Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 2.20 J/cm² @Temperature -40.0 °C |
10.5 ft-lb/in² @Temperature -40.0 °F |
DIN 53453 |
Nilit FRIANYL A63 H-SG40 Nylon 6.6 for injection molding, 40% mineral filled Nylon 6.6 for injection molding, heat stabilized (dark natural color).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 2.20 J/cm² @Temperature -40.0 °C |
10.5 ft-lb/in² @Temperature -40.0 °F |
DIN 53453 |
Nilit FRIANYL A63 SG40 Nylon 6.6 for injection molding, 40% mineral filled Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 2.20 J/cm² | 10.5 ft-lb/in² | DIN 53453 |
Nilit FRIANYL A63 KV40 Nylon 6.6 for injection molding, 40% glass ball reinforced Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 2.20 - 9.50 J/cm² | 10.5 - 45.2 ft-lb/in² | Average value: 5.15 J/cm² Grade Count:32 |
Overview of materials for Nylon 66, 10% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Carbon Fiber Filled". Specific grades with carbon fiber content between 5% and 14% are inc.. |
|||
Charpy Impact Unnotched | 2.20 - 9.00 J/cm² @Temperature -40.0 - -30.0 °C |
10.5 - 42.8 ft-lb/in² @Temperature -40.0 - -22.0 °F |
Average value: 4.59 J/cm² Grade Count:16 |
Overview of materials for Nylon 66, 10% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Carbon Fiber Filled". Specific grades with carbon fiber content between 5% and 14% are inc.. |
|||
Charpy Impact Unnotched | 2.20 J/cm² | 10.5 ft-lb/in² | flatwise; ISO 179 1fU |
Lehmann & Voss LUVOCOM® 1105-7760 PEEK, with carbon fiber, PTFE, lubricant modified, high viscosity Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m.. |
|||
Charpy Impact Unnotched | 2.20 J/cm² | 10.5 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 1-8490 Polyamide 66, with carbon fiber, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.High dimensionally stab.. |
|||
Charpy Impact Unnotched | 2.20 J/cm² | 10.5 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 19-7816 Polyamide 46, with carbon fiber, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.Electrical.. |
|||
Charpy Impact Unnotched | 2.20 J/cm² | 10.5 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 20-8112 Polyphthalamide, with carbon fiber, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Improved friction and wear.. |
|||
Charpy Impact Unnotched | 2.20 J/cm² | 10.5 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 20-8286 Polyphthalamide, with carbon fiber, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Improved friction and wear.. |
|||
Charpy Impact Unnotched | 2.20 J/cm² | 10.5 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 50-8022 Polycarbonate, with carbon fiber Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Strong, stiff parts.Reduced moment of inertia compared with me.. |
|||
Charpy Impact Unnotched | 2.20 J/cm² | 10.5 ft-lb/in² | ISO 179/1eU |
Lucite International Diakon® Frost 952 70 Acrylic Polymer Information provided by Lucite International |
|||
Charpy Impact Unnotched | 2.20 J/cm² | 10.5 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 19-7745 Polyamide 46, with PTFE, improved wear resistance Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Isotropic shrinkage characteristics.Good friction and wear behaviour especially at increased te.. |
|||
Charpy Impact Unnotched | 2.20 J/cm² @Temperature -30.0 °C |
10.5 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Lehmann & Voss LUVOCOM® 50/GF/20/TF/20/BK 100 Polycarbonate, with glass fiber and PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Charpy Impact Unnotched | 2.20 J/cm² @Temperature -30.0 °C |
10.5 ft-lb/in² @Temperature -22.0 °F |
|
Ineos ABS TRIAX® 1220 S ABS/Nylon Blend, Dry as Molded Extrusion and injection molding grade with good stress corrosion cracking resistance, good chemical resistance (fuel, cleaning agents), high impact and notched impact strength, good acoustical dampi.. |
|||
Charpy Impact Unnotched | 2.20 J/cm² | 10.5 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics LNP STAT-KON EX03319C PEI (Asia Pacific) LNP* Stat-Kon* EX03319C is a polyetherimide compound reinforced with carbon fiber for good stiffness, dimension stability and has extremely high level of cleanliness for the most demanding applicati.. |
|||
Charpy Impact Unnotched | 2.20 J/cm² | 10.5 ft-lb/in² | IS0179-1:2000 |
Zhejiang Juner PA-A7-1 Flame-Retardant & Glass Reinforced, Environmental PA66 Applications: Electric Cabinet BracketInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Charpy Impact Unnotched | 2.20 J/cm² | 10.5 ft-lb/in² | ISO 179-1 |
Unitika A1025GO PA6, Flame Retardant, Dry Information provided by Unitika Ltd. |
|||
Charpy Impact Unnotched | 2.20 J/cm² | 10.5 ft-lb/in² | Conditioned; ISO 179/IeU |
Addiplast Addinyl B2H G30 Flame Retardant Nylon 6, 30% Glass Bead Flame retardant, 30% glass bead filled, with halogensInformation provided by Addiplast. |
|||
Charpy Impact Unnotched | 2.20 J/cm² | 10.5 ft-lb/in² | ISO 179/1eU |
Polyplastic Armlen® PP MD 40-4HS-901 Polypropylene, 40% Mineral Filled Heat stabilizedInformation provided by PolyPlastic Group. |
|||
Charpy Impact Unnotched | 2.20 - 3.50 J/cm² @Temperature -40.0 - -30.0 °C |
10.5 - 16.7 ft-lb/in² @Temperature -40.0 - -22.0 °F |
Average value: 2.85 J/cm² Grade Count:2 |
Overview of materials for Polyethylene Terephthalate (PET), Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass/Mineral Reinforced". Each property range of values reported is m.. |
|||
Charpy Impact Unnotched | 2.20 J/cm² @Temperature -30.0 °C |
10.5 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Lehmann & Voss LUVOCOM® 50/GF/20/TF/10/BK Polycarbonate, with glass fiber and PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Charpy Impact Unnotched | 2.20 - 1000 J/cm² | 10.5 - 4760 ft-lb/in² | Average value: 4.15 J/cm² Grade Count:7 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified". Each property range of values reported.. |
|||
Charpy Impact Unnotched | 2.20 - 999.9 J/cm² @Temperature -30.0 - 30.0 °C |
10.5 - 4759 ft-lb/in² @Temperature -22.0 - 86.0 °F |
Average value: 3.22 J/cm² Grade Count:6 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified". Each property range of values reported.. |