Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 1.79 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 1.79 g/cc
0.0647 lb/in³
ISO 1183-1
Murtfeldt Murinyl® Polyvinylidinefluoride
As a fluorinated plastic, Murinyl® is exceptionally resistant to chemicals, hydrolysis, and sterilization. Its properties change very little at high service temperatures and after long-term exposur..
Density 1.79 g/cc
0.0647 lb/in³
ASTM D792
SABIC Innovative Plastics LNP KONDUIT PX11313 PA 6 (Asia Pacific)
Thermally conductive mineral filled PA6 FR compounding
Density 1.79 g/cc
0.0647 lb/in³
ASTM D792
Plenco 50240 PET, Pellet, Injection Molded, Natural Color  (discontinued **)
PLENCO 50240 is an engineering grade glass reinforced UL flame rated polyethylene terephthalate resin designed for excellent dimensional stability. It is UL listed and available in natural and black..
Density 1.79 g/cc
0.0647 lb/in³
ASTM D792
Plenco 51240 PET, Pellet, Injection Molded, Black  (discontinued **)
PLENCO 51240 is an engineering grade glass reinforced flame retarded recycled polyethylene terephthalate resin designed for excellent dimensional stability. It is UL listed.Information supplied by P..
Density 1.79 g/cc
0.0647 lb/in³
ISO 1183
SABIC Innovative Plastics LNP LUBRICOMP WFL369 PBT (Europe-Africa-Middle East)
LNP* LUBRICOMP* WFL369 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, PTFE. Added features include: Flame Retardant, Internally Lubricated.
Density 1.79 g/cc

