Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.15 J/cm @Temperature -30.0 °C |
2.15 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Cycoloy® CY6310 PC+ABS Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow / impact balance for a wide variety of thin wall or la.. |
|||
Izod Impact, Notched | 1.15 J/cm | 2.15 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® FXM2143H PC Copolymer FXM2143H is a high flow, UV stabilized, high heat polycarbonate copolymer with an HDT/Af of 142 C. |
|||
Izod Impact, Notched | 1.15 J/cm @Temperature -30.0 °C |
2.15 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® HFD1830 PC Copolymer 40 MFR LEXAN High Flow Ductile Copolymer UV Stabilized |
|||
Izod Impact, Notched | 1.15 J/cm | 2.15 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® XHT2141 PC Copolymer XHT2141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Izod Impact, Notched | 1.15 J/cm | 2.15 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® XHT2141 PC Copolymer (Asia Pacific) XHT2141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Izod Impact, Notched | 1.15 J/cm | 2.15 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® XHT2143 PC Copolymer (Europe-Africa-Middle East) XHT2143 is a high flow, UV stabilized, high heat polycarbonate copolymer with an HDT/Af of 142 C. It is available in a range of opaque and limited transparent colors. |
|||
Izod Impact, Notched | 1.15 J/cm | 2.15 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® XHT2146 PC Copolymer XHT2146 resin is a high flow, high heat polycarbonate copolymer with improved release performance compared to Lexan* XHT2141 resin. It is available in a range of opaque and limited transparent colo.. |
|||
Izod Impact, Notched | 1.15 J/cm | 2.15 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® XHT2146 PC Copolymer (Asia Pacific) XHT2146 resin is a high flow, high heat polycarbonate copolymer with improved release performance compared to Lexan* XHT2141 resin. It is available in a range of opaque and limited transparent colo.. |
|||
Izod Impact, Notched | 1.15 - 8.00 J/cm | 2.15 - 15.0 ft-lb/in | Average value: 4.92 J/cm Grade Count:3 |
Overview of materials for Medium Density Polyethylene (MDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Film Grade". Each property range of values reported is minimum and m.. |
|||
Izod Impact, Notched | 1.15 J/cm | 2.15 ft-lb/in | ASTM D256 |
Flint Hills P5C4K-089 Random Copolymer Polypropylene Features: Good clarity. Product does not contain animal derived components. Phthalate-freeApplications: Cast FilmInformation provided by Flint Hills Resources. |
|||
Izod Impact, Notched | 1.15 J/cm | 2.15 ft-lb/in | ASTM D256-03 |
Ipiranga Petrochem MB 0434 LS-L MDPE IPQ employs Spherilene technology from Basell in the production of MDPE. The raw materials, which are supplied by COPESUL, are pre-treated and fed into gas-phase reactors, where medium density polye.. |
|||
Izod Impact, Notched | 1.15 J/cm | 2.15 ft-lb/in | ASTM D256-03 |
Ipiranga Petrochem MB 0435 MDPE IPQ employs Spherilene technology from Basell in the production of MDPE. The raw materials, which are supplied by COPESUL, are pre-treated and fed into gas-phase reactors, where medium density polye.. |
|||
Izod Impact, Notched | 1.15 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
2.15 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Kingfa PA66-G30 30% Glass Fiber Reinforced PA66 Features:Good size stabilityLow tendency to wrapHigh mechanical propertiesGood low temperature resistanceGood surfaceExcellent balance propertiesApplications:Injection moldingAutomobile partsPower t.. |
|||
Izod Impact, Notched | 1.15 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
2.15 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Kingfa PA6-RG30 Flame Retardant, 30% Glass Fiber Reinforced PA6 Features:Flame retardantHigh strengthHigh temperature propertiesGood electric propertiesApplications:Injection moldingConnectorsRelayBobbinsPlugsInformation Provided by Kingfa Sci. & Tech. Co., Ltd... |
