Material Notes:
TOTAL Petrochemicals Polypropylene 4820WZ is a nucleated impact copolymer with a Melt Flow index of 35 g/10 min.TOTAL Polypropylene 4820WZ is characterized by improved stiffness, creep resistance, high impact resistance, excellent antistatic properties and has been formulated to allow faster cycling through early demolding.Total Polypropylene 4820WZ has been developed specifically for the injection molding of garden furniture, housewares, thin-walled articles and compounding.Information provided by Total Petrochemicals.
Physical Properties Metric English Comments
Specific Gravity 0.905 g/cc
0.905 g/cc
ASTM D1505
Melt Flow 35 g/10 min
35 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 27.0 MPa
3920 psi
ASTM D638
Elongation at Yield 6.0 %
6.0 %
ASTM D638
Flexural Modulus 1.38 GPa
200 ksi
ASTM D790
Izod Impact, Notched 0.370 J/cm

@Temperature -20.0 °C
0.693 ft-lb/in

@Temperature -4.00 °F
ASTM D256
0.800 J/cm

@Temperature 23.0 °C
1.50 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Charpy Impact, Notched 0.450 J/cm²

@Temperature -20.0 °C
2.14 ft-lb/in²

@Temperature -4.00 °F
DIN 53453
0.950 J/cm²

@Temperature 23.0 °C
4.52 ft-lb/in²

@Temperature 73.4 °F
DIN 53453
Thermal Properties Metric English Comments
Melting Point 160 - 165 °C
320 - 329 °F
TOTAL Method
Deflection Temperature at 0.46 MPa (66 psi) 100 °C
212 °F
Pressure unspecified; ASTM D648
Vicat Softening Point 150 °C
302 °F
ASTM D1525