Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.73 g/cc | 0.0625 lb/in³ | ISO 1183 |
DuPont Performance Polymers Rynite® RE19051 BK507 PET
(Unverified Data**) Rynite® RE19051 BK507 is a 40% glass and mineral reinforced, flame retardant, polyethylene terephthalate black resin.Information provided by DuPont Performance Polymers |
|||
Density | 1.73 g/cc | 0.0625 lb/in³ | ASTM D792 |
Plenco 50045 PET, Pellet, Injection Molded, Black
(discontinued **) PLENCO 50045 is an engineering grade glass reinforced polyethylene terephthalate resin designed for higher physical strength. It is UL listed and available in white, natural, and black.Information s.. |
|||
Density | 1.73 g/cc | 0.0625 lb/in³ | ISO 1183 |
Celanese ZENITE 7244 LCP, 40% Mineral / Glass Reinforced
(Unverified Data**) Zenite 7244 is a 40% glass mineral reinforced liquid crystal polymer resin with a high heat deflection temperature of 295C, high flow and good flatness."Information provided by Celanese |
|||
Density | 1.73 g/cc | 0.0625 lb/in³ | |
LATI Kelon® B FR H2 CEG/500-V0CT3 PA 6, Glass/Mineral Reinforced, Flame Retardant, Heat Stabilized Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers / Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Low thermal expansion co.. |
|||
Density | 1.73 g/cc | 0.0625 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP 2X98703 ETFE LNP* THERMOCOMP* 2X98703 is a compound based on ETFE Copolymer resin containint Proprietary Filler(s). |
|||
Density | 1.73 g/cc | 0.0625 lb/in³ | ASTM D 792 |
SABIC Innovative Plastics LNP Thermocomp 2C003 LNP* Thermocomp* 2C003 is a compound based on Ethylene Tetrafluoroethylene Copolymer resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was su.. |
|||
Density | 1.73 g/cc | 0.0625 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP 2C003 ETFE LNP* THERMOCOMP* 2C003 is a compound based on ETFE resin containing 15% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Density | 1.73 g/cc | 0.0625 lb/in³ | ASTM D792 |
Sumitomo Bakelite North America 2-530 Short-Glass Reinforced Diallyl Phthalate Isophthalate DAP Resin Isomer. Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Information provided by Sumitomo Bakelite Nor.. |
|||
Density | 1.73 g/cc | 0.0625 lb/in³ | ASTM D792 |
Sumitomo Bakelite North America E 7459A Long Glass Fiber Reinforced Epoxy EM 7459A is a medium strength fiberglass reinforced epoxy molding compound, which features enhanced impact strength and toughness.Information provided by Sumitomo Bakelite North America, Inc. |
|||
Density | 1.73 g/cc | 0.0625 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP Verton OV00A PPS (Asia Pacific) LNP* Verton* OV00A is a compound based on Polyphenylene Sulfide resin containing Long Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Density | 1.73 g/cc | 0.0625 lb/in³ | |
UCAR Carbon UCAR® PGX Pressure Molded Graphite Available in low ash monolithic sizes as large as 73" diameter, Grade PGX has excellent erosion resistance and thermal properties.Typical Applications:Fluidized bed reactors Centrifugal casting mold.. |
|||
Density | 1.73 g/cc | 0.0625 lb/in³ | ASTM D792 |
Plenco 6015 Phenolic, Briquette, Injection Molded PLENCO 06015 is a glass and mineral filled phenolic molding compound offering improved mechanical strength, dimensional stability and excellent electrical properties. 06015 is available in black.Inf.. |
|||
Density | 1.73 g/cc | 0.0625 lb/in³ | ISO 1183 |
Unitika E-RUNG60 PA66, 60% Glass Fiber Reinforced, Conditioned Information provided by Unitika Ltd. |
|||
Density | 1.73 g/cc | 0.0625 lb/in³ | ASTM D792 |
Unitika E-RUNG60 Ultra high-rigidity PA6, Conditioned Ultra high-rigidityInformation provided by Unitika Ltd. |
|||
Density | 1.73 g/cc | 0.0625 lb/in³ | ASTM D792 |
Tipco Tipcolite® THD 121 Phenolic Compound, Wood Flour, having Medium Flow & High Strength Medium Flow Phenolic Compound, Reinforced with Wood FlourApplications: Electrical & ElectronicsProcessing: Compression MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India... |
|||
Density | 1.73 g/cc | 0.0625 lb/in³ | ASTM D792 |
Plenco 6401 Phenolic, Briquette, Injection Molded PLENCO 06401 is a glass fiber and mineral filled two-stage phenolic molding compound. UL recognized under component file E40654. 06401 is available in black.Information supplied by Plenco. |
