| Category | Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Unreinforced, Flame Retardant |
| Manufacturer | Zhejiang Juner New Materials Co. |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Zhejiang Juner PC-A1-2 Top-Grade Flame Retardant UV-Resistant.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.20 g/cc | 0.0434 lb/in³ | GB/1033 |
| Water Absorption | 0.30 % | 0.30 % | GB/T1034 |
| Linear Mold Shrinkage | 0.0060 cm/cm | 0.0060 in/in | GB/15585 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 58.0 MPa | 8410 psi | GB/1040 |
| Flexural Strength | 89.0 MPa | 12900 psi | GB/9341 |
| Charpy Impact Unnotched | NB | NB | IS0179-1:2000 |
| Charpy Impact, Notched | 6.00 J/cm² | 28.6 ft-lb/in² | IS0179-1:2000 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 1.8 MPa (264 psi) | 125 °C | 257 °F | GB/1634 |
| Flammability, UL94 | V-2 | V-2 | GB/T2408 |
| Glow Wire Test | 850 °C | 1560 °F | < 30 sec; GB/2099.1 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+17 ohm-cm | 1.00e+17 ohm-cm | D257 |
| Comparative Tracking Index | 200 V | 200 V | GB/4207 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Processing Temperature | 250 - 290 °C | 482 - 554 °F | |
| Drying Temperature | 120 °C @Time 14400 sec |
248 °F @Time 4.00 hour |
Chute Hot-Wind |
| 120 °C @Time 21600 sec |
248 °F @Time 6.00 hour |
Horizontal Oven | |
| Injection Pressure | 80.0 - 120 MPa | 11600 - 17400 psi |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Chromatism (?E) | =0.6 | |
| Granule Diameter | Φ3x3-5 | |
| Speed of Shoot, % | 45-90 | |
| Surface Polish | High | |
| Weatherability | Good |