Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.65 g/cc | 1.65 g/cc | ASTM D-792 |
PlastiComp Complet® LGF50-PPA Polyphthalamide, 50% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polyphthalamide with 50% long glass fiber reinforcementInformation provided by PlastiC.. |
|||
Specific Gravity | 1.65 g/cc | 1.65 g/cc | ASTM D792 |
Ovation Polymers RIGITRON 20443 GF PBT, 43% Glass Reinforced PBT - Glass reinforced (43 %), high tensile strength, stiffness and HDT. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All samples are prepared acco.. |
|||
Specific Gravity | 1.65 - 2.15 g/cc | 1.65 - 2.15 g/cc | ASTM D792 |
Parker Chomerics CHO-SEAL 1350 Conductive Elastomer Standard material for high volume injection and compression molding and small extrusions; high performance in non-corrosive environments; used in grounding applications with little or no vibration.R.. |
|||
Specific Gravity | 1.65 - 2.15 g/cc | 1.65 - 2.15 g/cc | |
Parker Chomerics CHO-SEAL S6304 Conductive Elastomer Conductive Elastomer EMI/EMP GasketsInformation provided by Chomerics |
|||
Specific Gravity | 1.65 g/cc | 1.65 g/cc | ASTM D792 |
DuPont Performance Polymers Rynite® RE15022 NC010 PET
(Unverified Data**) Rynite® RE15022 NC010 is a 36% glass reinforced product designed for applications that need high burst strength.Information provided by DuPont Performance Polymers |
|||
Specific Gravity | 1.65 g/cc | 1.65 g/cc | ASTM D 792 |
RTP Company RTP 4087 A FR (Hot Water Moldable) Polyphthalamide (PPA), Carbon Fiber - Flame Retardant |
|||
Specific Gravity | 1.65 g/cc | 1.65 g/cc | Method A; ASTM D792 |
LNP Thermocomp® UF-1006 FR HS LEX BK8-115 Polyphthalamide, Glass Fiber Reinforcement
(discontinued **) Features: Heat Stabilized, Flame RetardantForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many L.. |
|||
Specific Gravity | 1.65 g/cc | 1.65 g/cc | ASTM D 792 |
RTP Company RTP 805 CC TFE 5 Acetal (POM), Glass Fiber Reinforced - PTFE Lubricated |
|||
Specific Gravity | 1.65 g/cc | 1.65 g/cc | ASTM D792 |
RTP Company RTP 205G FR Nylon 4/6 (PA 4/6) Glass Fiber 30% - Flame Retardant
(discontinued Glass Fiber 30% - Flame RetardantComments:Glass FiberFlame Retardant(Dry As Molded)Unless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properti.. |
|||
Specific Gravity | 1.65 g/cc | 1.65 g/cc | ASTM D297 |
Greene Tweed FLUORAZ® 799 Fluoroelastomer, FEPM Greene, Tweed`s Fluoraz® functions effortlessly in a variety of challenging process environments. Fluoraz performs well in aggressive chemicals where ultrapure materials are not required. Known f.. |
|||
Specific Gravity | 1.65 g/cc | 1.65 g/cc | Part A |
Lord Adhesives Circalokâ„¢ 6009 A/B Flame Retardant Epoxy Encapsulant Circalokâ„¢ 6009 A/B is a two component epoxy resin system which has moderate thermal conductivity and low viscosity. Circalokâ„¢ 6009 A/B meets UL 94V-0 specification for flame retardance.All.. |
|||
Specific Gravity | 1.65 g/cc @Temperature 25.0 °C |
1.65 g/cc @Temperature 77.0 °F |
STM 2 |
Lord Adhesives Thermosetâ„¢ EP-830 Ignition Coil Impregnating and Encapsulation Epoxy Lord EP-830 is a heat curing, two component epoxy formulation designed especially for use in automotive high voltage ignition coils where adhesion to segmented bobbins is critical. The combination o.. |
|||
