Material Notes:
Borcell™ ME1244 is a fully formulated compound for chemical foamed telesingles. ME1244 is a medium-density polyethylene compound containing chemical blowing agent. Applications Borcell™ ME1244 is intended for: foam or foam-skin insulation for telephone singles with typical expansion of 35-40%, and dry core and petroleum jelly filled cables. Specifications Borcell™ ME1244 meets the applicable requirements as below when processed using sound extrusion practice and testing procedure: ASTM D1248 Type II, Class A, Category 4, BS 6234: Type 03 EN 50290-2-23 IEC 60708 NF C32-060 ISO 1872-PE, KEHN, 33-D006.Information provided by Borealis AG
Physical Properties Metric English Comments
Density 0.934 g/cc
0.0337 lb/in³
base resin; ISO 1872-2/ISO 1183
0.937 g/cc
0.0339 lb/in³
compound; ISO 1872-2/ISO 1183
Thermal Stress Crack Resistance 1.50 hour

@Temperature 105 °C
1.50 hour

@Temperature 221 °F
IEC 60811-4-2/A
Oxidative Induction Time (OIT) 50 min

@Temperature 200 °C
50 min

@Temperature 392 °F
IEC 60811-4-2/B
Mechanical Properties Metric English Comments
Tensile Strength at Break 11.0 MPa
1600 psi
50mm/min; ISO 527
11.0 MPa
1600 psi
50mm/min, expanded 35% insulation; IEC 60811-1-1
Elongation at Break 500 %
500 %
50mm/min; ISO 527
500 %
500 %
50mm/min, 35% expanded insulation; IEC 60811-1-1
Electrical Properties Metric English Comments
Dielectric Constant 2.31

@Frequency 1.00e+6 Hz
2.31

@Frequency 1.00e+6 Hz
IEC 60250
Dissipation Factor 0.00050

@Frequency 1.00e+6 Hz
0.00050

@Frequency 1.00e+6 Hz
IEC 60250
Processing Properties Metric English Comments
Processing Temperature 100 - 120 °C
212 - 248 °F
conductor preheating temperature
Zone 1 155 °C
311 °F
Zone 2 170 °C
338 °F
Zone 3 185 °C
365 °F
Zone 4 195 °C
383 °F
Die Temperature 195 °C
383 °F
Melt Temperature 195 - 200 °C
383 - 392 °F
Descriptive Properties Value Comments
Petroleum Jelly Absorption (%) 10
IEC 60811-4-2