| Category | Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polystyrene (PS) |
| Manufacturer | SABIC Innovative Plastics (GE Plastics) |
| Trade Name | Noryl |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | SABIC Innovative Plastics NORYL SE100X PPE+PS.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.10 g/cc | 1.10 g/cc | ASTM D792 |
| Linear Mold Shrinkage, Flow | 0.0050 - 0.0070 cm/cm @Thickness 3.20 mm |
0.0050 - 0.0070 in/in @Thickness 0.126 in |
SABIC Method |
| Linear Mold Shrinkage, Transverse | 0.0050 - 0.0070 cm/cm | 0.0050 - 0.0070 in/in | on Tensile Bar; SABIC Method |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 46.0 MPa | 6670 psi | Type I, 50 mm/min; ASTM D638 |
| Tensile Strength, Yield | 57.0 MPa | 8270 psi | Type I, 50 mm/min; ASTM D638 |
| Elongation at Break | 25 % | 25 % | Type I, 50 mm/min; ASTM D638 |
| Elongation at Yield | 6.5 % | 6.5 % | Type I, 50 mm/min; ASTM D638 |
| Flexural Yield Strength | 82.0 MPa | 11900 psi | 2.6 mm/min, 100 mm span; ASTM D790 |
| Flexural Modulus | 2.30 GPa | 334 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
| Izod Impact, Notched | 2.56 J/cm | 4.80 ft-lb/in | ASTM D256 |
| 0.900 J/cm @Temperature -30.0 °C |
1.69 ft-lb/in @Temperature -22.0 °F |
ASTM D256 | |
| Dart Drop, Total Energy | 40.0 J | 29.5 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
| 16.0 J @Temperature -30.0 °C |
11.8 ft-lb @Temperature -22.0 °F |
Instrumented Impact Energy @ peak; ASTM D3763 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 102 °C @Thickness 6.40 mm |
216 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 92.0 °C @Thickness 6.40 mm |
198 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
| UL RTI, Electrical | 95.0 °C | 203 °F | UL 746B |
| UL RTI, Mechanical with Impact | 80.0 °C | 176 °F | UL 746B |
| UL RTI, Mechanical without Impact | 95.0 °C | 203 °F | UL 746B |
| Flammability, UL94 | V-1 @Thickness 1.47 mm |
V-1 @Thickness 0.0579 in |
UL 94 |
| V-0 @Thickness 5.99 mm |
V-0 @Thickness 0.236 in |
UL 94 | |
| Oxygen Index | 32.5 % | 32.5 % | ASTM D2863 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 3.10e+16 ohm-cm | 3.10e+16 ohm-cm | ASTM D257 |
| Surface Resistance | >= 1.00e+15 ohm | >= 1.00e+15 ohm | ASTM D257 |
| Dielectric Constant | 2.57 @Frequency 1.00e+6 Hz |
2.57 @Frequency 1.00e+6 Hz |
ASTM D150 |
| 2.66 @Frequency 50.0 - 60.0 Hz |
2.66 @Frequency 50.0 - 60.0 Hz |
ASTM D150 | |
| Dielectric Strength | 17.9 kV/mm @Thickness 3.20 mm |
455 kV/in @Thickness 0.126 in |
in oil; ASTM D149 |
| Dissipation Factor | 0.0026 @Frequency 1.00e+6 Hz |
0.0026 @Frequency 1.00e+6 Hz |
ASTM D150 |
| 0.0060 @Frequency 50.0 - 60.0 Hz |
0.0060 @Frequency 50.0 - 60.0 Hz |
ASTM D150 | |
| Arc Resistance | 0.00 - 60 sec | 0.00 - 60 sec | Tungsten; ASTM D495 |
| Comparative Tracking Index | 400 - 600 V | 400 - 600 V | UL 746A |
| High Voltage Arc-Tracking Rate, HVTR | >= 150 mm/min | >= 5.91 in/min | UL 746A |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Radiant Panel Listing | YES | UL Tested |
| UV-light, water exposure/immersion | F1 | UL 746C |