Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.73 g/cc | 0.0625 lb/in³ | STN 64 0111 |
Plastcom SLOVASTER® B GF 30 FRL 4 Polybutylene Terephthalate, 30% Chemically Coupled Glass Fiber, Bromine Hydrocarbon Flame Retardant FeaturesPBT with the content of 30% chemically coupled glass fiber and flame retardant based on bromine hydrocarbons. Anisotropy of shrinkage enables injection moulding of round, cylindrical or oth.. |
|||
Density | 1.73 g/cc | 0.0625 lb/in³ | ISO 1183 |
DuPont Performance Polymers Rynite® RE19051 BK507 PET
(Unverified Data**) Rynite® RE19051 BK507 is a 40% glass and mineral reinforced, flame retardant, polyethylene terephthalate black resin.Information provided by DuPont Performance Polymers |
|||
Density | 1.73 g/cc | 0.0625 lb/in³ | |
LATI Kelon® B FR H2 CEG/500-V0CT3 PA 6, Glass/Mineral Reinforced, Flame Retardant, Heat Stabilized Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers / Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Low thermal expansion co.. |
|||
Density | 1.73 g/cc | 0.0625 lb/in³ | |
LATI Larpeek 10 G/50 PEEK, 50% Glass Fiber Reinforced Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Density | 1.73 - 1.78 g/cc @Temperature 22.0 - 24.0 °C |
0.0625 - 0.0643 lb/in³ @Temperature 71.6 - 75.2 °F |
|
Shandong Dongyue Shenzhou New Material Co Fluorocarbon Solvent Conformable with: Q/DYS 012-2007Fluorocarbon solvent is a mixture of perfluorocarbon circular ether. It is a colorless transparent liquid, odorless, nontoxic and uninflammable. It is unsoluble in .. |
|||
Density | 1.73 g/cc | 0.0625 lb/in³ | ASTM D 792 |
SABIC Innovative Plastics LNP Thermocomp 2C003 LNP* Thermocomp* 2C003 is a compound based on Ethylene Tetrafluoroethylene Copolymer resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was su.. |
|||
Density | 1.73 - 1.88 g/cc | 0.0626 - 0.0678 lb/in³ | |
Saint-Gobain Chemfab® 1584N PTFE Coated Fiberglass Conveyor Belting Description: General Notes on Saint Gobain Belting Products:Saint Gobain Performance Plastics developed its belting materials for applications that require superior release characteristics, permeabi.. |
|||
Density | 1.73 g/cc | 0.0625 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP Verton OV00A PPS (Asia Pacific) LNP* Verton* OV00A is a compound based on Polyphenylene Sulfide resin containing Long Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Density | 1.73 g/cc | 0.0625 lb/in³ | |
UCAR Carbon UCAR® PGX Pressure Molded Graphite Available in low ash monolithic sizes as large as 73" diameter, Grade PGX has excellent erosion resistance and thermal properties.Typical Applications:Fluidized bed reactors Centrifugal casting mold.. |
|||
Density | 1.73 g/cc | 0.0625 lb/in³ | ASTM D792 |
Plenco 6015 Phenolic, Briquette, Injection Molded PLENCO 06015 is a glass and mineral filled phenolic molding compound offering improved mechanical strength, dimensional stability and excellent electrical properties. 06015 is available in black.Inf.. |
|||
Density | 1.73 g/cc | 0.0625 lb/in³ | ISO 1183 |
Unitika E-RUNG60 PA66, 60% Glass Fiber Reinforced, Conditioned Information provided by Unitika Ltd. |
|||
Density | 1.73 g/cc | 0.0625 lb/in³ | ISO 1183 |
Unitika E-RUNG60 PA66, 60% Glass Fiber Reinforced, Dry Information provided by Unitika Ltd. |
|||
Density | 1.73 g/cc | 0.0625 lb/in³ | ASTM D792 |
Plenco 6343 Phenolic, Granular, Compression Molded PLENCO 06343 is a mica reinforced phenolic molding compound, offering for a low power factor, low electrical losses, and good electrical properties after long exposures to high humidity. UL recogniz.. |
|||
Density | 1.73 g/cc | 0.0625 lb/in³ | |
Trelleborg Emerson & Cuming Eccobond® 2780-45 One-Component High Temperature Performance Epoxy Adhesive Emerson & Cuming 2780-45 Eccobond® One-Component High Temperature Performance Epoxy AdhesiveFilled, pourable, high temperature resistant, epoxy adhesive. Long term resistance to boiling glycol. Exc.. |
|||
Density | 1.73 g/cc | 0.0625 lb/in³ | ISO 1183 |
Eurostar Starflam RF0023E PA66/6, 10% Glass Filled, Injection Molded Starflam RF0023E is a Mineral Flame Retardant, Halogen Free and Phosphorous Free, Glass Fiber Reinforced, Polyamide 66/6 Injection Molding (also known as RF1002Z230EM)Information provided by Polymer.. |
