Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plenco 6500 Phenolic, Briquette, Transfer Molded

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic , Phenolic, Novolac, Glass/Flock Filled
Manufacturer Plenco (Plastics Engineering Company)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 6500 Phenolic, Briquette, Transfer Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLENCO 06500 is a glass reinforced phenolic molding compound offering improved strength, dimensional stability, and excellent electrical properties. UL recognized under component file E40654. 06500 is available in black.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.700 g/cc
0.0253 lb/in³
ASTM D1895
Density 1.76 g/cc
0.0636 lb/in³
ASTM D792
Water Absorption 0.101 %
0.101 %
ASTM D570
Linear Mold Shrinkage 0.00116 cm/cm
0.00116 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 99
99
ASTM D785
Tensile Strength, Ultimate 92.0 MPa
13300 psi
ASTM D638
Elongation at Break 0.85 %
0.85 %
ASTM D638
Tensile Modulus 14.3 GPa
2070 ksi
ASTM D638
Flexural Strength 145 MPa
21000 psi
ASTM D790
Flexural Modulus 14.5 GPa
2100 ksi
ASTM D790
Compressive Strength 243 MPa
35200 psi
ASTM D695
Poissons Ratio 0.31
0.31
ASTM D638
Shear Modulus 5.46 GPa
792 ksi
Calculated
Izod Impact, Notched 0.380 J/cm
0.712 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.370 J/cm²
1.76 ft-lb/in²
ASTM D256
Impact 230
230
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
CTE, linear 35.0 µm/m-°C

@Temperature 40.0 - 130 °C
19.4 µin/in-°F

@Temperature 104 - 266 °F
TMA; ASTM E831
Maximum Service Temperature, Air 196 °C
385 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 224 °C
435 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 3.00 mm
V-0

@Thickness 0.118 in
Oxygen Index 35 %
35 %
ASTM D2863
Shrinkage 0.043 %
0.043 %
72 hr, 120ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 6.60e+11 ohm-cm
6.60e+11 ohm-cm
ASTM D247
Dielectric Constant 5.1
5.1
ASTM D150
Dielectric Strength 17.1 kV/mm
434 kV/in
Short Time; ASTM D149
Dissipation Factor 0.033
0.033
ASTM D150
Arc Resistance 136 sec
136 sec
ASTM D495
Comparative Tracking Index 175 V
175 V
ASTM D3638