Material Notes:
KT Cast is a coarse-grained, white firing kaolin that is used primarily in casting bodies based on its fast casting and exceptional deflocculation characteristics.Information provided by Imerys
Physical Properties Metric English Comments
Particle Size 0.50 µm
0.50 µm
21% finer than
1.0 µm
1.0 µm
41% finer than
2.0 µm
2.0 µm
60% finer than
5.0 µm
5.0 µm
75% finer than
10 µm
10 µm
87% finer than
20 µm
20 µm
95% finer than
Particle Mesh Size 325 Mesh
325 Mesh
5.0% retained
pH 5.5
5.5
Specific Surface Area 12 m²/g
12 m²/g
Mechanical Properties Metric English Comments
Modulus of Rupture 0.00155 GPa
0.225 ksi
dry
Component Elements Properties Metric English Comments
Al2O3 38.8 %
38.8 %
CaO 0.10 %
0.10 %
Carbon, C 0.030 %
0.030 %
Fe2O3 0.40 %
0.40 %
K2O 0.10 %
0.10 %
Loss on Ignition(%) 13.6 %
13.6 %
MgO 0.10 %
0.10 %
Na2O 0.10 %
0.10 %
SiO2 45.1 %
45.1 %
Sulfur, S 0.030 %
0.030 %
TiO2 1.6 %
1.6 %
Descriptive Properties Value Comments
M.B.I. (meq/100g) 2.5