Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.320 - 0.800 J/cm² | 1.52 - 3.81 ft-lb/in² | Average value: 0.607 J/cm² Grade Count:3 |
Overview of materials for PCT, 40% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PCT, 40% Glass Reinforced". Specific grades with glass content between 35% and 44% are included. Each pr.. |
|||
Charpy Impact, Notched | 0.120 - 0.800 J/cm² | 0.571 - 3.81 ft-lb/in² | Average value: 0.377 J/cm² Grade Count:8 |
Overview of materials for Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled". Each property range of values repor.. |
|||
Charpy Impact, Notched | 0.350 - 0.800 J/cm² @Temperature -30.0 - -30.0 °C |
1.67 - 3.81 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 0.525 J/cm² Grade Count:4 |
Overview of materials for Acetal Copolymer, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% ar.. |
|||
Charpy Impact, Notched | 0.700 - 0.800 J/cm² @Temperature -30.0 - -30.0 °C |
3.33 - 3.81 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 0.750 J/cm² Grade Count:2 |
Overview of materials for Liquid Crystal Polymer (LCP), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Mineral Filled". Each property range of values reported is minimum and max.. |
|||
Charpy Impact, Notched | 0.800 - 0.800 J/cm² @Temperature -30.0 - -30.0 °C |
3.81 - 3.81 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 0.800 J/cm² Grade Count:1 |
Overview of materials for Medium Density Polyethylene (MDPE), Molded This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Molded". Each property range of values reported is minimum and maxim.. |
|||
Charpy Impact, Notched | 0.400 - 0.800 J/cm² @Temperature -30.0 - 30.0 °C |
1.90 - 3.81 ft-lb/in² @Temperature -22.0 - 86.0 °F |
Average value: 0.521 J/cm² Grade Count:9 |
Overview of materials for Nylon 66/6, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are incl.. |
|||
Charpy Impact, Notched | 0.0800 - 0.800 J/cm² @Temperature -30.0 - -20.0 °C |
0.381 - 3.81 ft-lb/in² @Temperature -22.0 - -4.00 °F |
Average value: 0.478 J/cm² Grade Count:10 |
Overview of materials for Nylon 66, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Bead Filled". Each property range of values reported is minimum and maximum values of ap.. |
|||
Charpy Impact, Notched | 0.150 - 0.800 J/cm² @Temperature -40.0 - 30.0 °C |
0.714 - 3.81 ft-lb/in² @Temperature -40.0 - 86.0 °F |
Average value: 0.357 J/cm² Grade Count:32 |
Overview of materials for Nylon 66, 40% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Mineral Filled". Specific grades with primary filler content between 35% and 44% are inclu.. |
|||
Charpy Impact, Notched | 0.300 - 0.800 J/cm² | 1.43 - 3.81 ft-lb/in² | ISO 179 |
Bulk Molding Compounds tetra-DUR F 4001 Bulk Molding Compound UL-Licensed, Abrasion resistance, free of fiber glass.Typical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipati.. |
|||
Charpy Impact, Notched | 0.400 - 0.800 J/cm² @Temperature -40.0 - -30.0 °C |
1.90 - 3.81 ft-lb/in² @Temperature -40.0 - -22.0 °F |
Average value: 0.625 J/cm² Grade Count:3 |
Overview of materials for Nylon 66, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, PTFE Filled". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Charpy Impact, Notched | 0.250 - 0.800 J/cm² @Temperature -30.0 - -20.0 °C |
1.19 - 3.81 ft-lb/in² @Temperature -22.0 - -4.00 °F |
Average value: 0.636 J/cm² Grade Count:11 |
Overview of materials for Polyethersulfone (PES) This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Charpy Impact, Notched | 0.600 - 0.800 J/cm² | 2.86 - 3.81 ft-lb/in² | Average value: 0.733 J/cm² Grade Count:3 |
Overview of materials for Polyethersulfone (PES), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% .. |
|||
Charpy Impact, Notched | 0.800 - 0.800 J/cm² @Temperature -30.0 - -30.0 °C |
3.81 - 3.81 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 0.800 J/cm² Grade Count:1 |
Overview of materials for Polyethersulfone (PES), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% .. |
|||
Charpy Impact, Notched | 0.100 - 0.800 J/cm² @Temperature -20.0 - -20.0 °C |
0.476 - 3.81 ft-lb/in² @Temperature -4.00 - -4.00 °F |
Average value: 0.425 J/cm² Grade Count:4 |
Overview of materials for Polypropylene, Glass Reinforced, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass Reinforced, Impact Modified". Each property range of values reported is minimum and.. |
|||
Charpy Impact, Notched | 0.150 - 0.800 J/cm² | 0.714 - 3.81 ft-lb/in² | Average value: 0.405 J/cm² Grade Count:11 |
Overview of materials for Epoxy, Molded, Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Molded, Glass Fiber Filler". Each property range of values reported is minimum and maximum values.. |
|||
Charpy Impact, Notched | 0.500 - 0.800 J/cm² @Temperature -40.0 - -30.0 °C |
2.38 - 3.81 ft-lb/in² @Temperature -40.0 - -22.0 °F |
Average value: 0.653 J/cm² Grade Count:3 |
Overview of materials for Polyethylene Terephthalate (PET), 20% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 20% Glass Reinforced". Specific grades with glass content between 15% .. |
|||
Charpy Impact, Notched | 0.350 - 0.800 J/cm² | 1.67 - 3.81 ft-lb/in² | Average value: 0.617 J/cm² Grade Count:3 |
Overview of materials for Polysulfone, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are inc.. |
|||
Charpy Impact, Notched | 0.700 - 0.800 J/cm² | 3.33 - 3.81 ft-lb/in² | Average value: 0.775 J/cm² Grade Count:4 |
Overview of materials for Polyphthalamide (PPA), Carbon Fiber + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Carbon Fiber + PTFE Filled". Each property range of values reported is minimum and maxi.. |