| Category | Polymer , Thermoplastic , Acetal (POM) , Acetal Copolymer, Unreinforced |
| Manufacturer | SABIC Innovative Plastics (GE Plastics) |
| Trade Name | LNP Stat-loy |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | SABIC Innovative Plastics LNP STAT-LOY K3000SZ Acetal Copoly.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.32 g/cc | 0.0477 lb/in³ | ASTM D792 |
| 1.33 g/cc | 0.0480 lb/in³ | ISO 1183 | |
| Moisture Absorption | 2.20 % | 2.20 % | 50% RH, 24 hrs; ASTM D570 |
| Linear Mold Shrinkage, Flow | 0.018 cm/cm @Time 86400 sec |
0.018 in/in @Time 24.0 hour |
ASTM D955 |
| 0.0181 cm/cm @Time 86400 sec |
0.0181 in/in @Time 24.0 hour |
ISO 294 | |
| Linear Mold Shrinkage, Transverse | 0.018 cm/cm @Time 86400 sec |
0.018 in/in @Time 24.0 hour |
ASTM D955 |
| 0.0183 cm/cm @Time 86400 sec |
0.0183 in/in @Time 24.0 hour |
ISO 294 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 31.0 MPa | 4500 psi | ASTM D638 |
| 36.0 MPa | 5220 psi | ISO 527 | |
| Tensile Strength, Yield | 41.0 MPa | 5950 psi | ASTM D638 |
| 42.0 MPa | 6090 psi | ISO 527 | |
| Elongation at Break | 49.3 % | 49.3 % | ISO 527 |
| 59.5 % | 59.5 % | ASTM D638 | |
| Elongation at Yield | 13.3 % | 13.3 % | ISO 527 |
| 15.8 % | 15.8 % | ASTM D638 | |
| Tensile Modulus | 1.50 GPa | 218 ksi | 1 mm/min; ISO 527 |
| 1.59 GPa | 231 ksi | 50 mm/min; ASTM D638 | |
| Flexural Strength | 40.0 MPa | 5800 psi | ISO 178 |
| 48.0 MPa | 6960 psi | ASTM D790 | |
| Flexural Modulus | 1.44 GPa | 209 ksi | ASTM D790 |
| 1.50 GPa | 218 ksi | ISO 178 | |
| Izod Impact, Notched | 1.49 J/cm | 2.79 ft-lb/in | ASTM D256 |
| Izod Impact, Unnotched | NB | NB | ASTM D4812 |
| Izod Impact, Notched (ISO) | 15.0 kJ/m² | 7.14 ft-lb/in² | 80*10*4; ISO 180/1A |
| Izod Impact, Unnotched (ISO) | NB | NB | 80*10*4; ISO 180/1U |
| Dart Drop, Total Energy | 29.0 J | 21.4 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
| Impact Test | 17.0 J | 12.5 ft-lb | Multiaxial Impact; ISO 6603 |
| Coefficient of Friction, Dynamic | 0.42 | 0.42 | ASTM D3702 Modified |
| Coefficient of Friction, Static | 0.24 | 0.24 | ASTM D3702 Modified |
| K (wear) Factor | 28.2 x 10<sup>-8</sup> mm³/N-M | 14.0 x 10<sup>-10</sup> in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 130 µm/m-°C @Temperature -40.0 - 40.0 °C |
72.2 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
| 130 µm/m-°C @Temperature -40.0 - 40.0 °C |
72.2 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 | |
| CTE, linear, Transverse to Flow | 133 µm/m-°C @Temperature -40.0 - 40.0 °C |
73.9 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
| 133 µm/m-°C @Temperature -40.0 - 40.0 °C |
73.9 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 | |
| Deflection Temperature at 0.46 MPa (66 psi) | 146 °C @Thickness 3.20 mm |
295 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 67.0 °C @Thickness 3.20 mm |
153 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Surface Resistance | 1.00e+9 - 1.00e+11 ohm | 1.00e+9 - 1.00e+11 ohm | ASTM D257 |