Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Charpy Impact, Notched = 0.800 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.320 - 0.800 J/cm²
1.52 - 3.81 ft-lb/in²
Average value: 0.607 J/cm² Grade Count:3
Overview of materials for PCT, 40% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "PCT, 40% Glass Reinforced". Specific grades with glass content between 35% and 44% are included. Each pr..
Charpy Impact, Notched 0.120 - 0.800 J/cm²
0.571 - 3.81 ft-lb/in²
Average value: 0.377 J/cm² Grade Count:8
Overview of materials for Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled". Each property range of values repor..
Charpy Impact, Notched 0.350 - 0.800 J/cm²

@Temperature -30.0 - -30.0 °C
1.67 - 3.81 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 0.525 J/cm² Grade Count:4
Overview of materials for Acetal Copolymer, 20% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% ar..
Charpy Impact, Notched 0.700 - 0.800 J/cm²

@Temperature -30.0 - -30.0 °C
3.33 - 3.81 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 0.750 J/cm² Grade Count:2
Overview of materials for Liquid Crystal Polymer (LCP), Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Mineral Filled". Each property range of values reported is minimum and max..
Charpy Impact, Notched 0.800 - 0.800 J/cm²

@Temperature -30.0 - -30.0 °C
3.81 - 3.81 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 0.800 J/cm² Grade Count:1
Overview of materials for Medium Density Polyethylene (MDPE), Molded
This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Molded". Each property range of values reported is minimum and maxim..
Charpy Impact, Notched 0.400 - 0.800 J/cm²

@Temperature -30.0 - 30.0 °C
1.90 - 3.81 ft-lb/in²

@Temperature -22.0 - 86.0 °F
Average value: 0.521 J/cm² Grade Count:9
Overview of materials for Nylon 66/6, 20% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are incl..
Charpy Impact, Notched 0.0800 - 0.800 J/cm²

@Temperature -30.0 - -20.0 °C
0.381 - 3.81 ft-lb/in²

@Temperature -22.0 - -4.00 °F
Average value: 0.478 J/cm² Grade Count:10
Overview of materials for Nylon 66, Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Bead Filled". Each property range of values reported is minimum and maximum values of ap..
Charpy Impact, Notched 0.150 - 0.800 J/cm²

@Temperature -40.0 - 30.0 °C
0.714 - 3.81 ft-lb/in²

@Temperature -40.0 - 86.0 °F
Average value: 0.357 J/cm² Grade Count:32
Overview of materials for Nylon 66, 40% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Mineral Filled". Specific grades with primary filler content between 35% and 44% are inclu..
Charpy Impact, Notched 0.300 - 0.800 J/cm²
1.43 - 3.81 ft-lb/in²
ISO 179
Bulk Molding Compounds tetra-DUR F 4001 Bulk Molding Compound
UL-Licensed, Abrasion resistance, free of fiber glass.Typical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipati..
Charpy Impact, Notched 0.400 - 0.800 J/cm²

@Temperature -40.0 - -30.0 °C
1.90 - 3.81 ft-lb/in²

@Temperature -40.0 - -22.0 °F
Average value: 0.625 J/cm² Grade Count:3
Overview of materials for Nylon 66, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, PTFE Filled". Each property range of values reported is minimum and maximum values of appropri..
Charpy Impact, Notched 0.250 - 0.800 J/cm²

@Temperature -30.0 - -20.0 °C
1.19 - 3.81 ft-lb/in²

@Temperature -22.0 - -4.00 °F
Average value: 0.636 J/cm² Grade Count:11
Overview of materials for Polyethersulfone (PES)
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone". Each property range of values reported is minimum and maximum values of appropriate M..
Charpy Impact, Notched 0.600 - 0.800 J/cm²
2.86 - 3.81 ft-lb/in²
Average value: 0.733 J/cm² Grade Count:3
Overview of materials for Polyethersulfone (PES), 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% ..
Charpy Impact, Notched 0.800 - 0.800 J/cm²

@Temperature -30.0 - -30.0 °C
3.81 - 3.81 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 0.800 J/cm² Grade Count:1
Overview of materials for Polyethersulfone (PES), 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% ..
Charpy Impact, Notched 0.100 - 0.800 J/cm²

@Temperature -20.0 - -20.0 °C
0.476 - 3.81 ft-lb/in²

@Temperature -4.00 - -4.00 °F
Average value: 0.425 J/cm² Grade Count:4
Overview of materials for Polypropylene, Glass Reinforced, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass Reinforced, Impact Modified". Each property range of values reported is minimum and..
Charpy Impact, Notched 0.150 - 0.800 J/cm²
0.714 - 3.81 ft-lb/in²
Average value: 0.405 J/cm² Grade Count:11
Overview of materials for Epoxy, Molded, Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Molded, Glass Fiber Filler". Each property range of values reported is minimum and maximum values..
Charpy Impact, Notched 0.500 - 0.800 J/cm²

@Temperature -40.0 - -30.0 °C
2.38 - 3.81 ft-lb/in²

@Temperature -40.0 - -22.0 °F
Average value: 0.653 J/cm² Grade Count:3
Overview of materials for Polyethylene Terephthalate (PET), 20% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 20% Glass Reinforced". Specific grades with glass content between 15% ..
Charpy Impact, Notched 0.350 - 0.800 J/cm²
1.67 - 3.81 ft-lb/in²
Average value: 0.617 J/cm² Grade Count:3
Overview of materials for Polysulfone, 20% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are inc..
Charpy Impact, Notched 0.700 - 0.800 J/cm²
3.33 - 3.81 ft-lb/in²
Average value: 0.775 J/cm² Grade Count:4
Overview of materials for Polyphthalamide (PPA), Carbon Fiber + PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Carbon Fiber + PTFE Filled". Each property range of values reported is minimum and maxi..
Copyright © lookpolymers.com All Rights Reserved