Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.160 - 4.50 J/cm² | 0.761 - 21.4 ft-lb/in² | Average value: 0.723 J/cm² Grade Count:35 |
Overview of materials for Polybutylene Terephthalate (PBT), Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Flame Retardant". Each property range of values reported is minimum an.. |
|||
Charpy Impact, Notched | 0.400 - 4.50 J/cm² | 1.90 - 21.4 ft-lb/in² | Average value: 1.23 J/cm² Grade Count:39 |
Overview of materials for Nylon 66/6, 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are incl.. |
|||
Charpy Impact, Notched | 0.400 - 4.50 J/cm² | 1.90 - 21.4 ft-lb/in² | Average value: 2.03 J/cm² Grade Count:34 |
Overview of materials for Nylon 66/6, 40% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 40% Glass Fiber Reinforced". Specific grades with glass content between 35% and 44% are incl.. |
|||
Charpy Impact, Notched | 0.300 - 4.50 J/cm² @Temperature -30.0 - 30.0 °C |
1.43 - 21.4 ft-lb/in² @Temperature -22.0 - 86.0 °F |
Average value: 1.92 J/cm² Grade Count:25 |
Overview of materials for Nylon 66/6, 40% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 40% Glass Fiber Reinforced". Specific grades with glass content between 35% and 44% are incl.. |
|||
Charpy Impact, Notched | 1.10 - 4.50 J/cm² @Temperature -30.0 - 30.0 °C |
5.24 - 21.4 ft-lb/in² @Temperature -22.0 - 86.0 °F |
Average value: 3.03 J/cm² Grade Count:8 |
Overview of materials for Nylon 66/6, 60% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 60% Glass Fiber Reinforced". Specific grades with glass content between 55% and 64% are incl.. |
|||
Charpy Impact, Notched | 0.350 - 4.50 J/cm² @Temperature -40.0 - 30.0 °C |
1.67 - 21.4 ft-lb/in² @Temperature -40.0 - 86.0 °F |
Average value: 1.39 J/cm² Grade Count:39 |
Overview of materials for Nylon 66, 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. .. |
|||
Charpy Impact, Notched | 3.50 - 4.50 J/cm² | 16.7 - 21.4 ft-lb/in² | DIN 53453 |
Zell-Metall Engineering Plastics Zellamid 1115 By special additives, impact strength and abrasion resistance are further improved. We particularly recommend this material for slipper pads for rolling mills.Color: IvoryApplications: slipper pads .. |
|||
Charpy Impact, Notched | 2.00 - 4.50 J/cm² | 9.52 - 21.4 ft-lb/in² | ISO 179 |
Bulk Molding Compounds tetra-DUR F 4308 Bulk Molding Compound UL-licensedTypical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion protection), thermal stabilit.. |
|||
Charpy Impact, Notched | 0.300 - 4.50 J/cm² | 1.43 - 21.4 ft-lb/in² | Average value: 2.14 J/cm² Grade Count:42 |
Overview of materials for Polypropylene with 40% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Glass Fiber Filler". Specific grades with glass content between 35% and 44% are i.. |