Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

CENTROPLAST CENTROLAB HT Polypropylene Higher Temperatures

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Extrusion Grade
Manufacturer CENTROPLAST Engineering Plastics GMBH
Trade Name CENTROLAB
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CENTROPLAST CENTROLAB HT Polypropylene Higher Temperatures.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PP-HT is a semi-crystalline plastic, with high acid and chemical resistance and mechanical strength. Due to its high resistance to temperature, PP-HT-plastics are often used in medical technology as sterilization boxes or for analysis devices. The BfR-/FDA approval, as well as the conformity in accordance with USP Class VI provide physiological safety. PP-HT is available in white.Information provided by CENTROPLAST Engineering Plastics GMBH
Physical Properties Metric English Comments
Density 0.930 g/cc
0.0336 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength 33.0 MPa
4790 psi
50 mm/min; ISO 527-2
Elongation at Break 25 %
25 %
ISO 527-2
Tensile Modulus 1.40 GPa
203 ksi
ISO 527-2
Flexural Modulus 1.15 GPa
167 ksi
ISO 178
Charpy Impact Unnotched 0.800 J/cm²
3.81 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 0.600 J/cm²
2.86 ft-lb/in²
ISO 179/IeA
Thermal Properties Metric English Comments
CTE, linear 86.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
47.8 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359
Melting Point 166 °C
331 °F
DSC, 10 K/m; ISO 3146
Maximum Service Temperature, Air 105 °C
221 °F
continuous
140 °C
284 °F
short term
Deflection Temperature at 0.46 MPa (66 psi) 80.0 °C
176 °F
ISO 75-2
Vicat Softening Point 98.0 °C
208 °F
VST/B/50; ISO 306
Minimum Service Temperature, Air -30.0 °C
-22.0 °F
Flammability, UL94 HB

@Thickness 3.00 - 6.00 mm
HB

@Thickness 0.118 - 0.236 in
Electrical Properties Metric English Comments
Dielectric Constant 2.3

@Frequency 100 Hz
2.3

@Frequency 100 Hz
IEC 60250
Dielectric Strength >= 80.0 kV/mm
>= 2030 kV/in
in transformer oil; IEC 60243-1
Dissipation Factor 0.00040

@Frequency 100 Hz
0.00040

@Frequency 100 Hz
IEC 60250
Comparative Tracking Index >= 600 V
>= 600 V
IEC 60112
Descriptive Properties Value Comments
Color White
Food Compliance BfR: Yes
Food Compliance FDA Yes
Users viewing this material also viewed the following: