Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Total PS CPDS FT876 Flame Retardant Polystyrene

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Flame Retardant
Manufacturer Total Atofina
Trade Name PS CPDS
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total PS CPDS FT876 Flame Retardant Polystyrene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
POLYSTYRENE (PS) COMPOUND (CPDS) FT876 is a high impact, halogen free flame retardant polystyrene with good thermal stability and processability.Main Characteristics:Bromine and Chlorine free,UL94 V0 @ 2.5 mm,High heat and good thermal and UV stability.Applications: Television covers, Decoders, Hi-Fi, Office automation.Information provided by Total Petrochemicals.
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
ISO 1183
Water Absorption <= 0.10 %
<= 0.10 %
ISO 62
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm
0.0040 - 0.0070 in/in
Melt Flow 3.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
3.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ISO 1133H
Mechanical Properties Metric English Comments
Tensile Strength at Break 40.0 MPa
5800 psi
ISO 527-2
Tensile Strength, Yield 30.0 MPa
4350 psi
ISO 527-2
Elongation at Break 40 %
40 %
ISO 527-2
Flexural Modulus 2.30 GPa
334 ksi
ISO 178
Izod Impact, Notched (ISO) 6.00 kJ/m²
2.86 ft-lb/in²
180/1A
Thermal Properties Metric English Comments
Vicat Softening Point 85.0 °C

@Load 5.10 kg
185 °F

@Load 11.2 lb
50°C per hour; ISO 306B50
Flammability, UL94 V-0

@Thickness 2.50 mm
V-0

@Thickness 0.0984 in
Black and Gray
Processing Properties Metric English Comments
Melt Temperature <= 280 °C
<= 536 °F