Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 1.20 GPa | 174 ksi | ISO 178 |
Premix Thermoplastics PRE-ELEC® ESD 6300 Static Dissipative Thermoplastic Compound PRE-ELEC® ESD 6300 is a static dissipative thermoplastic compound based on high impact polystyrene. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD6300 has be.. |
|||
Modulus of Elasticity | 1.20 GPa | 174 ksi | 4 mm thick;10.0 mm wide molded rod; ISO 178 |
Premix Thermoplastics PRE-ELEC® PE 1291 PRE-ELEC PE 1291 is a conductive thermoplastic compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PE 129.. |
|||
Modulus of Elasticity | 1.20 GPa | 174 ksi | ISO 178 |
Premix Thermoplastics PRE-ELEC® PP 1370 PRE-ELEC PP 1370 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELE.. |
|||
Modulus of Elasticity | 1.20 GPa | 174 ksi | ISO 178 |
Premix Thermoplastics PRE-ELEC® PP 1385 PRE-ELEC PP 1385 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELE.. |
|||
Modulus of Elasticity | 1.20 - 1.60 GPa | 174 - 232 ksi | ASTM D638-04 |
Proto3000 Objet Digital Materials™ DM_4310 Polypropylene-like Prototyping Polymer Primary material: DurusWhiteSecondary material: VeroWhitePlus, VeroBlue, VeroBlack or FullCure720Digital Materials are made up of two Objet materials. The two materials are combined in specific conc.. |
|||
Modulus of Elasticity | 1.20 - 1.60 GPa | 174 - 232 ksi | ASTM D638-04 |
Proto3000 Objet Digital Materials™ DM_4410 Polypropylene-like Prototyping Polymer Primary material: DurusWhiteSecondary material: VeroWhitePlus, VeroBlue, VeroBlack or FullCure720Digital Materials are made up of two Objet materials. The two materials are combined in specific conc.. |
|||
Modulus of Elasticity | 1.20 - 1.60 GPa | 174 - 232 ksi | ASTM D638-04 |
Proto3000 Objet Digital Materials™ DM_4510 Polypropylene-like Prototyping Polymer Primary material: DurusWhiteSecondary material: VeroWhitePlus, VeroBlue, VeroBlack or FullCure720Digital Materials are made up of two Objet materials. The two materials are combined in specific conc.. |
|||
Modulus of Elasticity | 1.20 - 1.60 GPa | 174 - 232 ksi | ASTM D638-04 |
Proto3000 Objet Digital Materials™ DM_4710 Polypropylene-like Prototyping Polymer Primary material: DurusWhiteSecondary material: VeroWhitePlus, VeroBlue, VeroBlack or FullCure720Digital Materials are made up of two Objet materials. The two materials are combined in specific conc.. |
|||
Modulus of Elasticity | 1.20 - 1.96 GPa | 174 - 284 ksi | Average value: 1.67 GPa Grade Count:19 |
Overview of materials for ECTFE Fluoropolymer This property data is a summary of similar materials in the MatWeb database for the category "ECTFE Fluoropolymer". Each property range of values reported is minimum and maximum values of appropriat.. |
|||
Modulus of Elasticity | 1.20 GPa | 174 ksi | ISO 527 |
Chevron Phillips Xtel® XE3200NA Polyphenylene Sulfide Alloy
(discontinued **) Xtel® XE3200NA is an un-reinforced high performance, PPS based alloy developed to provide exceptionally high ductility and impact resistance along with good thermal stability.Information provided b.. |
|||
Modulus of Elasticity | 1.20 GPa | 174 ksi | 0°C; ASTM D638 |
Micropol Isoplas P501 Crosslinkable Polyethylene Information provided by Micropol Limited |
|||
Modulus of Elasticity | >= 1.20 GPa | >= 174 ksi | Bending |
Sibur 21020-PM1 Polypropylene with Low Haze For production of three-layer PE/PP film, for production of sheets for cups and thin casting. It is allowed for contact with food products. |
|||
Modulus of Elasticity | >= 1.20 GPa | >= 174 ksi | Bending |
Sibur 21030-PM1 Polypropylene with Low Haze For production of three-layer PE/PP film, for production of sheets for cups and thin casting. It is allowed for contact with food products. |
|||