|||
Izod Impact, Notched | 1.15 J/cm | 2.15 ft-lb/in | ASTM D256 |
Solvay TECHNYL® A 218 V30 BK 34 NG-K PA66, 33% glass fiber, DRY Description: TECHNYL® A 218 V30 Black 34 NG-K is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. The product is available in black color. Benefits: Thi.. |
|||
Izod Impact, Notched | 1.15 J/cm | 2.15 ft-lb/in | ASTM D256 |
Solvay TECHNYL® A 218 V30 PA66, 30% glass fiber, DRY Description: TECHNYL® A 218 V30 is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Izod Impact, Notched | 1.15 J/cm | 2.15 ft-lb/in | ASTM D256 |
Solvay TECHNYL® A 30 H1 V30 PA66, 30% glass fiber, DRY Description: TECHNYL® A 30H1 V30 is a brominated flame retardant polyamide 66, reinforced with 30% of glass fiber, for injection molding. This product is available in natural & black color.Benefi.. |
|||
Izod Impact, Notched | 1.15 J/cm | 2.15 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON DD200C PC (Asia Pacific) PTFE free polycarbonate compounds with ESD safety and good lubricating perfomrance , suitable for Semiconductor and Hard Disk Drive (HDD) and semicon industry. Added features of this material includ.. |
|||
Izod Impact, Notched | 1.15 J/cm | 2.15 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® 5031 PBT (Europe-Africa-Middle East) VALOX 5031 is a 30% glass reinforced PBT+PC blend with low warpage characteristics. Applications: appliance handles, automotive doorhandles. This grade is a 508 with reduced warpage. |
|||
Izod Impact, Notched | 1.15 J/cm | 2.15 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics ULTEM 9085 PEI Blend High flow Polyetherimide blend. Meets FAR 25.853 and OSU 65/65 with low toxicity, smoke and flame evolution. |
|||
Izod Impact, Notched | 1.15 J/cm | 2.15 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics ULTEM 9085 PEI Blend (Europe-Africa-Middle East) High flow Polyetherimide blend. Meets FAR 25.853 and OSU 55/55 with low toxicity, smoke and flame evolution. |
|||
Izod Impact, Notched | 1.15 J/cm | 2.15 ft-lb/in | ASTM D256 |
A. Schulman POLYFLAM™ RABS 930-01 Information provided by A. Schulman. |
|||
Izod Impact, Notched | 1.15 J/cm @Temperature 23.0 °C |
2.15 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram PlusTek PA303G6 Nylon 6.6, Heat Stabilized, 30% Glass Fiber 30% glass fiber reinforced, heat stabilized and hydrolysis resistant polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 1.15 J/cm | 2.15 ft-lb/in | ASTM D256 |
A. Schulman POLYFLAM™ RABS 930-01 Information provided by A. Schulman. |
|||
Izod Impact, Notched | 1.15 J/cm @Temperature 23.0 °C |
2.15 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram PlusTek RA303G6 Nylon 6.6, 30% Glass Fiber 30% glass fiber reinforced, heat stabilized, and hydrolysis resistant polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 1.15 J/cm | 2.15 ft-lb/in | ASTM D256 |
A. Schulman POLYFLAM™ RABS 930-01 Information provided by A. Schulman. |
|||
Izod Impact, Notched | 1.15 J/cm | 2.15 ft-lb/in | ASTM D256 |
A. Schulman POLYFLAM™ RABS 930-01 Information provided by A. Schulman. |
|||
Izod Impact, Notched | 1.15 J/cm | 2.15 ft-lb/in | ASTM D256 |
E-Polymers Tekaster® F615G45 , 45% Glass Fiber Reinforced PET 45% Glass Fiber reinforced, High strength, Information provided by E-Polymers Co. Ltd. |
|||
Izod Impact, Notched | 1.15 J/cm @Temperature -30.0 °C |
2.15 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Cycolac® DL100LG ABS (Europe-Africa-Middle East) Cycolac DL100LG is a low gloss, high heat, high impact ABS/PC blend with low emission |
|||
Izod Impact, Notched | 1.15 J/cm @Temperature -30.0 °C |
2.15 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Cycoloy® CY6310 PC+ABS (Asia Pacific) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow / impact balance for a wide variety of thin wall or la.. |