Mechanical Properties Metric English Comments
Impact Test 50.0 J

@Temperature 23.0 °C
36.9 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Lexan® FXG173R PC
This data was supplied by SABIC-IP for the Americas region.
Impact Test 50.0 J

@Temperature 23.0 °C
36.9 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Noryl V0150BT PPE+HIPS
Noryl* V0150BT is an unfilled, injection moldable modified polyphenylene ether resin.. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 1.5 mm ..
Impact Test 50.0 J

@Temperature 23.0 °C
36.9 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Noryl V0150BT PPE+HIPS (Asia Pacific)
Noryl* V0150BT is an unfilled, injection moldable modified polyphenylene ether resin.. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 1.5 mm ..
Impact Test 50.0 J

@Temperature 23.0 °C
36.9 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Noryl V0150BT PPE+HIPS (Europe-Africa-Middle East)
Noryl* V0150BT is an unfilled, injection moldable modified polyphenylene ether resin.. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 1.5 mm ..
Impact Test 50.0 J

@Temperature 23.0 °C
36.9 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Xenoy® CL402 PBT+PC (Asia Pacific)
XENOY CL402 is a high viscosity, unfilled, elastomer modified PC/PBT blend for extrusion/blowmolding applications. ISO1043-label: PC+PBT-I.This data was supplied by SABIC-IP for the Asia Pacific reg..
Impact Test 50.0 J

@Temperature 23.0 °C
36.9 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Xenoy® CL402 PBT+PC (Europe-Africa-Middle East)
XENOY CL402 is a high viscosity, unfilled, elastomer modified PC/PBT blend for extrusion/blowmolding applications. ISO1043-label: PC+PBT-I.This data was supplied by SABIC-IP for the Europe-Africa-Mi..
Impact Test 50.0 J

@Temperature 23.0 °C
36.9 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Xenoy® IQ1103R PBT+PC
Xenoy* Resin iQ1103R - Environmetally responsible, sustainable, and low carbon footprint resin. Xenoy iQ1103R is an unreinforced, impact modified PC + iQ-PBT alloy with excellent low temperature im..
Impact Test 50.0 J

@Temperature 23.0 °C
36.9 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics LNP Stat-kon TD000
LNP* Stat-kon* TD000 is a compound based on Polyurethane resin. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the Americas region.
Impact Test 50.0 J

@Temperature 23.0 °C
36.9 ft-lb

@Temperature 73.4 °F
Instrumented Dart Total Energy
Styron Magnumâ„¢ 2620 ABS, Impact Grade
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ..
Impact Test 50.0 J

@Temperature 23.0 °C
36.9 ft-lb

@Temperature 73.4 °F
Instrumented Dart Total Energy
Styron Magnumâ„¢ 2630 ABS, High Impact
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ..
Impact Test 50.0 J

@Temperature 23.0 °C
36.9 ft-lb

@Temperature 73.4 °F
Instrumented Dart Total Energy
Styron Magnumâ„¢ 9030 ABS, High Gloss
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ..
Impact Test 50.0 J

@Temperature 23.0 °C
36.9 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Noryl GTX GTX979 PPE+PA
NORYL GTX979 is a conductive, high heat material. It is especially designed for in- and on-line painted bodypanels and fenders in particular, with conductivity for electro-static painting in an uniq..
Impact Test 50.0 J

@Temperature 23.0 °C
36.9 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Noryl GTX GTX979 PPE+PA (Asia Pacific)
NORYL GTX979 is a conductive, high heat material. It is especially designed for in- and on-line painted bodypanels and fenders in particular, with conductivity for electro-static painting in an uniq..
Impact Test 50.0 J

@Temperature 23.0 °C
36.9 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Noryl GTX GTX979 PPE+PA (Europe-Africa-Middle East)
NORYL GTX979 is a conductive, high heat material. It is especially designed for in- and on-line painted bodypanels and fenders in particular, with conductivity for electro-static painting in an uniq..
Impact Test 50.0 J
36.9 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP THERMOCOMP D7002IXH PC
LNP* THERMOCOMP* D7002IXH is a compound based on Polycarbonate siloxane copolymer resin containing proprietary antimicrobial additives. Designed for touch surfaces, housings, etc., in healthcare an..
Impact Test 50.0 J

@Thickness 3.20 mm
36.9 ft-lb

@Thickness 0.126 in
Instrumented Impact, Total Energy; 3.2 mm thick, 15 mph, 3 in. clamp, 0.5 in. dart; ASTM D3763
Covestro Makroblend® EL 703 Polycarbonate + Polyester-based Blend, Impact Modified, Flame-Retardant, UV Stabilized
Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.
Impact Test 50.0 J
36.9 ft-lb
tempering temperature of 500°C. Specimen size: 7x10x55 mm unnotched. Hardened at 1020°C. Quenched in air. Tempered twice
Assab Steels VANADIS 4 Cold Work Steel
VANADIS 4 is a chromium-molybdenum-vanadium alloyed steel which is characterized by:High wear resistanceHigh compressive strengthVery good through-hardening propertiesVery good toughnessExcellent di..
Impact Test 50.0 J

@Temperature 23.0 °C
36.9 ft-lb

@Temperature 73.4 °F
Instrumented Dart Total Energy
Styron Magnum™ 9020 ABS, High Gloss
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM AB..