Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 52.0 kJ/m² @Temperature -30.0 °C |
24.7 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP FARADEX NX07330 PC+ABS (Asia Pacific) Faradex NX07330 is a compound based on PC+ABS blend resin containing stainless steel and glass fiber. Added features of this material include EMI/RFI Shielding and ESD. |
|||
Izod Impact, Unnotched (ISO) | 52.0 - 95.0 kJ/m² @Temperature -30.0 - -30.0 °C |
24.7 - 45.2 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 75.0 kJ/m² Grade Count:5 |
Overview of materials for Thermoplastic Polyurethane, Elastomer, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Glass Filled". Each property range of values reported is minimum .. |
|||
Izod Impact, Unnotched (ISO) | 52.0 - 83.0 kJ/m² | 24.7 - 39.5 ft-lb/in² | Average value: 62.3 kJ/m² Grade Count:3 |
Overview of materials for Acetal Copolymer, Silicone Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Silicone Filled". Each property range of values reported is minimum and maximum values.. |
|||
Izod Impact, Unnotched (ISO) | 52.0 kJ/m² | 24.7 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP DFI14 PC LNP* Lubricomp* DFI14 is a compound based on Polycarbonate resin containing 20% Glass Fiber and 2% Silicone. Added features include: Internally Lubricated. |
|||
Izod Impact, Unnotched (ISO) | 52.0 kJ/m² | 24.7 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP DFL12 PC LNP* Lubricomp* DFL12 is a compound based on Polycarbonate resin containing 10% Glass Fiber and 5% PTFE. Added features include: Internally Lubricated. |
|||
Izod Impact, Unnotched (ISO) | 52.0 - 85.0 kJ/m² @Temperature -40.0 - -30.0 °C |
24.7 - 40.4 ft-lb/in² @Temperature -40.0 - -22.0 °F |
Average value: 74.0 kJ/m² Grade Count:2 |
Overview of materials for Nylon 66, 30% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are inclu.. |
|||
Izod Impact, Unnotched (ISO) | 52.0 kJ/m² @Temperature 23.0 °C |
24.7 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Lubricomp FX00617 PE LNP* Lubricomp* FX00617 is a compound based on Polyethylene resin containing Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Amer.. |
|||
Izod Impact, Unnotched (ISO) | 52.0 kJ/m² @Temperature 23.0 °C |
24.7 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Lubricomp FX00617 PE (Asia Pacific) LNP* Lubricomp* FX00617 is a compound based on Polyethylene resin containing Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Asia.. |
|||
Izod Impact, Unnotched (ISO) | 52.0 kJ/m² @Temperature 23.0 °C |
24.7 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Lubricomp KX99792 Acetal Copoly (Asia Pacific) LNP* Lubricomp* KX99792 is a compound based on Acetal Copolymer resin containing Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the .. |
|||
Izod Impact, Unnotched (ISO) | 52.0 kJ/m² @Temperature 23.0 °C |
24.7 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Lubricomp KX99792 Acetal Copolymer LNP* Lubricomp* KX99792 is a compound based on Acetal Copolymer resin containing Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the .. |
|||
Izod Impact, Unnotched (ISO) | 52.0 kJ/m² | 24.7 ft-lb/in² | 80*10*3; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP QCL34 PA6.10 LNP* LUBRICOMP* QCL34 is a compound based on Nylon 6/10 resin containing 15% PTFE, 20% Carbon Fiber. Added features of this material include: Wear Resistant, Electrically Conductive. |
|||
Izod Impact, Unnotched (ISO) | 52.0 kJ/m² | 24.7 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP RCL26 PA6.6 LNP* LUBRICOMP* RCL26 is a compound based on Nylon 66 containing 30% Carbon Fiber, 10% PTFE. Added features of this grade include: Wear Resistant, Electrically Conductive. |
|||
Izod Impact, Unnotched (ISO) | 52.0 kJ/m² | 24.7 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP RCL34 PA 66 LNP* LUBRICOMP* RCL34 is a compound based on Nylon 66 containing 20% Carbon Fiber, 15% PTFE. Added features of this grade includes: Wear Resistant, Electrically Conductive. |
|||
Izod Impact, Unnotched (ISO) | 52.0 kJ/m² @Temperature -30.0 °C |
