physical Properties Metric English Comments
Density 1.70 g/cc
0.0614 lb/in³
ASTM D792
Moisture Absorption 0.320 %
0.320 %
50% RH, 24 hrs; ASTM D570
0.470 %
0.470 %
23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0020 cm/cm

@Time 86400 sec
0.0020 in/in

@Time 24.0 hour
ASTM D955
0.0024 cm/cm

@Time 86400 sec
0.0024 in/in

@Time 24.0 hour
ISO 294
Linear Mold Shrinkage, Transverse 0.0067 cm/cm

@Time 86400 sec
0.0067 in/in

@Time 24.0 hour
ISO 294
0.0070 cm/cm

@Time 86400 sec
0.0070 in/in

@Time 24.0 hour
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 169 MPa
24500 psi
ASTM D638
175 MPa
25400 psi
ISO 527
Elongation at Break 1.6 %
1.6 %
ASTM D638
1.8 %
1.8 %
ISO 527
Tensile Modulus 18.7 GPa
2710 ksi
1 mm/min; ISO 527
24.61 GPa
3569 ksi
50 mm/min; ASTM D638
Flexural Strength 255 MPa
37000 psi
ASTM D790
271 MPa
39300 psi
ISO 178
Flexural Modulus 14.47 GPa
2099 ksi
ASTM D790
17.6 GPa
2550 ksi
ISO 178
Izod Impact, Notched 0.900 J/cm
1.69 ft-lb/in
ASTM D256
Izod Impact, Unnotched 6.46 J/cm
12.1 ft-lb/in
ASTM D4812
Izod Impact, Notched (ISO) 11.0 kJ/m²
5.23 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 44.0 kJ/m²
20.9 ft-lb/in²
80*10*4; ISO 180/1U
Dart Drop, Total Energy 6.00 J
4.43 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
Impact Test 3.00 J
2.21 ft-lb
Multiaxial Impact; ISO 6603
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) >= 240 °C
>= 464 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
242 °C

@Thickness 3.20 mm
468 °F

@Thickness 0.126 in
unannealed; ASTM D648
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
UL 94 by SABIC-IP
Electrical Properties Metric English Comments
Surface Resistance 100 - 1.00e+6 ohm
100 - 1.00e+6 ohm
ASTM D257