| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.00 g/cc | 1.00 g/cc | ASTM D792 |
| Water Absorption | 0.060 % @Time 86400 sec |
0.060 % @Time 24.0 hour |
ASTM D570 |
| Linear Mold Shrinkage, Flow | 0.0060 - 0.0080 cm/cm @Thickness 3.20 mm |
0.0060 - 0.0080 in/in @Thickness 0.126 in |
SABIC Method |
| Melt Flow | 43.6 g/10 min @Load 10.0 kg, Temperature 250 °C |
43.6 g/10 min @Load 22.0 lb, Temperature 482 °F |
ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 32.0 MPa | 4640 psi | SABIC - Japan Method |
| Elongation at Break | 16 % | 16 % | SABIC - Japan Method |
| Flexural Strength | 54.0 MPa | 7830 psi | ASTM D790 |
| Flexural Modulus | 2.15 GPa | 312 ksi | ASTM D790 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 68.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
37.8 µin/in-°F @Temperature -22.0 - 86.0 °F |
TMA |
| Deflection Temperature at 1.8 MPa (264 psi) | 95.0 °C @Thickness 6.40 mm |
203 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
| Flammability, UL94 | V-1 @Thickness 5.00 mm |
V-1 @Thickness 0.197 in |
UL 94 |
| 5VA @Thickness 5.00 mm |
5VA @Thickness 0.197 in |
UL 94 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Surface Resistance | 1.00e+17 ohm | 1.00e+17 ohm | ASTM D257 |
| Dielectric Constant | 2.27 @Frequency 100 Hz |
2.27 @Frequency 100 Hz |
ASTM D150 |