@Temperature 25.0 °C
0.0647 lb/in³

@Temperature 77.0 °F
Solvay Specialty Polymers Galden® LS200 PFPE VPS Fluid
Galden® LS and HS grades are specifically recommended for vapor phase soldering.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of servic..
Density 1.79 g/cc
0.0647 lb/in³
ASTM D792
Techmer ES HiFill® TPX-PVDF-03009 C
Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral FillerFeatures: Low Shrinkage and Low Smoke EmissionInformation provided by TP Composites, Inc.
Density 1.79 g/cc
0.0647 lb/in³
ASTM D792
Sumitomo Bakelite North America 4064 Mineral Filled Electrical Encapsulation Grade Epoxy
Rogers electrical encapsulation grade epoxy is recommended for capacitors, resistors, gold lead encapsulation, relays, coils and bobbins.Information provided by Sumitomo Bak North America, Inc.
Density 1.79 g/cc
0.0647 lb/in³
ASTM D792
Techmer ES HiFill® PA6/6 GF70 HS L BK 70% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 70% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedUL File N..
Density 1.79 g/cc
0.0647 lb/in³
ASTM D792
Sumitomo Bakelite North America 52-40-40-P Long-Glass Reinforced Diallyl Phthalate
Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type GDI-30F..
Density 1.79 g/cc
0.0647 lb/in³
Cosmic Plastics 6220 Short Glass Fiber Filled Iso Diallyl Phthalate Molding Compound
Data provided by the manufacturer.
Density 1.79 g/cc
0.0647 lb/in³
Cosmic Plastics 6220F Short Glass Fiber Filled Iso Diallyl Phthalate Molding Compound
Data provided by the manufacturer.
Density 1.79 g/cc
0.0647 lb/in³
ISO 1183
Vyncolit Neopreg Kinel® SK80 L8G Glass Fiber Reinforced Molding Compound
Epoxy based molding compound long glass fiber reinforced with excellent long term property retention over a wide temperature range and climate conditions. It is particularly suited for over mold..
Density 1.79 g/cc
0.0647 lb/in³
ASTM D792
Tipco Tipcolite® VASW 200 Phenolic Compound, Long Glass Fiber, in fluffy form, Medium -Soft Flow & Very High Strength
Density 1.79 g/cc
0.0647 lb/in³
Toho Tenax Besfight® G30-700 24K HTA-7D F402 Continuous Filament Carbon Fiber
Standard Modulus; Wide Band; Polyacrylonitrile (PAN) based fiberTypical values; measured by Toho Strand Test Method based on JIS R7601 for fiber selection purposes. Information provided by Toho Carb..
Density 1.79 g/cc
0.0647 lb/in³
Toho Tenax Besfight® G40-800 12K IMA5C EP03 Continuous Filament Carbon Fiber
Intermediate Modulus; Collimated; Polyacrylonitrile (PAN) based fiberTypical values; measured by Toho Strand Test Method based on JIS R7601 for fiber selection purposes. Information provided by Toho..
Density 1.79 g/cc
0.0647 lb/in³
Toho Tenax Besfight® G40-800 24K IMA5C EP03 Continuous Filament Carbon Fiber
Intermediate Modulus; Collimated; Polyacrylonitrile (PAN) based fiberTypical values; measured by Toho Strand Test Method based on JIS R7601 for fiber selection purposes. Information provided by Toho..
Density 1.79 g/cc
0.0647 lb/in³
Toho Tenax Besfight® G40-800 6K IMA-5C EP03 Continuous Filament Carbon Fiber
Intermediate Modulus; Collimated; Polyacrylonitrile (PAN) based fiberTypical values; measured by Toho Strand Test Method based on JIS R7601 for fiber selection purposes. Information provided by Toho..
Density 1.79 g/cc
0.0647 lb/in³
Hexcel® AS4D Carbon Fiber (12,000 Filaments)
Weight/length = 0.765 g/m.Information provided by Hexcel Corporation. Values are typical average lot properties.Continuous fiber can be combined with virtually all thermoset and thermoplastic resin..
Density 1.79 g/cc
0.0647 lb/in³
Fibre
Hexcel® HexPly® M48 180°C/356°F Curing Epoxy Matrix, M48/35%/150/IM7 GS
Fiber: IM7 GS, UD, 150 g/m2Information provided by HexCel
Density 1.79 g/cc
0.0647 lb/in³
Hexcel® IM9 Carbon Fiber (12,000 Filaments)
Weight/length = 0.331 g/m.Information provided by Hexcel Corporation. Values are typical average lot properties.Continuous fiber can be combined with virtually all thermoset and thermoplastic resin..
Density 1.79 g/cc
0.0647 lb/in³
Hexcel® AS4 Carbon Fiber (12,000 Filaments)
Weight/length = 0.858 g/m.Information provided by Hexcel Corporation. Values are typical average lot properties.Continuous fiber can be combined with virtually all thermoset and thermoplastic resin..
Density 1.79 g/cc
0.0647 lb/in³
Hexcel® AS4 Carbon Fiber (3000 Filaments)
Weight/length = 0.210 g/m.Information provided by Hexcel Corporation. Values are typical average lot properties.Continuous fiber can be combined with virtually all thermoset and thermoplastic resin..
Density 1.79 g/cc
0.0647 lb/in³
ISO 1183
DuPont Performance Polymers Rynite® FR543 NC010 PET
Rynite® FR543 NC010 is a flame retardant, 43% glass reinforced polyethylene terephthalate. Has a 155C temperature index that is equivalent to many thermosets. Recognized by UL as UL94V-0 at 0.8mm..
Density 1.79 g/cc

@Temperature -40.0 °C
0.0647 lb/in³

@Temperature -40.0 °F
3M Novec™ 649 Engineered Fluid
3M™ Novec™ 649 Engineered Fluid is a clear, colorless and low odor fluid, one in a line of 3M products designed as replacements for ozone depleting substances (ODSs) and compounds with high global..
Density 1.79 g/cc
0.0647 lb/in³
ASTM D792
Plenco 50240 PET, Pellet, Injection Molded, Black  (discontinued **)
PLENCO 50240 is an engineering grade glass reinforced UL flame rated polyethylene terephthalate resin designed for excellent dimensional stability. It is UL listed and available in natural and black..
Density 1.79 g/cc
0.0647 lb/in³
ASTM D792
Plenco 50240 PET, Pellet, Injection Molded, Green  (discontinued **)
PLENCO 50240 is an engineering grade glass reinforced UL flame rated polyethylene terephthalate resin designed for excellent dimensional stability. It is UL listed and available in natural and black..
Density 1.79 - 1.99 g/cc
0.0647 - 0.0719 lb/in³
Molded
Bulk Molding Compounds BMC T15(GPS) General Purpose Molding Compound
BMC T15(GPS) is a high strength, low shrink general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T15(GPS) is well suited for injection, transfer or compression..
Copyright © lookpolymers.com All Rights Reserved