| Category | Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polystyrene (PS) |
| Manufacturer | SABIC Innovative Plastics (GE Plastics) |
| Trade Name | LNP THERMOCOMP |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | SABIC Innovative Plastics LNP THERMOCOMP Noryl_FM4025 PPE+PS.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.29 g/cc | 1.29 g/cc | foam molded; ASTM D792 |
| 1.43 g/cc | 1.43 g/cc | ASTM D792 | |
| Water Absorption | 0.080 % @Time 86400 sec |
0.080 % @Time 24.0 hour |
ASTM D570 |
| Linear Mold Shrinkage, Flow | 0.0015 cm/cm @Thickness 6.40 mm |
0.0015 in/in @Thickness 0.252 in |
SABIC Method |
| Linear Mold Shrinkage, Transverse | 0.0025 cm/cm @Thickness 6.40 mm |
0.0025 in/in @Thickness 0.252 in |
SABIC Method |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell M | 85 | 85 | ASTM D785 |
| Tensile Strength, Yield | 82.0 MPa @Thickness 6.35 mm |
11900 psi @Thickness 0.250 in |
ASTM D638 |
| Elongation at Yield | 1.5 % @Thickness 6.35 mm |
1.5 % @Thickness 0.250 in |
ASTM D638 |
| Flexural Yield Strength | 121 MPa | 17500 psi | 6.4 mm; ASTM D790 |
| Flexural Modulus | 7.92 GPa | 1150 ksi | 6.4 mm; ASTM D790 |
| Poissons Ratio | 0.38 | 0.38 | ASTM E 132 |
| Izod Impact, Notched | 0.690 J/cm @Thickness 6.40 mm |
1.29 ft-lb/in @Thickness 0.252 in |
ASTM D256 |
| Coefficient of Friction, Static | 0.52 | 0.52 | steel; ASTM D1894 |
| 0.55 | 0.55 | self; ASTM D1894 | |
| Taber Abrasion, mg/1000 Cycles | 100 | 100 | CS-17, 1 kg; ASTM D1044 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 23.4 µm/m-°C @Temperature -40.0 - 95.0 °C |
13.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
| CTE, linear, Transverse to Flow | 34.2 µm/m-°C @Temperature -40.0 - 95.0 °C |
19.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
| Deflection Temperature at 0.46 MPa (66 psi) | 118 °C @Thickness 6.40 mm |
244 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 110 °C @Thickness 6.40 mm |
230 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
| UL RTI, Electrical | 50.0 °C | 122 °F | UL 746B |
| UL RTI, Mechanical with Impact | 50.0 °C | 122 °F | UL 746B |
| UL RTI, Mechanical without Impact | 50.0 °C | 122 °F | UL 746B |
| Flammability, UL94 | V-1 @Thickness 2.89 mm |
V-1 @Thickness 0.114 in |
UL 94 |
| V-0 @Thickness 5.00 mm |
V-0 @Thickness 0.197 in |
UL 94 | |
| 5VA @Thickness 2.89 mm |
5VA @Thickness 0.114 in |
UL 94 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+17 ohm-cm | 1.00e+17 ohm-cm | ASTM D257 |
| Surface Resistance | 1.00e+17 ohm | 1.00e+17 ohm | ASTM D257 |
| Arc Resistance | 60 - 120 sec | 60 - 120 sec | Tungsten; ASTM D495 |
| Comparative Tracking Index | 100 - 175 V | 100 - 175 V | UL 746A |
| Hot Wire Ignition, HWI | >= 120 sec | >= 120 sec | UL 746A |
| High Amp Arc Ignition, HAI | 0.00 - 15 arcs | 0.00 - 15 arcs | UL 746A |
| High Voltage Arc-Tracking Rate, HVTR | >= 150 mm/min | >= 5.91 in/min | UL 746A |
| Descriptive Properties | Value | Comments |
|---|---|---|
| FOAM - ELECTRICAL 6.4 mm Wt Reduction | 20% | |
| FOAM - Flame Class Minimum Density | 1.26g/cm^3 | |
| FOAM - IMPACT 6.4 mm Wt Reduction | 10% | |
| FOAM - MECHANICAL 6.4 mm Wt Reduction | 10% | |
| FOAM - PHYSICAL 6.4mm Wt Reduction | 10% | |
| FOAM - THERMAL 6.4mm Wt Reduction | 10% | |
| Weight Reduction | 10% | SABIC Method |