Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Victrex® Vicote® F804 Polyetheretherketone (PEEK) Liquid Dispersion

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK)
Manufacturer Victrex
Trade Name Vicote®
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Victrex® Vicote® F804 Polyetheretherketone (PEEK) Liquid Dispersion.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
VICOTE F804 has been specifically formulated to provide a resilient coating with high wear and abrasion resistance on ferrous substrates such as carbon and cast steels. These properties are retained at high temperatures where other coatings would potentially fail. Typical properties are high continuous use temperature of 260°C, excellent wear, abrasion and cut through resistance at these high temperatures combined with excellent chemical and radiation resistance. VICOTE dispersions have a low level of extractables and inherently flame retardant. Contact Victrex for further details.All information provided by Victrex.
Physical Properties Metric English Comments
Storage Temperature 5.00 - 25.0 °C
41.0 - 77.0 °F
Mechanical Properties Metric English Comments
Impact 1.0
1.0
1m, 1kg, Indent 15mm; BS EN ISO 6272, Part 1
Coefficient of Friction 0.53
0.53
µm @ 10 min., Using 100N Load; ASTM G 133
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 260 °C
500 °F
Processing Properties Metric English Comments
Drying Temperature 120 °C
248 °F
overnight before use
150 °C

@Time 10800 sec
302 °F

@Time 3.00 hour
Descriptive Properties Value Comments
Konig Hardness (seconds) 200
ISO 1522