Polymer Property : Charpy Impact Unnotched = 28.6 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact Unnotched 4.50 - 6.00 J/cm²

@Temperature -30.0 - -30.0 °C
21.4 - 28.6 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 5.25 J/cm² Grade Count:2
Overview of materials for Polyetheretherketone, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, PTFE Filled". Each property range of values reported is minimum and maximum values..
Charpy Impact Unnotched 3.00 - 6.00 J/cm²
14.3 - 28.6 ft-lb/in²
Average value: 4.80 J/cm² Grade Count:5
Overview of materials for Acetal Copolymer, 10% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% ar..
Charpy Impact Unnotched 4.50 - 6.00 J/cm²

@Temperature -30.0 - -30.0 °C
21.4 - 28.6 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 5.25 J/cm² Grade Count:4
Overview of materials for Acetal Copolymer, 10% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% ar..
Charpy Impact Unnotched 1.80 - 6.00 J/cm²

@Temperature -40.0 - -20.0 °C
8.57 - 28.6 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 3.64 J/cm² Grade Count:7
Overview of materials for Acetal Copolymer, 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% ar..
Charpy Impact Unnotched 5.00 - 6.00 J/cm²
23.8 - 28.6 ft-lb/in²
Average value: 5.36 J/cm² Grade Count:5
Overview of materials for Acetal Homopolymer, Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Glass Fiber Reinforced". Each property range of values reported is minimum and maxim..
Charpy Impact Unnotched 4.00 - 6.00 J/cm²

@Temperature 23.0 °C
19.0 - 28.6 ft-lb/in²

@Temperature 73.4 °F
ISO 179/ 1eU
Raschig Group 3572 Epoxy
Glass-fiber reinforced epoxy molding compound. Good mechanical strength and electrical strength, enhanced elasticity for ensuring good sealing under extreme heat and/or humidity, good chemical resis..
Charpy Impact Unnotched 4.00 - 6.00 J/cm²

@Temperature -30.0 - -20.0 °C
19.0 - 28.6 ft-lb/in²

@Temperature -22.0 - -4.00 °F
Average value: 4.87 J/cm² Grade Count:6
Overview of materials for Nylon 6, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of a..
Charpy Impact Unnotched 1.00 - 6.00 J/cm²
4.76 - 28.6 ft-lb/in²
Average value: 3.37 J/cm² Grade Count:31
Overview of materials for Nylon 66, Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Bead Filled". Each property range of values reported is minimum and maximum values of ap..
Charpy Impact Unnotched 2.70 - 6.00 J/cm²

@Temperature -40.0 - -30.0 °C
12.8 - 28.6 ft-lb/in²

@Temperature -40.0 - -22.0 °F
Average value: 4.42 J/cm² Grade Count:10
Overview of materials for Nylon 66, Glass Fiber/PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber/PTFE Filled". Each property range of values reported is minimum and maximum values..
Charpy Impact Unnotched 6.00 - 6.00 J/cm²

@Temperature -30.0 - -30.0 °C
28.6 - 28.6 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 6.00 J/cm² Grade Count:1
Overview of materials for Nylon 610, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of..
Charpy Impact Unnotched 4.00 - 6.00 J/cm²

@Temperature -30.0 - 30.0 °C
19.0 - 28.6 ft-lb/in²

@Temperature -22.0 - 86.0 °F
Average value: 5.50 J/cm² Grade Count:7
Overview of materials for Nylon 12, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of ..
Charpy Impact Unnotched 2.70 - 6.00 J/cm²
12.8 - 28.6 ft-lb/in²
Average value: 3.82 J/cm² Grade Count:12
Overview of materials for Polycarbonate, Glass + PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass + PTFE Filled". Each property range of values reported is minimum and maximum value..
Charpy Impact Unnotched 0.400 - 6.00 J/cm²
1.90 - 28.6 ft-lb/in²
Average value: 2.56 J/cm² Grade Count:22
Overview of materials for Epoxy, Molded, Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Molded, Glass Fiber Filler". Each property range of values reported is minimum and maximum values..
Charpy Impact Unnotched 2.00 - 6.00 J/cm²

@Temperature -40.0 - -30.0 °C
9.52 - 28.6 ft-lb/in²

@Temperature -40.0 - -22.0 °F
Average value: 4.35 J/cm² Grade Count:9
Overview of materials for Polyethylene Terephthalate (PET), 40% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 40% Glass Reinforced". Specific grades with glass content between 35% ..
Charpy Impact Unnotched 1.10 - 6.00 J/cm²
5.24 - 28.6 ft-lb/in²
Average value: 4.23 J/cm² Grade Count:7
Overview of materials for Polyphthalamide (PPA), Carbon Fiber + PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Carbon Fiber + PTFE Filled". Each property range of values reported is minimum and maxi..
Charpy Impact Unnotched 1.10 - 6.00 J/cm²

@Temperature -40.0 - -20.0 °C
5.24 - 28.6 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 3.55 J/cm² Grade Count:25
Overview of materials for Polypropylene with 20% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Glass Fiber Filler". Specific grades with glass content between 15% and 24% are i..