Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total Lumicene® MR30MX0 Metallocene Random Copolymer Polypropylene, Injection Molding and Injection Blow Molding Lumicene® MR30MX0 is a metallocene random copolymer with a melt flow index of 30 g/10 min for injection and injection stretch blow molding. Lumicene® MR30MX0 differs from the other random copolyme.. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total Lumicene® MR60MC2 Metallocene Random Copolymer Polypropylene, Injection Molding Lumicene® MR60MC2 is a metallocene random copolymer with a melt flow index of 60 g/10 min for injection molding. Lumicene® MR60MC2 differs from standard random copolymers by its molding reproducib.. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPC 10642 Polypropylene, Heterophasic Copolymer, Injection Molding Polypropylene PPC 10642 is a nucleated antistatic heterophasic copolymer with high Melt Flow index of 44 g/10 min.Polypropylene PPC 10642 is characterized by high fluidity with good mechanical prope.. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPC 11712 Polypropylene, Heterophasic Copolymer ATOFINA Propylene 11712 is a nucleated controlled-rheology heterophasic copolymer. PPC 11712 is characterized by good stiffness and impact resistance as well as low shrinkage and low warpage. It h.. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPC 7810 Polypropylene, Heterophasic Copolymer, High Impact Polypropylene PPC 7810 is a very high impact heterophasic copolymer with a Melt Flow index of 15 g/10 min.Polypropylene PPC 7810 has been specially developed for high impact and heavy duty applicati.. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPC 8780 Polypropylene, Heterophasic Copolymer, Injection Molding Polypropylene PPC 8780 is a controlled rheology heterophasic copolymer with a Melt Flow index of 18 g/10 min.Polypropylene PPC 8780 has been specially developed for the injection molding of lids com.. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPC 9612 Polypropylene, Heterophasic Copolymer, Injection Molding This product is a Total Ecosolutions grade.Polypropylene PPC 9612 has been developed specifically for the injection molding of crates and is characterized by a high Melt Flow index of 20 g/10 min. .. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPC 9642 Polypropylene, Heterophasic Copolymer ATOFINA Propylene 9642 is nucleated heterophasic copolymer. PPC 9642 is characterized by improved stiffness, creep resistance, high impact resistance, excellent antistatic properties and has been f.. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPH 10042 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 10042 is a nucleated antistatic homopolymer. PPH 10042 is characterized by high fluidity for high speed injection of thin wall articles such as dairy pots and tubs, salad .. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPH 3060 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 3060 is homopolymer.ApplicationATOFINA Polypropylene PPH 3060 is characterized by a low fluidity for continuous extrusion of strapping, rope fibers and high tenacity tapes .. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPH 3150 Polypropylene, Homopolymer Polypropylene PPH 3150 is a modified homopolymer polypropylene with a Melt Flow index of 2 g/10 min.Polypropylene PPH 3150 is intended for the production at very high speed of flat bioriented films .. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPH 4022 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 4022 is a clarified nucleated homopolymer.ApplicationATOFINA Polypropylene PPH 4022 has been developed for extrusion-thermoforming, providing improved rigidity and impact r.. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPH 4042 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 4042 is a nucleated homopolymer.ApplicationATOFINA Polypropylene PPH 4042 has been developed for extrusion-thermoforming, providing improved rigidity and impact resistance .. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPH 4054 Polypropylene Homopolymer Polypropylene PPH 4054 is a homopolymer polypropylene with a Melt Flow index of 3 g/10 min.Polypropylene PPH 4054 has been designed for the production of BOPP film with the tenter frame process. Th.. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPH 4060 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 4060 is homopolymer.ApplicationATOFINA Polypropylene PPH 4060 is specially suitable for tape extrusion for woven applications and for extrusion thermoforming. PPH 4060 is.. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPH 5069 Polypropylene Homopolymer, Fiber Polypropylene PPH 5069 is a homopolymer polypropylene with a Melt Flow index of 6 g/10 min.Polypropylene PPH 5069 is intended for extrusion of high tenacity staple fibers for non-woven applications... |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPH 7059 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 7059 is homopolymer.ApplicationATOFINA Polypropylene PPH 7059 is intended for extrusion of staple fibers for non-woven applications. It exhibits excellent spinning propert.. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPH 7069 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 7069 is homopolymer.ApplicationATOFINA Polypropylene PPH 7069 is characterized by medium fluidity for extrusion of continuous filament (CF) and bulk continuous filament (BC.. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPH 9059 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 9059 is homopolymer.ApplicationATOFINA Polypropylene PPH 9059 is intended for extrusion of bulk continuous filament (BCF) and continuous filament (CF) fibers. PPH 9059 has.. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPH 9069 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 9069 is homopolymer.ApplicationATOFINA Polypropylene PPH 9069 is intended for applications in non-wovens. It is also suitable for extrusion of bulk continuous filament (BC.. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPH 9081 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 9081 is a controlled-rheology homopolymer. PPH 9081 is characterized by a narrow molecular weight distribution and excellent flow properties, providing improved impact res.. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPH 9099 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 9099 is a very narrow molecular weight distribution homopolymer polypropylene, with anti gas-fading stabilization. ApplicationATOFINA Polypropylene PPH 9099 is intended for.. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPM H350 Polypropylene, Homopolymer Medical Grade Polypropylene PPM H350 is a homopolymer with a Melt Flow Index of 35 g/10 min recommended for the manufacture of medical packaging and medical devices, to the exclusion of implants.Polypropylene PPM.. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPC 12712 Polypropylene, Heterophasic Copolymer ATOFINA Propylene 12712 is a nucleated controlled-rheology heterophasic copolymer. PPC 12712 is characterized by good stiffness and impact resistance as well as low shrinkage and low warpage. It h.. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPC 13442 Polypropylene, Heterophasic Copolymer ATOFINA Propylene 13442 is a nucleated antistatic heterophasic copolymer. PPC 13442 is characterized by very high fluidity with good mechanical properties. It has been formulated for excellent ant.. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPC 13812 Polypropylene, Heterophasic Copolymer, Injection Molding Polypropylene PPC 13812 is a high fluidity heterophasic copolymer resin with fast nucleation.Polypropylene PPC 13812 is characterized by good stiffness and impact resistance as well as low shrinkage.. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPC 1640 Polypropylene, Heterophasic Copolymer, Non-pressure Pipes Polypropylene PPC 1640 is a nucleated heterophasic (block) copolymer with a Melt Flow index of 0.3 g/10 min. This resin has a long-term heat stabilization package. It exhibits high stiffness in co.. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPC 3150 MX5 Polypropylene, Heterophasic Copolymer, Automotive Polypropylene PPC 3150 MX5 is a high crystallinity and high impact polypropylene (HCPP) copolymer with a Melt Flow index of 15 g/10 min. The material is UV stabilized.Polypropylene PPC 3150 MX5 is .. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPC 3645 Polypropylene, Heterophasic Copolymer ATOFINA Polypropylene PPC 3645 is a nucleated heterophasic copolymer. PPC 3645 is characterized by improved stiffness, creep resistance and high impact resistance.ApplicationPPC 3645 has been devel.. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPC 3120 MU5 Polypropylene, Heterophasic Copolymer, Automotive Polypropylene PPC 3120 MU5 is a heterophasic copolymer with a Melt Flow index of 15 g/10 min. Polypropylene PPC 3120 MU5 is a high impact copolymer formulated to give good UV resistance.Polypropyle.. |