Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.65 g/cc | 1.65 g/cc | ASTM D-792 |
PlastiComp Complet® LGF50-PPA Polyphthalamide, 50% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polyphthalamide with 50% long glass fiber reinforcementInformation provided by PlastiC.. |
|||
Specific Gravity | 1.65 g/cc | 1.65 g/cc | ASTM D297 |
Process Technologies Inc Sanifluor® 1000 Formulated Aflas® Elastomer O-Rings, Gaskets and Seals produced from Sanifluor® 1000 have excellent chemical, heat and steam resistance. They provide superior performance in hot water, steam and virtually all caustics; makin.. |
|||
Specific Gravity | 1.65 - 1.85 g/cc | 1.65 - 1.85 g/cc | ISO 1183 |
Raschig Group DECAL® 666/8 Phenolic Glass-fiber reinforced phenolic molding compound with mineral fillers. High heat resistance, reduced mould shrinkage and post-shrinkage, good chemical resistance and mechanical properties. This prod.. |
|||
Specific Gravity | 1.65 g/cc | 1.65 g/cc | Method A; ASTM D792 |
LNP Lubricomp® OFL-4536 Polyphenylene Sulfide, Glass Fiber Reinforced, PTFE Lubricant
(discontinued **) Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |
|||
Specific Gravity | 1.65 g/cc | 1.65 g/cc | ASTM D 792 |
RTP Company RTP 4007 TFE 15 Polyphthalamide (PPA), Glass Fiber - PTFE Lubricated |
|||
Specific Gravity | 1.65 g/cc | 1.65 g/cc | ASTM D792 |
DuPont Performance Polymers Rynite® RE15022 NC010 PET
(Unverified Data**) Rynite® RE15022 NC010 is a 36% glass reinforced product designed for applications that need high burst strength.Information provided by DuPont Performance Polymers |
|||
Specific Gravity | 1.65 g/cc | 1.65 g/cc | Method A; ASTM D792 |
LNP Thermocomp® UF-1006 FR HS LEX BK8-115 Polyphthalamide, Glass Fiber Reinforcement
(discontinued **) Features: Heat Stabilized, Flame RetardantForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many L.. |
|||
Specific Gravity | 1.65 g/cc | 1.65 g/cc | ASTM D792 |
Solvay Specialty Polymers AvaSpire® AV-750 GF40 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-750 GF40 is a 40% glass reinforced polyaryletherketone (PAEK) designed to fill the marketplace need for a lower-priced PEEK (polyetheretherketone). This resin provides the typical chemic.. |
|||
Specific Gravity | 1.65 g/cc | 1.65 g/cc | ASTM D 792 |
RTP Company RTP 805 TFE 5 SI 2 Acetal (POM), Glass Fiber - PTFE Lubricated - Silicone Lubricated |
|||
Specific Gravity | 1.65 - 2.15 g/cc | 1.65 - 2.15 g/cc | ASTM D792 |
Parker Chomerics CHO-SEAL® 6307 Conductive Elastomer Description: Good performance in moderately corrosive environments; excellent NBC fluid resistance; good physical properties.Molded onlyRoHS CompliantInformation provided by Chomerics |
|||
Specific Gravity | 1.65 g/cc | 1.65 g/cc | ASTM D792 |
RTP Company RTP 205G FR Nylon 4/6 (PA 4/6) Glass Fiber 30% - Flame Retardant
(discontinued Glass Fiber 30% - Flame RetardantComments:Glass FiberFlame Retardant(Dry As Molded)Unless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properti.. |
|||
Specific Gravity | 1.65 g/cc | 1.65 g/cc | ASTM D792 |
PolyOne Therma-Tech™ NJ-6000C TC Nylon 12
(discontinued **) Therma-Tech™ Thermal Management Compounds have been engineered to combine the heat transfer and cooling capabilities of metals with the design freedom, weight reduction and cost advantages of therm.. |
|||
Specific Gravity | 1.65 g/cc | 1.65 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 1850/GF/30/TF/15/BK PBT, with glass fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
Specific Gravity | 1.65 g/cc | 1.65 g/cc | ASTM D792 |
LG Chemical LUSEP GP2400 PPS+GF40%, General Purpose Feature: Injection Molding, PPS+GF40%, General PurposeApplication: Pump Units, Motor Units, etc.CAS No. 25212-74-2 and 65997-17-3Information provided by LG Chemical |
|||
Specific Gravity | 1.65 g/cc | 1.65 g/cc | ASTM D297 |
