Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.265 - 8.02 J/cm | 0.496 - 15.0 ft-lb/in | Average value: 1.38 J/cm Grade Count:85 |
Overview of materials for Polybutylene Terephthalate (PBT), Unreinforced, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Unreinforced, Molded". Each property range of values reported is minim.. |
|||
Izod Impact, Notched | 0.427 - 8.00 J/cm | 0.800 - 15.0 ft-lb/in | Average value: 1.34 J/cm Grade Count:102 |
Overview of materials for Polycarbonate, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum a.. |
|||
Izod Impact, Notched | 0.907 - 8.01 J/cm | 1.70 - 15.0 ft-lb/in | Average value: 2.90 J/cm Grade Count:10 |
Overview of materials for PVC, Sheet Grade This property data is a summary of similar materials in the MatWeb database for the category "PVC, Sheet Grade". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Izod Impact, Notched | 0.198 - 8.01 J/cm | 0.370 - 15.0 ft-lb/in | Average value: 0.688 J/cm Grade Count:159 |
Overview of materials for Polypropylene with 20% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Talc Filler".Specific grades with primary filler content between 15% and 24% are .. |
|||
Izod Impact, Notched | 1.15 - 8.00 J/cm | 2.15 - 15.0 ft-lb/in | Average value: 4.92 J/cm Grade Count:3 |
Overview of materials for Medium Density Polyethylene (MDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Film Grade". Each property range of values reported is minimum and m.. |
|||
Izod Impact, Notched | 0.747 - 8.01 J/cm | 1.40 - 15.0 ft-lb/in | Average value: 3.27 J/cm Grade Count:15 |
Overview of materials for Fluorocarbon ETFE, with Glass or Carbon Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Fluorocarbon ETFE, with Glass or Carbon Fiber Filler". Each property range of values reported is minimum.. |
|||
Izod Impact, Notched | 6.00 - 8.00 J/cm | 11.2 - 15.0 ft-lb/in | ASTM D256 |
Loxim 100 00V0 Polycarbonate, Flame Retardant Information provided by Loxim Industries |
|||
Izod Impact, Notched | 6.00 - 8.00 J/cm | 11.2 - 15.0 ft-lb/in | ASTM D256 |
Loxim 100 00V2 Polycarbonate, Flame Retardant Information provided by Loxim Industries |
|||
Izod Impact, Notched | 6.00 - 8.00 J/cm @Temperature 23.0 °C |
11.2 - 15.0 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Loxim 600 00HB Polycarbonate/Polybutylene Terephthalate Information provided by Loxim Industries |
|||
Izod Impact, Notched | 2.67 - 8.01 J/cm | 5.00 - 15.0 ft-lb/in | |
Bulk Molding Compounds BMC 606 Mineral Filled, Glass Reinforced Polyester Compound BMC 606 is a mineral filled, glass reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is characterized by good moldability, excellent impact strength,.. |
|||
Izod Impact, Notched | 6.94 - 8.01 J/cm | 13.0 - 15.0 ft-lb/in | |
Bulk Molding Compounds BMC 5592 Arc, Track, and Weather Resistant Polyester BMC 5592 molding compound is an arc, track and weather resistant grade polyester compound suitable for compression, transfer and stuffer injection molding. It has excellent impact strength, flame re.. |
|||
Izod Impact, Notched | 5.00 - 8.01 J/cm | 9.37 - 15.0 ft-lb/in | Average value: 6.00 J/cm Grade Count:3 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Injection Molded This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Injection Molded". Each property range of values reported is mi.. |
|||
Izod Impact, Notched | 0.400 - 8.01 J/cm | 0.749 - 15.0 ft-lb/in | Average value: 2.40 J/cm Grade Count:9 |
Overview of materials for Nylon 11, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11, Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Izod Impact, Notched | 0.427 - 8.01 J/cm | 0.800 - 15.0 ft-lb/in | Average value: 1.98 J/cm Grade Count:61 |
Overview of materials for Polycarbonate, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, PTFE Filled". Each property range of values reported is minimum and maximum values of app.. |
|||
Izod Impact, Notched | 5.34 - 8.01 J/cm | 10.0 - 15.0 ft-lb/in | ASTM D256 |
Premix Premi-Glas® 1200-24 Polyester SMC
(discontinued **) Premi-Glas® 1200-24 is a 24% fiberglass-reinforced, thermoset, sheet molding compound designed for Class A Heavy Truck - Bus body panels and Marine cowls parts where smooth, flat, ripple free surfa.. |