|||
Density | 1.73 g/cc | 0.0625 lb/in³ | |
Dow Saran® 525 PVDC SARAN® 525 barrier polymer, a copolymer of vinylidene chloride and vinyl chloride, designed for sheet coextrusion and forming into rigid plastic barrier containers for food applications. It is supp.. |
|||
Density | 1.73 g/cc | 0.0625 lb/in³ | ISO 1183 |
Eurotec® Tecodur® PB70 GR50 BK002 CA01 PBT/PET, 50% glass fiber reinforced, heat & UV stabilized, natural Information provided by Eurotec® |
|||
Density | 1.73 g/cc | 0.0625 lb/in³ | ISO 1183 |
Eurotec® Tecodur® PB70 GR50 BK009 MX01 PBT/PET, 50% glass fiber reinforced, heat & UV stabilized, improved impact, natural Information provided by Eurotec® |
|||
Density | 1.73 g/cc | 0.0625 lb/in³ | ISO 1183 |
DSM Arnite® AV2 360 S PET-33% Glass Reinforced (European Grade) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |
|||
Density | 1.73 g/cc | 0.0625 lb/in³ | ISO 1183 |
Celanese ZENITE 7244 LCP, 40% Mineral / Glass Reinforced Zenite 7244 is a 40% glasslmineral reinforced liquid crystal polymer resin with a high heat deflection temperature of 295C, high flow and good flatness."Information provided by Celanese |
|||
Density | 1.73 g/cc | 0.0625 lb/in³ | ISO 1183 |
Celanese Zenite® 7244 BK010 LCP Zenite® 7244 BK010 is a 40% glass/mineral reinforced liquid crystal polymer resin with a high heat deflection temperature of 295°C, high flow and good flatness.Celenese acquired the Zenite product.. |
|||
Density | 1.73 g/cc | 0.0625 lb/in³ | |
A. Schulman ComAlloy Hiloy® 435 Glass/Mineral Reinforced, PBT Alloy Data provided by the manufacturer, ComAlloy International Company.50% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Density | 1.73 g/cc | 0.0625 lb/in³ | ISO 1183 |
Celanese CoolPoly® D5112 Thermally Conductive Polyphenylene Sulfide CoolPoly D series of thermally conductive plastics transfers heat, a characteristic previously unavailable in injection molding grade polymers. CoolPoly is lightweight, netshape moldable and allows .. |
|||
Density | 1.73 g/cc | 0.0625 lb/in³ | |
A. Schulman ComAlloy Voloy® 681 Nylon 6/6, Glass Fiber/Bead Reinforced, Nylon 6/6 Alloy, Flame Retardant, UL Data provided by the manufacturer, ComAlloy International Company.45% Glass Fiber/Bead Reinforced. Halogen- and phosphorous-freeThe ComAlloy product line has been integrated into the A Schulman prod.. |
|||
Density | 1.73 g/cc | 0.0625 lb/in³ | ASTM D792 |
Sumitomo Bakelite North America FS-80-P-1 Long-Glass Reinforced Diallyl Phthalate Isophthalate DAP Resin Isomer. Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type GI.. |
|||
Density | 1.73 g/cc | 0.0625 lb/in³ | ASTM D792 |
Sumitomo Bakelite North America RX® 1-501AN Mineral Filled Diallyl Phthalate Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Information provided by Sumitomo Bakelite North A.. |
|||
Density | 1.73 g/cc | 0.0625 lb/in³ | ISO 1183 |
Sumitomo Bakelite North America RX® 790 Fiberglass Reinforced Phenolic Novolac RX® 790 is a fiberglass reinforced phenolic novolac compound, featuring a good balance of strength and toughness. Information supplied by Sumitomo Bakelite North America. |
|||
Density | 1.73 g/cc | 0.0625 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP Verton OV00A PPS LNP* Verton* OV00A is a compound based on Polyphenylene Sulfide resin containing Long Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Density | 1.73 g/cc | 0.0625 lb/in³ | ISO 1183 |
BASF Ultradur® B 4300 G10 50% Glass Filled PBT Description: Injection-molding grades containing 50% of glass fibers, for industrial parts, rigid, tough and dimensionally stable, for example for program switches, thermostat parts, small-motor hou.. |
|||
Density | 1.73 g/cc | 0.0625 lb/in³ | ISO 1183 |
Hexion Bakelite™ PF 1142 Phenolic Formaldehyde Resin, High Mechanical Strength
(discontinued **) Phenolic molding compound, inorganically filled, glass fiber reinforced, high dimensional stability, good mechanical properties.Application areas: Insulating flanges, sealings, pulleys.Information p.. |