Modulus of Elasticity | >= 1.20 GPa | >= 174 ksi | Bending |
Sibur 21060-PM1 Polypropylene with Low Haze For production of three-layer PE/PP film, for production of sheets for cups and thin casting. It is allowed for contact with food products. |
|||
Modulus of Elasticity | >= 1.20 GPa | >= 174 ksi | Bending |
Sibur 21080-PM1 Polypropylene with Low Haze For production of three-layer PE/PP film, for production of sheets for cups and thin casting. It is allowed for contact with food products. |
|||
Modulus of Elasticity | 1.20 GPa | 174 ksi | MD; ExxonMobil Method |
ExxonMobil Label-Lyte™ 38DL247 OPP Film Product Description: A super white opaque, high gloss, high yield and highly cavitated BOPP film designed for use in reel-fed wrap-around labeling applications where superior graphics are desired.Av.. |
|||
Modulus of Elasticity | 1.20 GPa | 174 ksi | MD; ExxonMobil Method |
ExxonMobil Oppalyte™ 38DO447 OPP Film Product Description: A super white opaque BOPP film. The Diamex technology allows for super low density and very high yield. Diamex makes it possible to lower the density, without decreasing the mod.. |
|||
Modulus of Elasticity | 1.20 GPa | 174 ksi | ISO 178 |
Addiplast Addilene H 560 Polypropylene Homopolymer High heat resistance, detergent stabilized, anti-yellowingInformation provided by Addiplast. |
|||
Modulus of Elasticity | 1.20 GPa | 174 ksi | Conditioned; ISO 178 |
Addiplast Addilene PMD 50218 Flame Retardant Polypropylene Flame retardant, unreinforced, with halogensInformation provided by Addiplast. |
|||
Modulus of Elasticity | 1.20 GPa | 174 ksi | Conditioned; ISO 178 |
Addiplast Addinyl A2 Nylon 66 Unreinforced, medium viscosityInformation provided by Addiplast. |
|||
Modulus of Elasticity | 1.20 GPa | 174 ksi | ISO 527-2 |
BASF Ultraform® N2650 Z6 (LEV) POM Description: Is a POM + PUR, elastomer-modified injection-molding grade for applications requiring the highest impact strength together with low stiffness.Information provided by BASF |
|||
Modulus of Elasticity | 1.20 GPa | 174 ksi | ISO 527-1 |
Orbilan ORBILAN® PE 500 HMW-PE Orbilan PE 500 plastic is used as cutting boards for the food industry and gastronomy, in refrigeration chambers as ram protection and for swing doors as well as at sports grounds for sheets or hand.. |
|||
Modulus of Elasticity | 1.20 - 2.30 GPa @Temperature 60.0 - 90.0 °C |
174 - 334 ksi @Temperature 140 - 194 °F |
Average value: 1.67 GPa Grade Count:3 |
Overview of materials for Acetal Copolymer, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Glass Bead Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Modulus of Elasticity | 1.20 GPa | 174 ksi | ISO 527-1/-2 |
BASF Ultramid® B3S BK00464 PA6 (Conditioned) Description: Easy flowing, finely crystalline injection-molding grade for very fast processing. Uses include thin-walled technical parts (eg. housings, fittings, grips, small parts and fixing clamps.. |
|||
Modulus of Elasticity | 1.20 - 9.50 GPa | 174 - 1380 ksi | Average value: 3.85 GPa Grade Count:28 |
Overview of materials for Nylon 6, MoS2 Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropria.. |
|||
Modulus of Elasticity | 1.20 - 2.50 GPa @Temperature 60.0 - 90.0 °C |
174 - 363 ksi @Temperature 140 - 194 °F |
Average value: 1.85 GPa Grade Count:1 |
Overview of materials for Polypropylene with 40% Mica Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Mica Filler". Specific grades with primary filler content between 35% and 44% are.. |
|||
Modulus of Elasticity | 1.20 - 3.03 GPa | 174 - 440 ksi | Average value: 1.96 GPa Grade Count:18 |
Overview of materials for Polypropylene with 30% Calcium Carbonate (CaCO3) Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Calcium Carbonate (CaCO3) Filler". Each property range of values reported is mini.. |