SABIC Innovative Plastics LNP Thermocomp JF002E PES (Asia Pacific)

Category Polymer , Thermoplastic , Polyethersulfone (PES)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP Thermocomp JF002E PES (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
LNP THERMOCOMP* JF002E is a compound based on Polyethersulfone resin containing Glass Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the Asia Pacific region.
Physical Properties Metric English Comments
Density 1.45 g/cc
0.0524 lb/in³
ASTM D 792
Linear Mold Shrinkage, Flow 0.0060 - 0.0080 cm/cm

@Time 86400 sec
0.0060 - 0.0080 in/in

@Time 24.0 hour
ASTM D 955
Linear Mold Shrinkage, Transverse 0.0060 - 0.0080 cm/cm

@Time 86400 sec
0.0060 - 0.0080 in/in

@Time 24.0 hour
ASTM D 955
Mechanical Properties Metric English Comments
Tensile Strength at Break 108 MPa
15700 psi
ASTM D 638
Elongation at Break 3.1 %
3.1 %
ASTM D 638
Flexural Strength 168 MPa
24400 psi
ASTM D 790
Flexural Modulus 4.96 GPa
719 ksi
ASTM D 790
Izod Impact, Notched 0.430 J/cm

@Temperature 23.0 °C
0.806 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Izod Impact, Unnotched 4.16 J/cm

@Temperature 23.0 °C
7.79 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 204 °C

@Thickness 3.20 mm
399 °F

@Thickness 0.126 in
unannealed; ASTM D 648