Specific Gravity | 1.65 - 1.70 g/cc | 1.65 - 1.70 g/cc | ASTM D792 |
Loxim 230 01V0 Polybutylene Terephthalate Information provided by Loxim Industries |
|||
Specific Gravity | 1.65 g/cc | 1.65 g/cc | ASTM D792 |
SABIC Innovative Plastics Valox® IQ4860HR PBT (Asia Pacific) Valox iQ* Resin iQ4860HR: Environmentally responsible iQ* PBT resin with 30% Glass reinforcement + UL94 V-0. Hydrolytically stable and impact modified. |
|||
Specific Gravity | 1.65 g/cc | 1.65 g/cc | ASTM D792 |
Saint-Gobain Meldin® 3140 Thermoplastic Bearing Material Meldin 3140 is an ideal thrust washer material and is well suited for thrust washer applications. Its high strength and stiffness, combined with its excellent heat dissipation properties, make it a.. |
|||
Specific Gravity | 1.65 g/cc | 1.65 g/cc | ASTM D792 |
Samsung Cheil Industries Infino® VB-5302GR PBT, 30% Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
Specific Gravity | 1.65 g/cc | 1.65 g/cc | ASTM D 792 |
RTP Company ESD C 1305 Polyphenylene Sulfide (PPS), Glass Fiber - ESD Protection - Electrically Conductive |
|||
Specific Gravity | 1.65 g/cc | 1.65 g/cc | ASTM D 792 |
RTP Company RTP 1305 TFE 10 Polyphenylene Sulfide (PPS); Glass Fiber - PTFE Lubricated |
|||
Specific Gravity | 1.65 g/cc | 1.65 g/cc | ASTM D 792 |
RTP Company RTP 205 A FR UV Nylon 6 (PA), Glass Fiber - Flame Retardant - UV Stabilized - UL94 V-0 |
|||
Specific Gravity | 1.65 g/cc | 1.65 g/cc | ASTM D792 |
Colorite Polymers CS7566LS Wire and Cable Jacket Vinyl Compound Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai.. |
|||
Specific Gravity | 1.65 g/cc | 1.65 g/cc | ASTM D792 |
Celanese Celanex® 3314 PBT, 30% Glass Reinforced Celanex 3314 is a non-exuding (UL approved V-0 at 1/64 inch), 30% fiberglass reinforced polybutylene terephthalate which has an excellent balance of mechanical properties and processability. It is w.. |
|||
Specific Gravity | 1.65 g/cc | 1.65 g/cc | |
Aremco Aremco-Bond™ 657 High Performance Epoxide Stainless Steel-Filled, High Corrosion Resistance. |
|||
Specific Gravity | 1.65 - 1.80 g/cc | 1.65 - 1.80 g/cc | ISO 1183 |
Raschig Group DECAL® 152CL Phenolic Glass-fiber and mineral reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and mechanical properties. This product meet.. |
|||
Specific Gravity | 1.65 g/cc | 1.65 g/cc | ASTM D 792 |
RTP Company RTP 4405 FR High Temperature Nylon (HTN), Glass Fiber - Flame Retardant |
|||
Specific Gravity | 1.65 g/cc | 1.65 g/cc | ASTM D 792 |
RTP Company RTP 804 TFE 10 Acetal (POM), Glass Fiber - PTFE Lubricated |
|||
Specific Gravity | 1.65 g/cc | 1.65 g/cc | ASTM D792 |
RTP Company RTP 2205 TFE 15 Polyetheretherketone (PEEK) Glass Fiber 30% - PTFE 15%
(discon Glass Fiber 30% - PTFE 15%Comments:Glass FiberPTFE LubricatedUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provide.. |
|||
Specific Gravity | 1.65 g/cc | 1.65 g/cc | ASTM D 792 |
RTP Company RTP PA66 30 GF FR0 BLK Nylon 6/6 (PA), Value Product - Glass Fiber - Flame Retardant - Non-PBDE/PBB - UL94 |
|||
Specific Gravity | 1.65 g/cc | 1.65 g/cc | ASTM D 792 |
RTP Company RTP PA66 30 GF FR0 NAT Nylon 6/6 (PA), Value Product - Glass Fiber - Flame Retardant - Non-PBDE/PBB - UL94 |
|||
Specific Gravity | 1.65 g/cc | 1.65 g/cc | ASTM D 792 |
RTP Company VLF 84009 Polyphthalamide (PPA), Long Glass Fiber - Heat Stabilized |