Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.347 J/cm | 0.650 ft-lb/in | ASTM D256 |
Omni Plastics OmniTech™ PA6/6 SI2 FD Wear-and-Friction Silicone filled Nylon OmniTech™ is a family of non-standard products custom developed for applications with unique functional requirements, including but not limited to: Flame Retardant, Conductive, Wear Resistant, and .. |
|||
Izod Impact, Notched | 0.347 J/cm | 0.650 ft-lb/in | ASTM D256 |
Omni Plastics OmniTech™ PA6/6 SI2 FD WH Flame Retardant UL Approved MaterialOmniTech™ is a family of non-standard products custom developed for applications with unique functional requirements, including but not limited to: Flame Retardant, Conductive, .. |
|||
Izod Impact, Notched | 0.347 J/cm | 0.650 ft-lb/in | |
Reliance Industries Polypropylene - 40% Suzorex mica (surface treated) filled Information provided by Reliance Industries |
|||
Izod Impact, Notched | 0.347 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
0.650 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
Method A, Injection Molded; ASTM D256 |
PolyOne Lubri-Tech™ PS-15GB/15T Polybutylene Terephthalate (PBT), Glass Bead Filled, PTFE Lubricated
(discont Description/Features:Glass Bead FilledPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Izod Impact, Notched | 0.347 - 1.98 J/cm | 0.650 - 3.71 ft-lb/in | Average value: 0.626 J/cm Grade Count:18 |
Overview of materials for Polyphenylene Sulfide (PPS) with 20% Carbon Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 20% Carbon Fiber Filler". Specific grades with carbon fiber content bet.. |
|||
Izod Impact, Notched | 0.347 J/cm | 0.650 ft-lb/in | ASTM D256 |
LyondellBasell Alathon® H4250 High Density Polyethylene, Injection Molding Grade ALATHON H4250 is a high-flow “freezer†grade resin that exhibits enhanced cold temperature impact performance, enhanced processing and thermal stability, with good color and organoleptic p.. |
|||
Izod Impact, Notched | 0.347 J/cm @Temperature 22.8 °C |
0.650 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Spartech PP5110 Talc Filled Homopolymer Offers an excellent balance of processing improvement and high levels of stiffness and heat deflection temperatureInformation provided by Spartech |
|||
Izod Impact, Notched | 0.347 J/cm @Thickness 3.17 mm |
0.650 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PBT G/CF30 40% Glass Bead Filler Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 40% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 0.347 J/cm | 0.650 ft-lb/in | ASTM D256 |
Sumitomo Bakelite Durez® 31906 Phenolic, Compression Grade Durez 31906 Black Phenolic is an asbestos free, medium impact, molding compound. It is designed for applications where additional mechanical strength is required.Information provided by Sumitomo Ba.. |
|||
Izod Impact, Notched | 0.347 J/cm @Thickness 3.17 mm |
0.650 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill FR® PP GF10 FR BK 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 10% Filler by WeightFeatures: Flame Retardant Appearance: BlackInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 0.347 J/cm | 0.650 ft-lb/in | |
Master Bond EP126 Two Component Toughened Epoxy Adhesive System Master Bond Polymer System EP126 is a two component toughened epoxy resin based high temperature resistant adhesive system with continuous service capability at 500°F and outstanding chemical resis.. |
|||
Izod Impact, Notched | 0.347 J/cm | 0.650 ft-lb/in | |
Tra-Con Tra-Cast 3357 High Temperature Rigid Epoxy Casting System TRA-CAST 3357 is a smooth pouring, low viscosity casting resin system recommended for rigid, large mass potting, encapsulating, laminating, filament-winding and coil embedment applications where the.. |
|||
Izod Impact, Notched | 0.347 J/cm | 0.650 ft-lb/in | ASTM D256 |
Ensinger Tecatron® XP-81 Compression Molded PPS Compound, Filled with 15% Graphite and 15% Carbon Fiber Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p.. |
|||
Izod Impact, Notched | 0.347 J/cm | 0.650 ft-lb/in | ASTM D256A |
Dow 5D98 Polypropylene Homopolymer Resin OverviewConsistent processabilityGood optical propertiesHigh strength propertiesComplies with: U.S. FDA 21 CFR 177.1520 (c)1.1a, Europe EU-Directive 2002/72/ECDOW 5D98 Polypropylene Resin is intende.. |
|||
Izod Impact, Notched | 0.347 J/cm | 0.650 ft-lb/in | molded and tested in accordance with ASTM D 4101; ASTM D256A |
Dow 5D98 Polypropylene Resin DOW 5D98 is intended for use in oriented polypropylene (OPP) film processes.Information provided by DowDow Announced Sale of Global Polypropylene Business to Braskem in July 2011. |
|||
Izod Impact, Notched | 0.347 J/cm | 0.650 ft-lb/in | ASTM D256 |
Asahi Kasei Thermofil P-20TC-5103 20% Talc Reinforced, Lubricated, Heat Stabilized Information provided by Asahi Thermofil |