Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polyram PlusTek PA301G50 Nylon 6.6, Heat Stabilized, 50% Glass Fiber

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 50% Glass Fiber Filled
Manufacturer Polyram
Trade Name PlusTek
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyram PlusTek PA301G50 Nylon 6.6, Heat Stabilized, 50% Glass Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Heat stabilized, 50% glass fiber reinforced polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
Physical Properties Metric English Comments
Density 1.55 g/cc
0.0560 lb/in³
DIN 53479
Water Absorption 4.0 %
4.0 %
DIN 53495
Moisture Absorption at Equilibrium 1.2 %
1.2 %
50%RH; DIN 53714
Linear Mold Shrinkage 0.0010 - 0.0025 cm/cm
0.0010 - 0.0025 in/in
Mechanical Properties Metric English Comments
Hardness, Rockwell R 122
122
ASTM-D785
Tensile Strength, Yield 230 MPa
33400 psi
ASTM-D638
Elongation at Break 2.0 %
2.0 %
ASTM-D638
Flexural Strength 330 MPa
47900 psi
ASTM D790
Flexural Modulus 15.0 GPa
2180 ksi
ASTM-D790
Izod Impact, Notched 1.30 J/cm

@Temperature 23.0 °C
2.44 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Thermal Properties Metric English Comments
Melting Point 256 °C
493 °F
Maximum Service Temperature, Air 100 °C
212 °F
Continuous Use
240 °C
464 °F
Short peaks operation
Deflection Temperature at 0.46 MPa (66 psi) 250 °C
482 °F
DIN 53461
Deflection Temperature at 1.8 MPa (264 psi) 250 °C
482 °F
DIN 53461
Flammability, UL94 HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
DIN 53482
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
DIN 53482
Dielectric Constant 3.8

@Frequency 1e+6 Hz
3.8

@Frequency 1e+6 Hz
VDE 0303/4
Dielectric Strength 90.0 kV/mm
2290 kV/in
VDE 0303/4
Users viewing this material also viewed the following: