Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 26.0 - 40.0 kJ/m² @Temperature -30.0 - -30.0 °C |
12.4 - 19.0 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 33.0 kJ/m² Grade Count:2 |
Overview of materials for Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled".Specific grades with glass content between 5% .. |
|||
Izod Impact, Unnotched (ISO) | 40.0 - 40.0 kJ/m² @Temperature -30.0 - -30.0 °C |
19.0 - 19.0 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 40.0 kJ/m² Grade Count:1 |
Overview of materials for Polycarbonate, 30% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 30% Glass Filled". Specific grades with glass content between 25% and 34% are included. E.. |
|||
Izod Impact, Unnotched (ISO) | 29.8 - 39.9 kJ/m² | 14.2 - 19.0 ft-lb/in² | Average value: 33.3 kJ/m² Grade Count:9 |
Overview of materials for Polycarbonate, Carbon Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximum v.. |
|||
Izod Impact, Unnotched (ISO) | 25.0 - 40.0 kJ/m² @Temperature -30.0 - -30.0 °C |
11.9 - 19.0 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 34.7 kJ/m² Grade Count:5 |
Overview of materials for Nylon 6, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Bead Filled". Each property range of values reported is minimum and maximum values of app.. |
|||
Izod Impact, Unnotched (ISO) | 10.0 - 40.0 kJ/m² | 4.76 - 19.0 ft-lb/in² | Average value: 30.8 kJ/m² Grade Count:7 |
Overview of materials for Acetal Copolymer, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Glass Bead Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Izod Impact, Unnotched (ISO) | 25.0 - 40.0 kJ/m² @Temperature -30.0 - -30.0 °C |
11.9 - 19.0 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 32.5 kJ/m² Grade Count:2 |
Overview of materials for Polybutylene Terephthalate (PBT), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Mineral Filled". Each property range of values reported is minimum and.. |
|||
Izod Impact, Unnotched (ISO) | 13.0 - 40.0 kJ/m² @Temperature -30.0 - -30.0 °C |
6.19 - 19.0 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 27.3 kJ/m² Grade Count:6 |
Overview of materials for Polypropylene with 20% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Glass Fiber Filler". Specific grades with glass content between 15% and 24% are i.. |
|||
Izod Impact, Unnotched (ISO) | 40.0 - 40.0 kJ/m² @Temperature -30.0 - -30.0 °C |
19.0 - 19.0 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 40.0 kJ/m² Grade Count:1 |
Overview of materials for Polybutylene Terephthalate (PBT), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Carbon Fiber Filled". Each property range of values reported is minimu.. |