|||
Density | 1.73 g/cc | 0.0625 lb/in³ | ISO 1183 |
Polyplastics Duranex® 702MS Polybutylene Terephthalate (PBT), Higher gloss, Better surface appearance, GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Density | 1.73 g/cc | 0.0625 lb/in³ | |
Trelleborg Emerson & Cuming Eccobond® 2780-45 One-Component High Temperature Performance Epoxy Adhesive Emerson & Cuming 2780-45 Eccobond® One-Component High Temperature Performance Epoxy AdhesiveFilled, pourable, high temperature resistant, epoxy adhesive. Long term resistance to boiling glycol. Exc.. |
|||
Density | 1.73 g/cc | 0.0625 lb/in³ | ISO 1183 |
DuPont Performance Polymers Rynite® RE19051 BK507 Polyethylene Terephthalate (PET) 40% Glass/Mineral Reinforced Flame Retardant Polyethylene Terephthalate Rynite RE19051 BK507 is a 40% glass and mineral reinforced flame retardant polyethylene terephthalate black resin.Information .. |
|||
Density | 1.73 g/cc | 0.0625 lb/in³ | ISO 1183 |
Eurostar Starflam RF0023E PA66/6, 10% Glass Filled, Injection Molded Starflam RF0023E is a Mineral Flame Retardant, Halogen Free and Phosphorous Free, Glass Fiber Reinforced, Polyamide 66/6 Injection Molding (also known as RF1002Z230EM)Information provided by Polymer.. |
|||
Density | 1.73 g/cc | 0.0625 lb/in³ | ISO 1183 |
Eurotec® Tecodur® PB70 GR50 BK002 CA01 PBT/PET, 50% glass fiber reinforced, heat & UV stabilized, natural Information provided by Eurotec® |
|||
Density | 1.73 g/cc | 0.0625 lb/in³ | ISO 1183 |
Eurotec® Tecodur® PB70 GR50 BK009 MX01 PBT/PET, 50% glass fiber reinforced, heat & UV stabilized, improved impact, natural Information provided by Eurotec® |
|||
Density | 1.73 g/cc | 0.0625 lb/in³ | ISO 1183 |
BASF Ultradur B 4040 G10 BK5110 50% Glass Filled PBT Injection-molding grades containing 50% of glass fibers, for industrial parts with excellent surface quality.Applications: External door handles in vehicles, visible sunroof frames, over door handle.. |
|||
Density | 1.73 g/cc | 0.0625 lb/in³ | ISO 1183 |
Celanese ZENITE 7244 LCP, 40% Mineral / Glass Reinforced Zenite 7244 is a 40% glasslmineral reinforced liquid crystal polymer resin with a high heat deflection temperature of 295C, high flow and good flatness."Information provided by Celanese |
|||
Density | 1.73 g/cc | 0.0625 lb/in³ | ISO 1183 |
Celanese Zenite® 7244 BK010 LCP Zenite® 7244 BK010 is a 40% glass/mineral reinforced liquid crystal polymer resin with a high heat deflection temperature of 295°C, high flow and good flatness.Celenese acquired the Zenite product.. |
|||
Density | 1.73 g/cc | 0.0625 lb/in³ | ISO 1183 |
Celanese CoolPoly® D5112 Thermally Conductive Polyphenylene Sulfide CoolPoly D series of thermally conductive plastics transfers heat, a characteristic previously unavailable in injection molding grade polymers. CoolPoly is lightweight, netshape moldable and allows .. |
|||
Density | 1.73 g/cc | 0.0625 lb/in³ | |
A. Schulman ComAlloy Voloy® 681 Nylon 6/6, Glass Fiber/Bead Reinforced, Nylon 6/6 Alloy, Flame Retardant, UL Data provided by the manufacturer, ComAlloy International Company.45% Glass Fiber/Bead Reinforced. Halogen- and phosphorous-freeThe ComAlloy product line has been integrated into the A Schulman prod.. |
|||
Density | 1.73 g/cc | 0.0625 lb/in³ | ISO 1183 |
Celanese Impet® 340R PET, 45% Glass Reinforced
(Unverified Data**) Impet 340R is a 45% glass-reinforced injection moldable polyester made with post consumer recycled PET. It provides an excellent combination of strength, stiffness, and high temperature resistance.4.. |
|||
Density | 1.73 g/cc | 0.0625 lb/in³ | ASTM D792 |
Plenco 50130 PET, Pellet, Injection Molded, Black
(discontinued **) PLENCO 50130 is an engineering grade glass reinforced UL flame rated polyethylene terephthalate resin designed for good physical strength. It is UL listed and available in natural and black.Informat.. |
|||
Density | 1.73 g/cc | 0.0625 lb/in³ | ISO 1183 |
Sumitomo Bakelite North America RX® 790 Fiberglass Reinforced Phenolic Novolac RX® 790 is a fiberglass reinforced phenolic novolac compound, featuring a good balance of strength and toughness. Information supplied by Sumitomo Bakelite North America. |