Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.18 - 1.33 g/cc | 0.0426 - 0.0480 lb/in³ | Average value: 1.27 g/cc Grade Count:20 |
Overview of materials for PETG Copolyester This property data is a summary of similar materials in the MatWeb database for the category "PETG Copolyester". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Density | 1.04 - 1.33 g/cc | 0.0376 - 0.0480 lb/in³ | Average value: 1.18 g/cc Grade Count:142 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant". Each property range of values rep.. |
|||
Density | 1.24 - 1.33 g/cc @Temperature 270 - 290 °C |
0.0448 - 0.0480 lb/in³ @Temperature 518 - 554 °F |
Average value: 1.29 g/cc Grade Count:2 |
Overview of materials for Nylon 6, 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. E.. |
|||
Density | 1.11 - 1.33 g/cc | 0.0401 - 0.0480 lb/in³ | Average value: 1.19 g/cc Grade Count:7 |
Overview of materials for Nylon 66 Fiber This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66 Fiber". Each property range of values reported is minimum and maximum values of appropriate Mat.. |
|||
Density | 1.22 - 1.33 g/cc | 0.0441 - 0.0480 lb/in³ | |
Sibur O-40 Compound 239 Polyvinyl Chloride (PVC) Shall correspond to control sample, approved in accordance with the established procedure. Pores, which can be seen by eyes, are not allowed. Plastic shall no burn at stop of worm extruder for a p.. |
|||
Density | 1.29 - 1.33 g/cc | 0.0466 - 0.0480 lb/in³ | ASTM D792 |
Shinkong Synthetic Fibers Shinite® D201K002 PBT, Low Viscosity Information from Shinkong Synthetic Fibers Corp. |
|||
Density | 1.29 - 1.33 g/cc | 0.0466 - 0.0480 lb/in³ | ASTM D792 |
Shinkong Synthetic Fibers Shinite® D201K006 PBT, Medium Viscosity Information from Shinkong Synthetic Fibers Corp. |
|||
Density | 1.29 - 1.33 g/cc | 0.0466 - 0.0480 lb/in³ | ASTM D792 |
Shinkong Synthetic Fibers Shinite® D201K008 PBT, High Viscosity Information from Shinkong Synthetic Fibers Corp. |
|||
Density | 1.29 - 1.33 g/cc | 0.0466 - 0.0480 lb/in³ | ASTM D792 |
Shinkong Synthetic Fibers Shinite® D201K011 PBT, Super Viscosity Information from Shinkong Synthetic Fibers Corp. |
|||
Density | 1.29 - 1.33 g/cc | 0.0466 - 0.0480 lb/in³ | ASTM D792 |
Shinkong Synthetic Fibers Shinite® D201K002 PBT, Low Viscosity Information from Shinkong Synthetic Fibers Corp. |
|||
Density | 1.29 - 1.33 g/cc | 0.0466 - 0.0480 lb/in³ | ASTM D792 |
Shinkong Synthetic Fibers Shinite® D201K006 PBT, Medium Viscosity Information from Shinkong Synthetic Fibers Corp. |
|||
Density | 1.29 - 1.33 g/cc | 0.0466 - 0.0480 lb/in³ | ASTM D792 |
Shinkong Synthetic Fibers Shinite® D201K008 PBT, High Viscosity Information from Shinkong Synthetic Fibers Corp. |
|||
Density | 1.29 - 1.33 g/cc | 0.0466 - 0.0480 lb/in³ | ASTM D792 |
Shinkong Synthetic Fibers Shinite® D201K011 PBT, Super Viscosity Information from Shinkong Synthetic Fibers Corp. |
|||
Density | 1.29 - 1.33 g/cc | 0.0466 - 0.0480 lb/in³ | ISO R 1183 |
Fainplast Compounds CL 8315 Flexible PVC, Sheathing Sheath coaxial TV Cable |
|||
Density | 1.29 - 1.33 g/cc | 0.0466 - 0.0480 lb/in³ | ISO R 1183 |
Fainplast Compounds GS 6530 Flexible PVC, Injection Molding for Footwear Soles |
|||
Density | 1.29 - 1.33 g/cc | 0.0466 - 0.0480 lb/in³ | ISO R 1183 |
Fainplast Compounds GS 9015 Flexible PVC, Injection Molding for Footwear Technical items for soles |
|||
Density | 1.29 - 1.33 g/cc | 0.0466 - 0.0480 lb/in³ | ISO R 1184 |
Fainplast Compounds KL 94 Flexible PVC, Insulation for High Temperatures Lead Free Automotive cables low thickness |
|||
Density | 1.29 - 1.33 g/cc | 0.0466 - 0.0480 lb/in³ | ISO R 1184 |
Fainplast Compounds KL 95 Flexible PVC, Insulation for High Temperatures Lead Free Automotive cables low thickness |
|||
Density | 1.29 - 1.33 g/cc | 0.0466 - 0.0480 lb/in³ | ISO R 1183 |
Fainplast Compounds MRT 168 Medical Rigid PVC, Injection Molding Anti impact connectors |
|||
Density | 1.29 - 1.33 g/cc | 0.0466 - 0.0480 lb/in³ | ISO R 1183 |
Fainplast Compounds MRT 256/G Medical Rigid PVC, Injection Molding Beta and gamma resistant connectors |
|||
Density | 1.29 - 1.33 g/cc | 0.0466 - 0.0480 lb/in³ | ISO R 1183 |
Fainplast Compounds PM 5740 Flexible PVC, Extrusion Gaskets for frames |
|||
Density | 1.29 - 1.33 g/cc | 0.0466 - 0.0480 lb/in³ | ISO R 1184 |
Fainplast Compounds KL 95/3 Flexible PVC, Insulation for High Temperatures Lead Free Operating temperature 90°C |
|||
Density | 1.29 - 1.33 g/cc | 0.0466 - 0.0480 lb/in³ | ISO R 1183 |
Fainplast Compounds PM 5840 Flexible PVC, Extrusion Gaskets for frames |
|||
Density | 1.29 - 1.33 g/cc | 0.0466 - 0.0480 lb/in³ | ISO R 1183 |
Fainplast Compounds PM 8220 Flexible PVC, Lead Free Various profiles |
|||
Density | 1.24 - 1.33 g/cc | 0.0448 - 0.0480 lb/in³ | Average value: 1.29 g/cc Grade Count:24 |
Overview of materials for Polyphenylene Ether, 30% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 30% Glass Filled". Specific grades with glass content between 25% and 34% are inclu.. |
|||
Density | 1.30 - 1.33 g/cc | 0.0470 - 0.0480 lb/in³ | RP-17617 |
Solvay RHODOLINE® 270 Surfactant Description: Polyacid dispersant. Highly versatile, economical and low foam, flat to gloss, ideal for interior application.Identification: ACRYLIC POLYMERCAS: 9003-04-7Available in: North America IR.. |