Greene Tweed FLUORAZ® 799 Fluoroelastomer, FEPM Greene, Tweed`s Fluoraz® functions effortlessly in a variety of challenging process environments. Fluoraz performs well in aggressive chemicals where ultrapure materials are not required. Known f.. |
|||
Specific Gravity | 1.65 g/cc | 1.65 g/cc | ASTM D297 |
Greene Tweed FLUORAZ® 890 Fluoroelastomer, FEPM Sanitary gaskets made from Fluoraz® 890 are ideal for use in standard SIP and CIP applications where EPDMs and FKMs fail. While EDPMs and FKMs can provide a deal for extended periods, changes in.. |
|||
Specific Gravity | 1.65 - 1.70 g/cc | 1.65 - 1.70 g/cc | ASTM D792 |
Loxim 230 01V0 Polybutylene Terephthalate Information provided by Loxim Industries |
|||
Specific Gravity | 1.65 g/cc | 1.65 g/cc | ASTM D792 |
SABIC Innovative Plastics Valox® IQ4860HR PBT (Asia Pacific) Valox iQ* Resin iQ4860HR: Environmentally responsible iQ* PBT resin with 30% Glass reinforcement + UL94 V-0. Hydrolytically stable and impact modified. |
|||
Specific Gravity | 1.65 g/cc | 1.65 g/cc | |
Silberline EternaBrite® Premier 255 EternaBrite® Premier 255 is a fine, very bright, leafing aluminum pigment with excellent opacity and distinctness of image (D.O.I) for solvent based general industrial coatings. This product is s.. |
|||
Specific Gravity | 1.65 g/cc | 1.65 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP UF00ASW PPA LNP* Thermocomp* UF00ASW is a compound based on Polyphthalamide (PPA) containing glass fiber. Characteristics of this grade of Heat Stabilized and Hot Water Moldable. |
|||
Specific Gravity | 1.65 g/cc | 1.65 g/cc | ASTM D 792 |
RTP Company ESD C 1305 Polyphenylene Sulfide (PPS), Glass Fiber - ESD Protection - Electrically Conductive |
|||
Specific Gravity | 1.65 g/cc | 1.65 g/cc | ASTM D 792 |
RTP Company RTP 205 D FR Nylon 6/12 (PA), Glass Fiber - Flame Retardant - UL94 V-0 |
|||
Specific Gravity | 1.65 g/cc | 1.65 g/cc | ASTM D792 |
DuPont Performance Polymers Rynite® RE15022 NC010 Polyethylene Terephthalate (PET) 36% Glass Reinforced Polyethylene TerephthalateRynite RE15022 NC010 is a 36% glass reinforced product designed for applications that need high burst strength.Information provided by DuPont Performan.. |
|||
Specific Gravity | 1.65 g/cc | 1.65 g/cc | Part A |
Epoxy Technology EPO-TEK® T905BN-3 Thermally Conductive Epoxy Product Description: EPO-TEK® T905BN-3 is a thermally conductive, electrically insulating epoxy designed for heat sinking and encapsulation. Advantages & Application Notes: Potting applications:Lo.. |
|||
Specific Gravity | 1.65 g/cc | 1.65 g/cc | ASTM D792 |
Celanese Celanex® 3318 PBT, 30% Glass Reinforced Celanex 3318 is a non-exuding (UL approved V-0 at 1/64 inch), 30% fiberglass reinforced polybutylene terephthalate which has an excellent balance of mechanical properties and processability. It is w.. |
|||
Specific Gravity | 1.65 g/cc | 1.65 g/cc | ASTM D792 |
RTP Company RTP 4299 X 93109 Thermoplastic Polyimide (TPI) Electronic Encapsulation
(disc Electronic EncapsulationComments:Encapsulation GradeUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP .. |
|||
Specific Gravity | 1.65 g/cc | 1.65 g/cc | ASTM D793 |
Saint-Gobain Meldin® 1277 Thermoplastic Bearing Material Meldin 1277 has structural integrity and low deformation. This material also exhibits good electrical insulative properties and dimensional stability.Meldin® 1000 series components are used in app.. |
|||
Specific Gravity | 1.65 g/cc | 1.65 g/cc | ASTM D 792 |
RTP Company RTP 4405 FR High Temperature Nylon (HTN), Glass Fiber - Flame Retardant |
|||
Specific Gravity | 1.65 g/cc | 1.65 g/cc | ASTM D 792 |
RTP Company VLF 84707 Polytrimethylene Terephthalate (PTT), Long Glass Fiber
(discontinued **) Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade. |
|||
Specific Gravity | 1.65 g/cc | 1.65 g/cc | ASTM D 792 |
RTP Company RTP PA66 30 GF FR0 NAT Nylon 6/6 (PA), Value Product - Glass Fiber - Flame Retardant - Non-PBDE/PBB - UL94 |