24.7 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics Valox® 553 PBT (Europe-Africa-Middle East) VALOX 553 is a 30% glass fibre reinforced, flame retardant PBT+PC blend with good warpage characteristics. Applications: appliance handles, spotlights, electric motors, pumphousings. |
|||
Izod Impact, Unnotched (ISO) | 52.0 kJ/m² | 24.7 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics Valox® K4560 PBT (Europe-Africa-Middle East) 30% glass reinforced PBT. Impact modified, high flow, hydrolytically stable. |
|||
Izod Impact, Unnotched (ISO) | 52.0 kJ/m² | 24.7 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON KX02764 Acetal LNP STAT-KON* KX02764 is a compound based on Acetal resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive. |
|||
Izod Impact, Unnotched (ISO) | 52.0 kJ/m² | 24.7 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP DF006HL PC LNP THERMOCOMP* DF006HL is a compound based on Polycarbonate resin containing 30% Glass Fiber. Added features of this material include: Low Extractible, Healthcare. |
|||
Izod Impact, Unnotched (ISO) | 52.0 kJ/m² | 24.7 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP DFZ22P PC (Asia Pacific) LNP* THERMOCOMP* DFZ22P is a compound based on Polycarbonate resin containing Glass Fiber, Milled Glass. Added features of this material include: Exceptional Processing. |
|||
Izod Impact, Unnotched (ISO) | 52.0 kJ/m² | 24.7 ft-lb/in² | GB/T 1843-2008 |
Sichuan Deyang Haton® hGR30 Polyphenylene Sulfide, Glass Fiber Reinforced Injection moldingInformation provided by Sichuan Deyang Chemical Co., LTD |
|||
Izod Impact, Unnotched (ISO) | 52.0 kJ/m² | 24.7 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP RF006H PA 66 LNP THERMOCOMP* RF006H is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added feature of this grade is: Healthcare. |
|||
Izod Impact, Unnotched (ISO) | 52.0 kJ/m² | 24.7 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP RF006XXZ PA 66 LNP THERMOCOMP* RF006XXZ is a compound based on Nylon 66 resin containing 30% Glass Fiber |
|||
Izod Impact, Unnotched (ISO) | 52.0 kJ/m² | 24.7 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP VERTON MX02795 PP (Asia Pacific) LNP* Verton* MX02795 is a compound based on Polypropylene resin containing Long Glass Fiber. Added features of this material include: Chemically Coupled, Heat Stabilized, UV Stabilized. |
|||
Izod Impact, Unnotched (ISO) | 52.0 kJ/m² | 24.7 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP DFZ22P PC LNP THERMOCOMP* DFZ22P is a compound based on Polycarbonate resin containing 10% Glass Fiber, 10% Milled Glass. Added features of this material include: Exceptional Processing. |
|||
Izod Impact, Unnotched (ISO) | 52.0 kJ/m² | 24.7 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP VERTON MX02795 PP LNP* VERTON* MX02795 is a compound based on Polypropylene resin containing Proprietary Fillers. Added features of this material include: Heat Stabilized, UV Stabilized, Structural. |
|||
Izod Impact, Unnotched (ISO) | 52.0 kJ/m² | 24.7 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP VERTON RV007SX9 PA 66 (Europe-Africa-Middle East) LNP* VERTON* RV007SX9 is a compound based on PA 66 resin containing Long Glass Fiber. |
|||
Izod Impact, Unnotched (ISO) | 52.0 kJ/m² @Temperature -30.0 °C |
24.7 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1eU |
Lubrizol ESTALOC® T514 Ester-Type, Reinforced Engineering Thermoplastic (European Grade) Description: Estaloc® RETP (Reinforced Engineering Thermoplastic) is a tough, dimensionally stable, abrasion-resistant thermoplastic that withstands demanding environments. Developed as an extensio.. |
|||
Izod Impact, Unnotched (ISO) | 52.0 kJ/m² | 24.7 ft-lb/in² | 80x10x4; ISO 180/1U |
Eurostar Star L PA66 30Y D51 PA66, Carbon Fiber Filled, Injection Molded Star L PA66 30Y D51 is a PTFE Lubricated, Carbon Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Unnotched (ISO) | 52.0 kJ/m² | 24.7 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP VERTON RV0079 PA 66 LNP VERTON* RV0079 is a compound based on Nylon 66 resin containing 35% Long Glasss Fiber. Added features of this material include: Flame Retardant, Structural. |
|||
Izod Impact, Unnotched (ISO) | 51.9 kJ/m² | 24.7 ft-lb/in² | ISO 180 |
LNP Thermocomp® UF-1008 Polyphthalamide, Glass Fiber Reinforcement